公开(公告)号:US20110151202A1
公开(公告)日:2011-06-23
申请号:US12641851
申请日:2009-12-18
申请人: Casey J. FEINSTEIN , Kuo-Hua Sung , John Z. Zhong
发明人: Casey J. FEINSTEIN , Kuo-Hua Sung , John Z. Zhong
CPC分类号: B32B7/14 , B32B37/003 , B32B37/1292 , B32B2037/1253 , B32B2307/728 , B32B2307/73 , B32B2310/025 , B32B2310/0806 , B32B2310/12 , B32B2457/00 , Y10T428/24802
摘要: Controllable placement of a liquid adhesive on a substrate to confine the adhesive to a desired area of the substrate is disclosed. A controllable placement method can include dispensing a liquid adhesive into a designated area on a surface of a substrate, controllably confining the dispensed liquid adhesive to the designated area, and curing the confined liquid adhesive. The dispensed liquid adhesive can be controllably confined using various techniques, such as electrical repulsion, electrical attraction, capacitance, electrowetting, light curing, adhesive attracting-repulsing coatings, and substrate topography. A substrate having a controllably placed liquid adhesive thereon can be incorporated into electronic devices, such as a mobile telephone, a digital media player, or a personal computer.
摘要翻译: 公开了将液体粘合剂可控地放置在基底上以将粘合剂限制在基底的期望区域上。 可控放置方法可以包括将液体粘合剂分配到基底表面上的指定区域中,可控制地将分配的液体粘合剂限制在指定区域上,并固化限制的液体粘合剂。 分配的液体粘合剂可以使用各种技术,例如电排斥,电吸引,电容,电润湿,光固化,粘合剂吸引 - 斥斥涂层和基底形貌来控制地限制。 在其上具有可控地放置液体粘合剂的基板可以结合到诸如移动电话,数字媒体播放器或个人计算机的电子设备中。
-
公开(公告)号:US20100154992A1
公开(公告)日:2010-06-24
申请号:US12408636
申请日:2009-03-20
申请人: Casey J. Feinstein , Silvio Grespan , Kuo-Hua Sung , John Z. Zhong , Lynn Youngs
发明人: Casey J. Feinstein , Silvio Grespan , Kuo-Hua Sung , John Z. Zhong , Lynn Youngs
IPC分类号: B32B43/00
CPC分类号: B32B43/006 , B23K26/00 , B23K26/06 , B23K26/0604 , B23K26/50 , B23K26/57 , B26D1/547 , B26D3/28 , B26D3/282 , B26D7/086 , B26D7/10 , B26D2001/0013 , B26D2001/006 , B32B7/12 , B32B37/12 , B32B37/16 , B32B37/18 , B32B38/0004 , B32B38/16 , B32B2038/045 , B32B2310/022 , B32B2310/028 , B32B2310/0806 , B32B2310/0825 , B32B2310/0843 , B32B2310/0862 , B32B2457/20 , G02F1/1309 , G02F1/133308 , G02F1/13338 , G06F3/03547 , G06F2200/1634 , G06F2200/1635 , Y10T156/1153 , Y10T156/1158 , Y10T156/1184 , Y10T156/1911 , Y10T156/1917 , Y10T156/1967
摘要: Delamination of a laminated multilayer stack is provided by generating a layer-specific energy distribution in the stack during delamination. A localized energy transferrer can generate localized heating, cooling heating, cooling, or other form of energy absorption or transmission, in a bonding layer of a multilayer stack. Localized energy transfer can include thermal energy transfer, such as heating and/or cooling, acoustic energy transfer, such as applying ultrasonic energy, electromagnetic energy transfer, such as applying laser light, directed microwaves, etc. Localized energy transfer can generate a layer-specific energy distribution that can weaken the bonding layer while reducing damage to other layers of the stack.
摘要翻译: 通过在分层期间在堆叠中产生层特定的能量分布来提供层压多层叠层的分层。 局部能量转移器可以在多层叠层的粘合层中产生局部加热,冷却加热,冷却或其它形式的能量吸收或传输。 局部能量转移可以包括诸如加热和/或冷却之类的热能传递,诸如施加超声波能量的声能传递,诸如施加激光的电磁能量传递,定向微波等。局部能量传递可以产生层 - 比能量分布可以削弱结合层,同时减少对堆叠的其它层的损伤。
-
公开(公告)号:US09944554B2
公开(公告)日:2018-04-17
申请号:US13233978
申请日:2011-09-15
申请人: Seung Jae Hong , Casey J. Feinstein , Lili Huang , Sunggu Kang , Kuo-Hua Sung , John Z. Zhong
发明人: Seung Jae Hong , Casey J. Feinstein , Lili Huang , Sunggu Kang , Kuo-Hua Sung , John Z. Zhong
CPC分类号: C03C21/002 , C03C17/002 , Y10T29/49124
摘要: Methods for chemically strengthening the edges of glass sheets are provided. Voids can be formed in a mother sheet. The edges of these voids may correspond to a portion of the new edges that would normally be created during separation and free shaping of the mother sheet. The mother sheet can then be immersed in a chemical strengthener. The edges of the voids can be chemically strengthened in addition to the front and back sides of the mother sheet. After thin film processing and separation, each of the resulting individual sheets has been chemically strengthened on both sides and on a portion of its edges.
-
公开(公告)号:US20130068505A1
公开(公告)日:2013-03-21
申请号:US13233978
申请日:2011-09-15
申请人: Seung Jae Hong , Casey J. Feinstein , Lili Huang , Sunggu Kang , Kuo-Hua Sung , John Z. Zhong
发明人: Seung Jae Hong , Casey J. Feinstein , Lili Huang , Sunggu Kang , Kuo-Hua Sung , John Z. Zhong
CPC分类号: C03C21/002 , C03C17/002 , Y10T29/49124
摘要: Methods for chemically strengthening the edges of glass sheets are provided. Voids can be formed in a mother sheet. The edges of these voids may correspond to a portion of the new edges that would normally be created during separation and free shaping of the mother sheet. The mother sheet can then be immersed in a chemical strengthener. The edges of the voids can be chemically strengthened in addition to the front and back sides of the mother sheet. After thin film processing and separation, each of the resulting individual sheets has been chemically strengthened on both sides and on a portion of its edges.
摘要翻译: 提供了化学强化玻璃边缘的方法。 可以在母片中形成空隙。 这些空隙的边缘可以对应于通常在分离期间产生的新边缘的一部分,并且母板的自由成形。 然后将母片浸入化学加强剂中。 除了母板的正面和背面之外,空隙的边缘可以被化学强化。 在薄膜加工和分离之后,每个所得到的各个片材在两侧和其一部分边缘上已被化学强化。
-
公开(公告)号:US08196636B2
公开(公告)日:2012-06-12
申请号:US12842905
申请日:2010-07-23
申请人: Kuo-Hua Sung , Troy J. Edwards , Casey J. Feinstein , John Z. Zhong , Steven Porter Hotelling , Andrew David Lauder
发明人: Kuo-Hua Sung , Troy J. Edwards , Casey J. Feinstein , John Z. Zhong , Steven Porter Hotelling , Andrew David Lauder
IPC分类号: B29C65/02
CPC分类号: B32B38/1866 , B29C63/0047 , B29C63/0073 , B32B17/064 , B32B37/003 , B32B37/0053 , B32B37/10 , B32B37/12 , B32B38/1858 , B32B2037/264 , B32B2038/047 , B32B2457/00 , G06F3/03543 , Y10T156/10 , Y10T156/1028 , Y10T156/17 , Y10T156/1793 , Y10T156/18
摘要: A method of laminating a surface of a flexible material to a surface of a rigid, curved material. The method includes pressing an area of the surface of the flexible material into the surface of the rigid, curved material with a holder to create a contact area while the flexible material is conformed to the holder, which has a curvature greater than a curvature of the rigid, curved material surface; and changing the contact area between the surface of the flexible material and the surface of the rigid, curved material while maintaining pressure on the contact area until the surface of the flexible material and the surface of the rigid curved material are laminated.
-
公开(公告)号:US09409383B2
公开(公告)日:2016-08-09
申请号:US12408636
申请日:2009-03-20
申请人: Casey J. Feinstein , Silvio Grespan , Kuo-Hua Sung , John Z. Zhong , Lynn Youngs
发明人: Casey J. Feinstein , Silvio Grespan , Kuo-Hua Sung , John Z. Zhong , Lynn Youngs
IPC分类号: B29C63/00 , B32B43/00 , B26D7/10 , B26D1/547 , B26D3/28 , G02F1/13 , G02F1/1333 , G06F3/0354 , B32B7/12 , B32B37/16 , B32B38/16 , B23K26/00 , B23K26/06 , B32B38/00 , B26D7/08 , B26D1/00 , B32B37/18 , B32B38/04 , B32B37/12
CPC分类号: B32B43/006 , B23K26/00 , B23K26/06 , B23K26/0604 , B23K26/50 , B23K26/57 , B26D1/547 , B26D3/28 , B26D3/282 , B26D7/086 , B26D7/10 , B26D2001/0013 , B26D2001/006 , B32B7/12 , B32B37/12 , B32B37/16 , B32B37/18 , B32B38/0004 , B32B38/16 , B32B2038/045 , B32B2310/022 , B32B2310/028 , B32B2310/0806 , B32B2310/0825 , B32B2310/0843 , B32B2310/0862 , B32B2457/20 , G02F1/1309 , G02F1/133308 , G02F1/13338 , G06F3/03547 , G06F2200/1634 , G06F2200/1635 , Y10T156/1153 , Y10T156/1158 , Y10T156/1184 , Y10T156/1911 , Y10T156/1917 , Y10T156/1967
摘要: Delamination of a laminated multilayer stack is provided by generating a layer-specific energy distribution in the stack during delamination. A localized energy transferrer can generate localized heating, cooling heating, cooling, or other form of energy absorption or transmission, in a bonding layer of a multilayer stack. Localized energy transfer can include thermal energy transfer, such as heating and/or cooling, acoustic energy transfer, such as applying ultrasonic energy, electromagnetic energy transfer, such as applying laser light, directed microwaves, etc. Localized energy transfer can generate a layer-specific energy distribution that can weaken the bonding layer while reducing damage to other layers of the stack.
摘要翻译: 通过在分层期间在堆叠中产生层特定的能量分布来提供层压多层叠层的分层。 局部能量转移器可以在多层叠层的粘合层中产生局部加热,冷却加热,冷却或其它形式的能量吸收或传输。 局部能量转移可以包括诸如加热和/或冷却之类的热能传递,诸如施加超声波能量的声能传递,诸如施加激光的电磁能量传递,定向微波等。局部能量传递可以产生层 - 比能量分布可以削弱结合层,同时减少对堆叠的其它层的损伤。
-
公开(公告)号:US08608896B2
公开(公告)日:2013-12-17
申请号:US13231818
申请日:2011-09-13
IPC分类号: B05D1/14
CPC分类号: C09J5/00 , B29C65/4855 , B29C65/5021 , B29C65/5057 , B29C65/5064 , B29C65/524 , B29C66/342 , B29C66/3452 , B29C66/45 , C09J2201/36
摘要: Methods for liquid adhesive lamination for precision adhesive control are provided. Precision liquid adhesive control can be obtained by first patterning liquid adhesive in a thin pre-coat layer on a substrate. A second adhesive layer can then be patterned on top of the pre-coat layer. When the second substrate is pressed onto the first substrate, the second substrate first comes into contact with the second adhesive layer. The adhesive can then be spread uniformly across the two substrates without forming voids. Alternatively, a single liquid adhesive layer can be formed in a three dimensional gradient pattern.
摘要翻译: 提供了用于精密粘合剂控制的液体粘合剂层压方法。 通过首先在基材上的薄预涂层中图案化液体粘合剂可以获得精密的液体粘合剂控制。 然后可以在预涂层的顶部上构图第二粘合剂层。 当第二基板被按压到第一基板上时,第二基板首先与第二粘合剂层接触。 然后可以将粘合剂均匀地铺展在两个基材上而不形成空隙。 或者,可以以三维梯度图案形成单个液体粘合剂层。
-
公开(公告)号:US20130062011A1
公开(公告)日:2013-03-14
申请号:US13231818
申请日:2011-09-13
CPC分类号: C09J5/00 , B29C65/4855 , B29C65/5021 , B29C65/5057 , B29C65/5064 , B29C65/524 , B29C66/342 , B29C66/3452 , B29C66/45 , C09J2201/36
摘要: Methods for liquid adhesive lamination for precision adhesive control are provided. Precision liquid adhesive control can be obtained by first patterning liquid adhesive in a thin pre-coat layer on a substrate. A second adhesive layer can then be patterned on top of the pre-coat layer. When the second substrate is pressed onto the first substrate, the second substrate first comes into contact with the second adhesive layer. The adhesive can then be spread uniformly across the two substrates without forming voids. Alternatively, a single liquid adhesive layer can be formed in a three dimensional gradient pattern.
摘要翻译: 提供了用于精密粘合剂控制的液体粘合剂层压方法。 通过首先在基材上的薄预涂层中图案化液体粘合剂可以获得精密的液体粘合剂控制。 然后可以在预涂层的顶部上构图第二粘合剂层。 当第二基板被按压到第一基板上时,第二基板首先与第二粘合剂层接触。 然后可以将粘合剂均匀地铺展在两个基材上而不形成空隙。 或者,可以以三维梯度图案形成单个液体粘合剂层。
-
公开(公告)号:US20120111479A1
公开(公告)日:2012-05-10
申请号:US12940500
申请日:2010-11-05
申请人: Kuo-Hua Sung , Casey J. Feinstein , Silvio Grespan
发明人: Kuo-Hua Sung , Casey J. Feinstein , Silvio Grespan
CPC分类号: B32B38/1866 , B32B17/10036 , B32B17/10146 , B32B17/10174 , B32B17/10211 , B32B2457/208
摘要: A method of forming a curved touch surface is disclosed. According to an embodiment, the method includes depositing a touch sensor pattern on a flexible substrate; and curving the flexible substrate, using a chuck surface supporting the flexible substrate, to conform to a shape of a curved cover surface. Then, the curved flexible substrate can be laminated or otherwise adhered to the cover surface. The flexible substrate can be a glass substrate greater than 200 μm in thickness, and can be reduced to a desired thickness below 200 μm after the touch sensor pattern is deposited thereon. The flexible substrate can be curved by supporting the flexible substrate on the chuck surface such that the flexible substrate conforms to a shape of the chuck surface, or forcing the flexible substrate against the cover surface, such that the flexible substrate conforms to the shape of the curved cover surface.
摘要翻译: 公开了一种形成弯曲的触摸表面的方法。 根据实施例,该方法包括将触摸传感器图案沉积在柔性基板上; 并且使用支撑柔性基板的卡盘表面弯曲柔性基板,以符合弯曲盖表面的形状。 然后,弯曲的柔性基板可以层压或以其他方式粘附到盖表面。 柔性基板可以是厚度大于200μm的玻璃基板,并且可以在其上沉积触摸传感器图案之后将其减小到低于200μm的期望厚度。 柔性基板可以通过将柔性基板支撑在卡盘表面上而弯曲,使得柔性基板符合卡盘表面的形状,或者将柔性基板强制抵靠盖表面,使得柔性基板符合 弯曲的盖面。
-
公开(公告)号:US08875652B2
公开(公告)日:2014-11-04
申请号:US13232902
申请日:2011-09-14
IPC分类号: B05C9/08 , B05C11/00 , B05C3/18 , C23C16/52 , B29C65/00 , B29C65/14 , B05C9/12 , C23C14/02 , C08J7/18 , C09J5/00 , H01L23/00 , B32B7/12 , B29C65/48 , B29L31/34 , B29C65/52
CPC分类号: B05C9/12 , B05C3/18 , B05C11/00 , B29C65/1406 , B29C65/1435 , B29C65/1448 , B29C65/1464 , B29C65/1496 , B29C65/4845 , B29C65/52 , B29C66/324 , B29C66/345 , B29C66/45 , B29C66/8322 , B29L2031/3475 , B32B7/12 , C08J7/18 , C09J5/00 , C09J2205/31 , C23C14/02 , H01L24/00 , H01L24/75 , H01L24/83 , H01L2224/75901 , H01L2224/83874 , H01L2224/83909 , H01L2224/83951
摘要: A system for controlling a boundary of spreading liquid adhesive on a surface is disclosed. The system includes one or more ultra-violet (UV) sources configurable to emit UV light onto the liquid adhesive; and a control circuit coupled to the one or more UV sources and configured to control the one or more UV sources to selectively apply the UV light at selected locations on the liquid adhesive to cure the adhesive and prevent its further spread at those locations.