摘要:
A method for processing a thermoplastic material that comprises a microwave-sensitive polymeric region, wherein the method includes exposing the microwave-sensitive polymeric region to microwaves; wherein the exposing results in an increase in the temperature of the polymeric region; and processing the thermoplastic material is disclosed.
摘要:
A composition comprising at least the following: A) an interpolymer comprising, in polymerized form, ethylene, an α-olefin and a nonconjugated polyene, and wherein the interpolymer comprises less than, or equal to, 5 weight percent of the polyene, based on the total amount of polymerized monomers, and wherein the interpolymer has a molecular weight distribution (Mw/Mn) less than 3; B) an interpolymer comprising, in polymerized form, ethylene, an α-olefin and a nonconjugated polyene, and wherein the interpolymer comprises greater than, or equal to, 5 weight percent of the polyene, based on the total amount of polymerized monomer; and wherein the total polyene content is less than 7 weight percent.
摘要:
The present invention relates to crosslinked, olefin elastic fibers where the olefin materials are specifically selected to provide a more robust fiber with higher tenacity and greater temperature stability. Such fibers will be less subject to breakage during fiber spinning and post-spinning (downstream processing) operations including spool formation and unwinding. The specific olefin material used is a blend having an overall melt index (I2) of less than 2.5 g/10 min before crosslinking with a density in the range of 0.865 to 0.885 g/cm3. One component of the blend will be characterized as having either a density in the range of from 0.855 to 0.88 g/cm3 or a residual crystallinity at 80° C. of greater than 9 percent but not both. The at least one other component will meet at least whichever characteristic the first component does not meet.
摘要翻译:本发明涉及交联的烯烃弹性纤维,其中烯烃材料被特别选择以提供具有更高韧性和更高温度稳定性的更坚固的纤维。 在纤维纺丝和后纺(下游处理)操作中,这种纤维将不会发生断裂,包括卷筒的形成和展开。 使用的特定烯烃材料是在0.865至0.885g / cm 3的密度交联之前具有小于2.5g / 10min的总体熔体指数(I 2)的共混物。 共混物的一种组分将被表征为具有在0.855至0.88g / cm 3范围内的密度或在80℃下的残余结晶度大于9%但不是均为二者。 至少一个其他组件将至少满足第一个组件不符合的特征。
摘要:
The invention provides a composition comprising at least the following: A) from “greater than zero” to “less than 100” phr (based on sum weight of Components A and B) of an interpolymer comprising, in polymerized form, ethylene, an α-olefin and a nonconjugated polyene, and wherein the interpolymer comprises less than, or equal to, 5 weight percent of the polyene, based on the total amount of polymerized monomers, and wherein the interpolymer has a molecular weight distribution (Mw/Mn) less than 3; B) from “less than 100” to “greater than zero” phr (based on sum weight of Components A and B) of an interpolymer comprising, in polymerized form, ethylene, an α-olefin and a nonconjugated polyene, and wherein the interpolymer comprises greater than, or equal to, 5 weight percent of the polyene, based on the total amount of polymerized monomer; and wherein the total polyene content is less than 7 weight percent (based on the total amount of polymerized monomers in the interpolymers of Components A and B).
摘要:
Knit fabric compositions have now been discovered that often have a balanced combination of desirable properties. Said fibric compositions comprise fibers of olefin block interpolymers or homogeneous branched ethylene polymers or a combination thereof. The fibers are characterized by an amount of crosslinking such that the fabric is capable of being molded.
摘要:
A fiber is obtainable from or comprises a blend of a propylene based polymer and an ethylene/α-olefin interpolymer characterized by an elastic recovery, Re, in percent at 300 percent strain and 1 cycle and a density, d, in grams/cubic centimeter, wherein the elastic recovery and the density satisfy the following relationship: Re>1481−1629(d). Such interpolymer can also be characterized by other properties. The fibers made therefrom have a relatively high elastic recovery and a relatively low coefficient of friction. The fibers can be cross-linked, if desired. Woven, knitted or non-woven fabrics can be made from such fibers.
摘要:
A fiber is obtainable from or comprises an ethylene/α-olefin interpolymer characterized by an elastic recovery, Re, in percent at 300 percent strain and (1) cycle and a density, d, in grams/cubic centimeter, wherein the elastic recovery and the density satisfy the following relationship: Re>1481−1629(d). Such interpolymer can also be characterized by other properties. The fibers made therefrom have a relatively high elastic recovery and a relatively low coefficient of friction. The fibers can be cross-linked, if desired. Woven or non-woven fabrics can be made from such fibers.
摘要:
Dyed fabric compositions have now been discovered that often have a balanced combination of desirable properties. The dyed fabric comprises one or more elastic fibers wherein the elastic fibers comprise the reaction product of at least one ethylene olefin block polymer and at least one crosslinking agent. Often the fabrics are characterized by a color change of greater than or equal to about 3.0 according to AATCC evaluation after a first wash by AATCC61-2003-2A.
摘要:
Substantially linear olefin polymers having a melt flow ratio, I10/I2,≧5.63, a molecular weight distribution, Mw/Mn, defined by the equation: Mw/Mn≦(I10/I2)−4.63, and a critical shear stress at onset of gross melt fracture of greater than about 4×106 dyne/cm2 and their method of manufacture are disclosed. The substantially linear olefin polymers preferably have at least about 0.01 long chain branches/1000 carbons and a molecular weight distribution from about 1.5 to about 2.5. The new polymers have improved processability over conventional olefin polymers and are useful in producing fabricated articles such as fibers, films, and molded parts.
摘要:
Substantially linear olefin polymers having a melt flow ratio, I10/I2, ≧5.63, a molecular weight distribution, Mw/Mn, defined by the equation: Mw/Mn≦(I10/I2)−4.63, and a critical shear stress at onset of gross melt fracture of greater than about 4×106 dyne/cm2 and their method of manufacture are disclosed. The substantially linear olefin polymers preferably have at least about 0.01 long chain branches/1000 carbons and a molecular weight distribution from about 1.5 to about 2.5. The new polymers have improved processability over conventional olefin polymers and are useful in producing fabricated articles such as fibers, films, and molded parts.