FOAM COMPOSITIONS AND USES THEREOF
    9.
    发明公开

    公开(公告)号:US20230257544A1

    公开(公告)日:2023-08-17

    申请号:US18306317

    申请日:2023-04-25

    申请人: NIKE, Inc.

    摘要: A variety of forms and foam components are provided, including foam components for articles of footwear and athletic equipment. The articles include a composition having a foam structure, wherein the composition includes a thermoplastic copolyester elastomer comprising: (a) a plurality of first segments, each first segment derived from a dihydroxy-terminated polydiol; (b) a plurality of second segments, each second segment derived from a diol; and (c) a plurality of third segments, each third segment derived from an aromatic dicarboxylic acid. Methods of making the compositions and foams are provided, as well as methods of making an article of footwear including at least one of the foam components. In some aspects, the foams and foam components can be made by extrusion or injection molding to foam the polymeric composition, or extrusion or injection molding to foam the polymeric composition followed by compression molding of the foam.

    METHOD FOR PREPARING POLYIMIDE AEROGEL HAVING LOW DIELECTRIC PROPERTIES, HIGH INSULATION, AND HIGH STRENGTH, AND POLYIMIDE AEROGEL PRODUCED THEREFROM

    公开(公告)号:US20230174735A1

    公开(公告)日:2023-06-08

    申请号:US18102921

    申请日:2023-01-30

    IPC分类号: C08J9/28

    摘要: The present invention relates to: a method for producing a polyimide aerogel having low dielectric properties, high insulation, and high strength; and a polyimide aerogel prepared therefrom. The present invention has the technical gist of a method for producing a polyimide aerogel having low dielectric properties, high insulation, and high strength, and a polyimide aerogel prepared therefrom, the method including: a first step of preparing a solvent; a second step of preparing a polyamic acid resin by reacting a diamine-based monomer with an acid anhydride monomer in a solvent; a third step of preparing a polyimide resin solution by imidizing the polyamic acid resin at 150 to 200° C.; a fourth step of preparing a polyimide wet gel by mixing a crosslinking agent and an acid with the polyimide resin solution; and a fifth step of preparing a polyimide aerogel by replacing the solvent contained in the polyimide wet gel with a main substitution solvent and a minor substitution solvent and then drying, wherein, in the fifth step, the main substitution solvent and the minor substitution solvent are each added to the polyimide wet gel in a stepwise manner to produce a polyimide aerogel having the porosity of 80 to 85 vol % while forming a skeletal structure having nano-pores through solvent-exchange.