    摘要: To provide a chloroprene rubber composition providing good permanent compression set and excellent mechanical strength, a vulcanizate of the composition, and a molded article of the composition. A chloroprene rubber composition including a chloroprene rubber and a natural rubber in a total amount of 100 parts by mass, a copolymer of styrene and butadiene in an amount of 0.1 to 10 parts by mass, ethylene thiourea in an amount of 0.1 to 3.0 parts by mass, and dipentamethylenethiuram tetrasulfide in an amount of 0.1 to 3.0 parts by mass is vulcanized after or during molding of the composition to yield a vulcanized molding.

    摘要翻译: 提供提供良好的永久压缩永久变形和优异的机械强度的氯丁橡胶组合物,该组合物的硫化橡胶和该组合物的模塑制品。 总计为100质量份的氯丁橡胶和天然橡胶的氯丁二烯橡胶组合物,苯乙烯与丁二烯的共聚物的量为0.1〜10质量份,乙烯硫脲的含量为0.1〜3.0份 质量和0.1〜3.0质量份的二亚戊基秋兰姆四硫化物在组合物成型后或之后硫化,得到硫化成型品。

    Chloroprene rubber composition, and vulcanizates and moldings thereof
    6.
    发明授权
    Chloroprene rubber composition, and vulcanizates and moldings thereof 有权
    氯丁橡胶组合物及其硫化橡胶及其成型品

    公开(公告)号:US09260592B2

    公开(公告)日:2016-02-16

    申请号:US13884458

    申请日:2011-09-12

    申请人: Uichiro Yamagishi

    发明人: Uichiro Yamagishi

    摘要: To provide a chloroprene rubber composition that provides excellent low temperature characteristics such as low temperature permanent compression set and dynamic characteristics at low temperature and provides good permanent compression set, mechanical strength, and processing characteristics also at high temperature thus to achieve excellent characteristics within a wide temperature region, and a vulcanizate and a molding thereof.To a chloroprene rubber including a 2,3-dichlorobutadiene unit in an amount of 5 to 20% by mass, a natural rubber is added so as to give a ratio (chloroprene rubber/natural rubber) of 60/40 to 95/5 by mass ratio. Then, with respect to 100 parts by mass of the rubber components, ethylene thiourea is added in an amount of 0.1 to 3.0 parts by mass and dipentamethylenethiuram tetrasulfide is added in an amount of 0.1 to 3.0 parts by mass, thereby preparing the chloroprene rubber composition.

    摘要翻译: 为了提供一种在低温下提供低温永久压缩永久变形和动态特性等优异的低温特性的氯丁橡胶组合物,并且在高温下也提供良好的永久压缩永久变形,机械强度和加工特性,从而在宽的范围内实现优异的特性 温度区域,硫化橡胶及其成型体。 对于含有5〜20质量%的2,3-二氯丁二烯单元的氯丁二烯橡胶,添加天然橡胶,使得(氯丁二烯橡胶/天然橡胶)的比率(60/40〜95/5)为 质量比。 然后,相对于100质量份的橡胶成分,以0.1〜3.0质量份的量加入乙烯硫脲,以0.1〜3.0质量份的量加入二亚甲基秋兰姆四硫化物,由此制备氯丁二烯橡胶组合物 。

    FINISHING AGENT FOR TRIVALENT CHROMIUM CHEMICAL CONVERSION COATING FILM, AND METHOD FOR FINISHING BLACK TRIVALENT CHROMIUM CHEMICAL CONVERSION COATING FILM
    7.
    发明申请
    FINISHING AGENT FOR TRIVALENT CHROMIUM CHEMICAL CONVERSION COATING FILM, AND METHOD FOR FINISHING BLACK TRIVALENT CHROMIUM CHEMICAL CONVERSION COATING FILM 有权
    用于多色铬化学转化涂膜的成色剂及其黑色三价铬化学转化涂膜的方法

    公开(公告)号:US20140017514A1

    公开(公告)日:2014-01-16

    申请号:US14008362

    申请日:2012-03-30

    IPC分类号: C08K13/02 C23C16/56

    摘要: The purpose of the present invention is to provide a water-soluble finishing agent for a trivalent chromium chemical conversion coating film, which has low insulation, no problems with tightening properties, outstanding gloss and high corrosion resistance, and can obtain a trivalent chromium chemical conversion coating film, especially a black trivalent chromium chemical conversion coating film, having few scratches and flaws. The finishing agent for a trivalent chromium chemical conversion coating film is characterized by containing a trivalent chromium source, a phosphate ion source, a zinc ion source, a chelating agent which can form a complex with trivalent chromium, and a non-ionic water-soluble polymer compound selected from a group comprising poly(vinyl alcohol) and derivatives thereof, poly(vinyl pyrrolidone) and derivatives thereof, poly(alkylene glycol)s and derivatives thereof, and cellulose ethers and derivatives thereof.

    摘要翻译: 本发明的目的是提供一种用于三价铬化学转化涂膜的水溶性整理剂,它具有低绝缘性,没有紧固性能,优异的光泽和高耐腐蚀性的问题,并且可以获得三价铬化学转化 涂膜,特别是黑色三价铬化学转化涂膜,几乎没有划痕和缺陷。 三价铬化学转化膜的整理剂的特征在于含有三价铬源,磷酸根离子源,锌离子源,可与三价铬形成络合物的螯合剂和非离子水溶性 选自聚(乙烯醇)及其衍生物,聚(乙烯基吡咯烷酮)及其衍生物,聚(亚烷基二醇)及其衍生物,以及纤维素醚及其衍生物的聚合物化合物。

    Abrasion Resistant Elastomeric Compositions
    8.
    发明申请
    Abrasion Resistant Elastomeric Compositions 有权
    耐磨弹性组合物

    公开(公告)号:US20080033101A1

    公开(公告)日:2008-02-07

    申请号:US11871304

    申请日:2007-10-12

    IPC分类号: C08L41/00

    摘要: The present invention includes elastomeric compositions of BIMS elastomers suitable for abrasion resistant, high traction and/or air barrier articles. The compositions and articles made from those compositions of the invention can be described in any number of embodiments. In one embodiment, the composition suitable for an abrasion resistant article includes from 5 to 100 phr of a terpolymer of C4 to C7 isoolefin derived units, p-alkylstyrene derived units and p-bromomethylstyrene derived units; at least one filler such as carbon black, silica, precipitated silica, clay, or combinations thereof, and from 0.1 to 3 phr of at least one thiourea. The composition can also include from 5 to 80 phr of at least one elastomer selected from natural rubbers, polyisoprene rubber, styrene butadiene rubber (SBR), polybutadiene rubber, isoprene butadiene rubber (IBR), styrene-isoprene-butadiene rubber (SIBR), butyl rubber, halogenated butyl rubber, butadiene-acrylonitrile-styrene rubber (SNBR), and mixtures thereof. The composition can be cured by using one or a combination of curatives known in the rubber industry. For example, the composition may include from 0.1 to 10 phr of at least one of a peroxide, sulfur, a metal oxide, or a combination thereof. In a further embodiment, the thiourea is present from 0.2 to 1.5 phr in the composition.

    摘要翻译: 本发明包括适用于耐磨,高牵引和/或阻气制品的BIMS弹性体的弹性体组合物。 由本发明的组合物制成的组合物和制品可以在任何数量的实施方案中进行描述。 在一个实施方案中,适用于耐磨制品的组合物包括5至100phr的C 4〜C 7异构烯烃衍生单元的三元共聚物,对烷基苯乙烯衍生单元 和对溴甲基苯乙烯衍生单元; 至少一种填料如炭黑,二氧化硅,沉淀二氧化硅,粘土或其组合,以及0.1至3phr的至少一种硫脲。 该组合物还可以包括5-80phr的至少一种弹性体,其选自天然橡胶,聚异戊二烯橡胶,苯乙烯丁二烯橡胶(SBR),聚丁二烯橡胶,异戊二烯丁二烯橡胶(IBR),苯乙烯 - 异戊二烯 - 丁二烯橡胶(SIBR) 丁基橡胶,卤化丁基橡胶,丁二烯 - 丙烯腈 - 苯乙烯橡胶(SNBR)及其混合物。 组合物可以通过使用橡胶工业中已知的一种或其组合的固化剂来固化。 例如,组合物可以包括0.1至10phr的过氧化物,硫,金属氧化物或其组合中的至少一种。 在另一个实施方案中,组合物中硫脲的含量为0.2-1.5phr。

    Abrasion resistant elastomeric compositions
    9.
    发明申请
    Abrasion resistant elastomeric compositions 有权
    耐磨损弹性体组合物

    公开(公告)号:US20050085594A1

    公开(公告)日:2005-04-21

    申请号:US10503368

    申请日:2003-02-21

    摘要: The present invention includes elastomeric compositions of BIMS elastomers suitable for abrasion resistant, high traction and/or barrier articles. The compositions and articles made from those compositions of the inventions can be described in any number of embodiments. In one embodiment, the composition suitable for an abrasion resistant article includes from 5 to 100 phr of a terpolymer of C4 to C7 isoolefin derived units, p-alkylstyrene derived units and p-bromomehtylstyrene derived units; at least one filler such as carbon black, silica, precipitated silica, clay, or combinations thereof; and from 0.1 to 3 phr of at least one thiourea. The composition can also include from 5 to 80 phr of at least one elastomer selected from natural rubbers, polyisoprene rubber, styrene butadiene rubber (SBR), polybutadiene rubber, isoprene butadiene rubber (IBR), styrene-isoprene-butadiene rubber (SIBR), butyl rubber, halogenated butyl rubber, butadiene-acrylonitrile-styrene rubber (SNBR), and mixtures thereof The composition can be cured by using one or a combination of curatives known in the rubber industry. For example, the composition may include from 0.1 to 10 phr of at least one of a peroxide, sulfur, a metal oxide, or a combination thereof. In a further embodiment, the thiourea is present from 0.2 to 1.5 phr in the composition.

    摘要翻译: 本发明包括适用于耐磨,高牵引和/或阻挡物品的BIMS弹性体的弹性体组合物。 由本发明的组合物制成的组合物和制品可以在任何数量的实施方案中进行描述。 在一个实施方案中,适用于耐磨制品的组合物包括5至100phr的C 4〜C 7异构烯烃衍生单元的三元共聚物,对烷基苯乙烯衍生单元 和对溴甲基苯乙烯衍生单元; 至少一种填料如炭黑,二氧化硅,沉淀二氧化硅,粘土或其组合; 和0.1至3phr的至少一种硫脲。 该组合物还可以包括5-80phr的至少一种弹性体,其选自天然橡胶,聚异戊二烯橡胶,苯乙烯丁二烯橡胶(SBR),聚丁二烯橡胶,异戊二烯丁二烯橡胶(IBR),苯乙烯 - 异戊二烯 - 丁二烯橡胶(SIBR) 丁基橡胶,卤化丁基橡胶,丁二烯 - 丙烯腈 - 苯乙烯橡胶(SNBR)及其混合物。组合物可以通过使用橡胶工业中已知的一种或其组合的固化剂来固化。 例如,组合物可以包括0.1至10phr的过氧化物,硫,金属氧化物或其组合中的至少一种。 在另一个实施方案中,组合物中硫脲的含量为0.2-1.5phr。