摘要:
Disclosed herein are methods for preparing fluorided solid oxides by contacting an acidic fluorine-containing compound with an inorganic base to form an aqueous mixture having a pH of at least 4, followed by contacting a solid oxide with the aqueous mixture to produce the fluorided solid oxide. Also disclosed are methods for preparing fluorided solid oxides by contacting an acidic fluorine-containing compound with a solid oxide to produce a mixture, followed by contacting the mixture with a inorganic base to produce the fluorided solid oxide at a pH of at least about 4. The fluorided solid oxide can be used as an activator component in a catalyst system for the polymerization of olefins.
摘要:
The present invention relates to a catalyst article for the exhaust system of a natural gas engine with improved sulphur and/or water tolerance. The catalyst article comprises a doped palladium-on-alumina catalyst, wherein the palladium-on-alumina catalyst is doped with manganese and/or zinc. The invention further relates to an exhaust gas treatment system, a natural gas combustion engine and to a method for the treatment of an exhaust gas from a natural gas combustion engine.
摘要:
Zn-promoted and/or Ga-promoted cracking catalysts, such as cracking catalysts comprising an MSE framework zeolite or an MFI framework zeolite can provide unexpectedly superior conversion of branched paraffins when used as part of a catalyst during reforming of a hydrocarbon fuel stream. The conversion and reforming of the hydrocarbon fuel stream can occur, for example, in an internal combustion engine. The conversion and reforming can allow for formation of higher octane compounds from the branched paraffins.
摘要:
Disclosed are methods for synthesizing an ester or a carboxylic acid from an organic alcohol. To form the ester one reacts, in the presence of oxygen gas, the alcohol with methanol or ethanol. This reaction occurs in the presence of a catalyst comprising palladium and a co-catalyst comprising bismuth, tellurium, lead, cerium, titanium, zinc and/or niobium (most preferably at least bismuth and tellurium). Alternatively that catalyst can be used to generate an acid from that alcohol, when water is also added to the reaction mix.
摘要:
A photocatalytic functional film has a structure of a substrate, a barrier layer and a photocatalytic layer stacked one on another. The barrier layer is an amorphous TiO2 film, the photocatalyst layer comprises an amorphous TiO2 film, and particles of visible light responsive photocatalytic material formed on the surface of the amorphous TiO2 film. A method for producing a photocatalytic functional film includes: adding an alcohol solvent and an acid to a titanium precursor to obtain a TiO2 amorphous sol by dehydration and de-alcoholization reaction; applying and drying the TiO2 amorphous sol on a substrate to form a barrier layer; and applying and drying a composition formed by mixing particles of visible light responsive photocatalyst material with the TiO2 amorphous sol on the barrier layer, to form a photocatalyst layer.
摘要:
A silica-based material comprising: silicon; aluminum; at least one fourth period element selected from the group consisting of iron, cobalt, nickel and zinc; and at least one basic element selected from the group consisting of alkali metal elements, alkali earth metal elements and rare earth elements, wherein the silica-based material comprises 42 to 90 mol % of the silicon, 3 to 38 mol % of the aluminum, 0.5 to 20 mol % of the fourth period element and 2 to 38 mol % of the basic element, based on a total mole of the silicon, the aluminum, the fourth period element and the basic element.
摘要:
A silica-based material comprising: silicon; aluminum; at least one fourth period element selected from the group consisting of iron, cobalt, nickel and zinc; and at least one basic element selected from the group consisting of alkali metal elements, alkali earth metal elements and rare earth elements, wherein the silica-based material comprises 42 to 90 mol % of the silicon, 3 to 38 mol % of the aluminum, 0.5 to 20 mol % of the fourth period element and 2 to 38 mol % of the basic element, based on a total mole of the silicon, the aluminum, the fourth period element and the basic element.
摘要:
A photocatalyst injection system including: a reactor primary system coolant collection section collecting a reactor primary system coolant containing a noble metal or noble metal ion from a reactor primary system; a photocatalyst addition section adding a photocatalyst to the collected reactor primary system coolant; an ultraviolet irradiation section irradiating, with ultraviolet rays, the coolant to which the photocatalyst has been added for producing, in the coolant, a noble metal-carrying photocatalyst in which the noble metal is carried on a surface of the photocatalyst; and a noble metal-carrying photocatalyst injection section injecting the coolant containing the noble metal-carrying photocatalyst into the reactor primary system.
摘要:
The present disclosure relates to a novel photocatalyst composition and a process of using the photocatalyst for the photocatalytic degradation of methyl tertiary-butyl ether (MTBE) in water. Palladium doped nano zinc oxide photocatalyst was prepared by zinc nitrate hexahydrate and an ammonium carbonate and the photocatalyst composition demonstrated more than 90-99% degradation of MTBE at room temperatures in a photo catalytic reaction conducted in an oxygen saturated aqueous medium.