Abstract:
A process for treating organic compounds includes providing a composition which includes a substantially mesoporous structure of refractory oxide containing at least 97% by volume of pores having a pore size ranging from about 15 Å to about 30 Å and having a micropore volume of at least about 0.01 cc/g, wherein the mesoporous structure has incorporated therewith at least about 0.02% by weight of at least one catalytically and/or chemically active heteroatom selected from the group consisting of Al, Ti, V, Cr, Zn, Fe, Sn, Mo, Ga, Ni, Co, In, Zr, Mn, Cu, Mg, Pd, Pt and W, and the catalyst has an X-ray diffraction pattern with one peak at 0.3° to about 3.5° at 2 theta (θ). The catalyst is contacted with an organic feed under reaction conditions wherein the treating process is selected from alkylation, acylation, oligomerization, selective oxidation, hydrotreating, isomerization, demetalation, catalytic dewaxing, hydroxylation, hydrogenation, ammoximation, isomerization, dehydrogenation, cracking and adsorption.
Abstract:
A process for treating organic compounds includes providing a composition which includes a substantially mesoporous structure of silica containing at least 97% by volume of pores having a pore size ranging from about 15 Å to about 30 Å and having a micropore volume of at least about 0.01 cc/g, wherein the mesoporous structure has incorporated therewith at least about 0.02% by weight of at least one catalytically and/or chemically active heteroatom selected from the group consisting of Al, Ti, V, Cr, Zn, Fe, Sn, Mo, Ga, Ni, Co, In, Zr, Mn, Cu, Mg, Pd, Pt and W, and the catalyst has an X-ray diffraction pattern with one peak at 0.3° to about 3.5° at 2θ. The catalyst is contacted with an organic feed under reaction conditions wherein the treating process is selected from alkylation, acylation, oligomerization, selective oxidation, hydrotreating, isomerization, demetalation, catalytic dewaxing, hydroxylation, hydrogenation, ammoximation, isomerization, dehydrogenation, cracking and adsorption.
Abstract:
An aromatic alkylation process includes contacting an aromatic compound with an alkylating agent in the presence of a zeolite beta in a reaction zone under alkylation reaction conditions, wherein said zeolite beta is a high performance zeolite beta possessing a ratio of strong acid sites/weak acid sites greater than 1. The high performance zeolite beta is superior to conventional zeolite beta in the aromatics alkylation reaction, such as benzene alkylation with ethylene for ethylbenzene production, and benzene alkylation with propylene for cumene production.
Abstract:
A method for making a mesoporous or combined mesoporous/microporous inorganic oxide includes reacting a source of inorganic oxide with a complexing agent at a complexation temperature to provide a complex; decomposing the complex to provide a porous material precursor having an inorganic oxide framework containing at least some organic pore-forming agent; and removing the organic pore forming agent from the inorganic oxide framework by solvent extraction and/or calcination.
Abstract:
A catalytic material includes a microporous zeolite supported on a mesoporous inorganic oxide support. The microporous zeolite can include zeolite beta, zeolite Y or ZSM-5. The mesoporous inorganic oxide can be, e.g., silica or alumina, and can optionally include other metals. Methods for making and using the catalytic material are described herein.
Abstract:
The present invention is related to a novel method for assaying high quantity of nucleic acid fragments, by using the single-stranded anchor nucleic acid probe with biotin and this single-stranded anchor nucleic acid hereto form double-stranded nucleic acid with the target nucleic acid fragment. To detect the target fragment does not need electrophoresis or nucleic acid sequencing but needs the antibody against double-stranded nucleic acid or the specific single-stranded reporter nucleic acid labeled with a fluorescent dye. The present invention is also related to a kit of assaying high quantity of nucleic acid fragments. A container (the multiwell plate) coating the avidin family molecule is a tool for connecting with the biotinylated target nucleic acid and subjected to the antibody reaction or fluorescence detection.
Abstract:
A catalytic material includes microporous zeolites supported on a mesoporous inorganic oxide support. The microporous zeolite can include zeolite Beta, zeolite Y (including “ultra stable Y”—USY), mordenite, Zeolite L, ZSM-5, ZSM-11, ZSM-12, ZSM-20, Theta-1, ZSM-23, ZSM-34, ZSM-35, ZSM-48, SSZ-32, PSH-3, MCM-22, MCM-49, MCM-56, ITQ-1, ITQ-2, ITQ-4, ITQ-21, SAPO-5, SAPO-11, SAPO-37, Breck-6, ALPO4-5, etc. The mesoporous inorganic oxide can be e.g., silica or silicate. The catalytic material can be further modified by introducing some metals e.g. aluminum, titanium, molybdenum, nickel, cobalt, iron, tungsten, palladium and platinum. It can be used as catalysts for acylation, alkylation, dimerization, oligomerization, polymerization, hydrogenation, dehydrogenation, aromatization, isomerization, hydrotreating, catalytic cracking and hydrocracking reactions.
Abstract:
A catalyst composition includes an oxygen compound of an element selected from Group IVB or Group IVA of the Periodic Table of the Elements; an oxygen compound of an element selected from Group VIB or Group VIA of the Periodic Table of the Elements; and at least about 1% by weight based upon total catalyst weight of fumed silica particles. The catalyst composition is advantageously employed in hydrocarbon conversion processes such as isomerization.
Abstract:
An integrated process combines olefin epoxidation with production of cyclohexanone and cyclohexanol for nylon. Cyclohexanone and cyclohexanol normally produced by the oxidation of cyclohexane, in which cyclohexyl hydroperoxide is generated and is removed or decomposed down stream. However, this invention utilizes the intermediate of cyclohexyl hydroperoxide as an oxidant for the olefin epoxidation and meanwhile generates a valuable product.
Abstract:
A method for making a zeolite includes providing a reaction mixture containing mixed inorganic oxides and an organic templating agent, heating the reaction mixture, removing the templating agent at a temperature of no greater than 550° C. and under conditions such that the resulting zeolite is has an AAI of at least 1.2. The zeolite is preferably zeolite beta, TEA-mordenite or TEA-ZSM-12.