摘要:
The present invention relates to a thermosetting resin composition. The composition comprises from about 20 wt. % to about 70 wt. % of a thermosetting resin, from about 1 wt. % to about 30 wt. % of a curing agent, from about 0 wt. % to about 10 wt. % of an accelerant, a tungsten compound, and an inorganic filler. A prepreg may be prepared in an impregnation manner or a coating product may be prepared in a coating manner. The composition may decrease the thermal expansion coefficient of laminates and may effectively block UV light and decrease the light transmissivity.
摘要:
The invention pertains to a (per)fluoroelastomer composition comprising at least one (per)fluoroelastomer comprising iodine and/or bromine atoms, at least one polyunsaturated compound, at least one organic peroxide and at least one organic compound selected from the group consisting of (thio)urea compounds, cyclic addition products of ammonia or primary amine and aldehyde; (thio)carbamates.
摘要:
Provided are a rubber composition that achieves a balanced improvement in grip performance during the initial to late phases of running and abrasion resistance, and a pneumatic tire formed from the rubber composition. The present invention relates to a rubber composition containing a rubber component, sulfur, and a molten mixture of a solid resin and a plasticizer, the solid resin having an SP value of 9.2 to 13 and/or a softening point of 130° C. or higher, the plasticizer including at least one compound selected from the group consisting of phosphoric acid esters, phthalic acid esters, aliphatic polybasic acid esters, trimellitic acid esters, acetic acid esters, and ricinoleic acid esters, the solid resin being present in an amount of 1 part by mass or more per 100 parts by mass of the rubber component.
摘要:
The present invention provides a powder-free polymeric coating comprising a latex polymer, a metal oxide and a cross-linking agent, the latex polymer comprising a diene and an acrylic acid; and a powder-free glove comprising the powderless coating polymer.
摘要:
The present invention relates to a silica-containing rubber mixture produced from at least one rubber, one sulphur-containing alkoxysilane, one crosslinking agent, one filler, and optionally further rubber auxiliary products and from 0.1 to 15 phr of a polysulphide additive of the formula (I) A-S—(S)x—S—Y—S—(S)x—S-A (I) where x is 0, 1 or 2, Y is an aliphatic, cycloaliphatic or aromatic group that is optionally substituted or else comprises heteroatoms and A is an optionally substituted hydroxyethyl, carboxyaryl, hydroxyaryl, carboxyalkyl or thionamide moiety, and comprises from 0.1 to 15 parts by weight, based on 100 parts by weight of rubber used, of 1,6-bis(N,N-dibenzylthiocarbamoyldithio)hexane (CAS No.: 151900-44-6).
摘要:
The invention relates to a rubber composition prepared with pre-treated precipitated silica and tire with component comprised of such rubber composition. The rubber composition is comprised of at least one diene-based elastomer and said pre-treated precipitated silica together with a sulfur cure package comprised of elemental sulfur together with 1,6-bis (N,N′-dibenzylthiocarbamoyldithio)-hexane crosslinking agent and sulfenamide accelerator.
摘要:
A method of treating mineral slurries to inhibit bacterial growth includes adding an effective amount of one or more of sodium N-methyldithiocarbamate or methylammonium monomethyldithiocarbamate to the mineral slurry to inhibit bacterial growth.
摘要:
A method of treating mineral slurries to inhibit bacterial growth includes adding an effective amount of one or more of sodium N-methyldithiocarbamate or methylammonium monomethyldithiocarbamate to the mineral slurry to inhibit bacterial growth.
摘要:
The present invention provides a powder-free polymeric coating comprising a latex polymer, a metal oxide and a cross-linking agent, the latex polymer comprising a diene and an acrylic acid; and a powder-free glove comprising the powderless coating polymer.
摘要:
The present invention provides a method for producing a rubber composition containing a rubber component (A) of at least one selected from natural rubbers and synthetic dienic rubbers, an inorganic filler (B), a silane coupling agent (C) and an acidic compound (D), wherein the rubber composition is kneaded in multiple stages, and in the final stage of kneading, the acidic compound (D) is added, and the highest temperature of the rubber composition in the final stage of kneading is from 60 to 120° C. The production method enables production of a rubber composition having a low-heat-generation property while successfully preventing the coupling function activity of the silane coupling agent from lowering.