摘要:
Disclosed are a red light and near-infrared light-emitting material and a preparation method thereof, and a light-emitting device including the light-emitting material. The red light and near-infrared light-emitting material contains a compound represented by a molecular formula, aSc2O3·Ga2O3·bR2O3, wherein the element R includes one or two of Cr, Ni, Fe, Yb, Nd or Er; 0.001≤a≤0.6; and 0.001≤b≤0.1. The light-emitting material can be excited by a spectrum having a wide wavelength range (ultraviolet light or purple light or blue light) to emit light with a wide spectrum of 650 nm to 1700 nm or multiple spectra, thus having higher light-emitting intensity.
摘要:
Provided is an oxide fluorescent material having a light emission peak in a wavelength range from red light to near-infrared light. The oxide fluorescent material has a composition including: a first element M1 being at least one element selected from the group consisting of Li, Na, K, Rb, and Cs; a second element M2 being at least one element selected from the group consisting of Ca, Sr, Mg, Ba, and Zn; Ge; O (oxygen); and Cr, the composition optionally including: a third element M3 being at least one element selected from the group consisting of Si, Ti, Zr, Sn, Hf, and Pb; and a fourth element M4 being at least one element selected from the group consisting of Eu, Ce, Tb, Pr, Nd, Sm, Yb, Ho, Er, Tm, Ni, and Mn. When the molar ratio of Ge, or the total molar ratio of the third element M3 and Ge in the case of comprising the third element M3, in 1 mol of the composition of the oxide fluorescent material is 6, the molar ratio of the first element M1 is 1.5 or more and 2.5 or less, the molar ratio of the second element M2 is 0.7 or more and 1.3 or less, the molar ratio of the third element M3 is 0 or more and 0.4 or less, the molar ratio of O (oxygen) is 12.9 or more and 15.1 or less, and the molar ratio of Cr is 0.2 or less. The oxide fluorescent material has a light emission peak wavelength of 700 nm or more and 1,050 nm or less in a light emission spectrum of the oxide fluorescent material.
摘要:
This light emitting device is provided with: a light emitting element which emits excitation light; and a far-red phosphor which is excited by the light of the light emitting element and emits light that has a peak wavelength within the range of 700-800 nm. The far-red phosphor has a median diameter within the range of 1-20 μm.
摘要:
This light emitting device is provided with: a light emitting element which emits excitation light; and a far-red phosphor which is excited by the light of the light emitting element and emits light that has a peak wavelength within the range of 700-800 nm. The far-red phosphor has a median diameter within the range of 1-20 μm.
摘要:
Aspects of the present invention provide a family of phosphor compositions that may be used in the field of lighting applications. These phosphor compositions have crystal structures and chemical bond arrangements that enable broad band absorption and excitation using radiation up to and including the blue wavelength region. A preferred embodiment of the phosphor compositions has a general formula of (AxAy . . . Az)3-(1+q)m(W1-rMor)O6:Lnm,Dqm, wherein x+y+ . . . +z=1; 0≦r≦1; 0≦q≦1; 0
摘要:
Provided is an aerosol method, and accompanying apparatus, for preparing powdered products of a variety of materials involving the use of an ultrasonic aerosol generator including a plurality of ultrasonic transducers underlying and ultrasonically energizing a reservoir of liquid feed which forms droplets of the aerosol. Carrier gas is delivered to different portions of the reservoir by a plurality of gas delivery ports delivering gas from a gas delivery system. The aerosol is pyrolyzed to form particles, which are then cooled and collected. The invention also provides powders made by the method and devices made using the powders.
摘要:
Some embodiments provide a compound represented by Formula 1. Other embodiments provide an organic light-emitting diode device, such as a light-emitting device for phototherapy, comprising a compound of Formula 1. Other embodiments provide an organic light-emitting device optionally comprising a wavelength convertor. Methods related to the treatment of diseases using phototherapy area also described.
摘要:
The invention relates to a transparent, luminescent plastic glass containing luminescent particles and to a method for producing the same. The glass hardly differs or differs only slightly in terms of transparency from pure plastic glass. In addition, said glass is easy to produce.
摘要:
A process for synthesizing nanoparticles, in particular metal salt nanoparticles. To the synthesis mixture is added a modifying reagent which binds, by means of a first functional group, to the nanoparticle surface and which carries a second functional group for binding to molecules which are specifically selected in dependence on the subsequent use of the nanoparticles. This dispenses with a postsynthetic, separate, application-specific modification step. A new substance class, the pentaalkyl iminobis(methylenephosphono)carboxylates, are particularly suitable for this purpose. These modifying reagents permit the nanoparticles to grow in a specifically controlled manner and, at the same time, modify the surface of the growing nanoparticles, (in-situ) during the synthesis, such that the particles can be very readily dissolved in a large number of solvents and carry functional groups for coupling on molecules, resulting in the particles having, immediately after having been synthesized, a certain all-round usability.
摘要:
A light-emitting material includes a matrix section 12 and light-emitting sections 11 dispersed and buried in the matrix section. The matrix section 12 comprises a first material and the light-emitting sections comprise a second material showing a eutectic relationship with the first material.