摘要:
An all (111) MTJ stack is disclosed in which there are no transitions between different crystalline orientations when going from layer to layer. This is accomplished by providing strongly (111)-textured layers immediately below the MgO tunnel barrier to induce a (111) orientation therein.
摘要:
A magnetic element in a spintronic device or serving as a propagation medium in a domain wall motion device is disclosed wherein first and second interfaces of a free layer with a perpendicular Hk enhancing layer and tunnel barrier, respectively, produce enhanced surface perpendicular anisotropy to increase thermal stability in a magnetic tunnel junction. The free layer may be a single layer or a composite and is comprised of a glassing agent that has a first concentration in a middle portion thereof and a second concentration less than the first concentration in regions near first and second interfaces. A CoFeB free layer selectively crystallizes along first and second interfaces but maintains an amorphous character in a middle region containing a glass agent providing the annealing temperature is less than the crystallization temperature of the middle region.
摘要:
An all (111) MTJ stack is disclosed in which there are no transitions between different crystalline orientations when going from layer to layer. This is accomplished by providing strongly (111)-textured layers immediately below the MgO tunnel barrier to induce a (111) orientation therein.
摘要:
A boron or boron containing dusting layer such as CoB or FeB is formed along one or both of top and bottom surfaces of a free layer at interfaces with a tunnel barrier layer and capping layer to improve thermal stability while maintaining other magnetic properties of a MTJ stack. Each dusting layer has a thickness from 0.2 to 20 Angstroms and may be used as deposited, or at temperatures up to 400° C. or higher, or following a subsequent anneal at 400° C. or higher. The free layer may be a single layer of CoFe, Co, CoFeB or CoFeNiB, or may include a non-magnetic insertion layer. The resulting MTJ is suitable for STT-MRAM memory elements or spintronic devices. Perpendicular magnetic anisotropy is maintained in the free layer at temperatures up to 400° C. or higher. Ku enhancement is achieved and the retention time of a memory cell for STT-MRAM designs is increased.
摘要:
Enhanced Hc and Hk in addition to higher thermal stability to 400° C. are achieved in magnetic devices by adding dusting layers on top and bottom surfaces of a spacer in a synthetic antiferromagnetic (SAF) structure to give a RL1/DL1/spacer/DL2/RL2 reference layer configuration where RL1 and RL2 layers exhibit perpendicular magnetic anisotropy (PMA), the spacer induces antiferromagnetic coupling between RL1 and RL2, and DL1 and DL2 are dusting layers that enhance PMA. RL1 and RL2 layers are selected from laminates such as (Ni/Co)n, L10 alloys, or rare earth-transition metal alloys. The reference layer may be incorporated in STT-MRAM memory elements or in spintronic devices including a spin transfer oscillator. Dusting layers and a similar SAF design may be employed in a free layer for Ku enhancement and to increase the retention time of a memory cell.
摘要:
Enhanced Hc and Hk in addition to higher thermal stability to 400° C. are achieved in magnetic devices by adding dusting layers on top and bottom surfaces of a spacer in a synthetic antiferromagnetic (SAF) structure to give a RL1/DL1/spacer/DL2/RL2 reference layer configuration where RL1 and RL2 layers exhibit perpendicular magnetic anisotropy (PMA), the spacer induces antiferromagnetic coupling between RL1 and RL2, and DL1 and DL2 are dusting layers that enhance PMA. RL1 and RL2 layers are selected from laminates such as (Ni/Co)n, L10 alloys, or rare earth-transition metal alloys. The reference layer may be incorporated in STT-MRAM memory elements or in spintronic devices including a spin transfer oscillator. Dusting layers and a similar SAF design may be employed in a free layer for Ku enhancement and to increase the retention time of a memory cell.
摘要:
A synthetic antiferromagnetic (SAF) structure for a spintronic device is disclosed and has an AP2/antiferromagnetic (AF) coupling/CoFeB configuration. The SAF structure is thinned to reduce the fringing (Ho) field while maintaining high coercivity. The AP2 reference layer has intrinsic perpendicular magnetic anisotropy (PMA) and induces PMA in a thin CoFeB layer through AF coupling. In one embodiment, AF coupling is improved by inserting a Co dusting layer on top and bottom surfaces of a Ru AF coupling layer. When AP2 is (Co/Ni)4, and CoFeB thickness is 7.5 Angstroms, Ho is reduced to 125 Oe, Hc is 1000 Oe, and a balanced saturation magnetization-thickness product (Mst)=0.99 is achieved. The SAF structure may also be represented as FL2/AF coupling/CoFeB where FL2 is a ferromagnetic layer with intrinsic PMA.
摘要:
A magnetic element is disclosed wherein first and second interfaces of a free layer with a perpendicular Hk enhancing layer and tunnel barrier, respectively, produce enhanced surface perpendicular anisotropy to increase thermal stability in a magnetic tunnel junction (MTJ). The free layer may be a single layer or a composite and is comprised of one or more glassing agents that have a first concentration in a middle portion thereof and a second concentration less than the first concentration in regions near first and second interfaces. As a result, a CoFeB free layer, for example, selectively crystallizes along first and second interfaces but maintains an amorphous character in a middle region containing a glass agent providing the annealing temperature is less than the crystallization temperature of the middle region. The magnetic element may be part of a spintronic device or serve as a propagation medium in a domain wall motion device.
摘要:
A MTJ for a spintronic device is disclosed and includes a thin seed layer that enhances perpendicular magnetic anisotropy (PMA) in an overlying laminated layer with a (Co/X)n or (CoX)n composition where n is from 2 to 30, X is one of V, Rh, Ir, Os, Ru, Au, Cr, Mo, Cu, Ti, Re, Mg, or Si, and CoX is a disordered alloy. A CoFeB layer may be formed between the laminated layer and a tunnel barrier layer to serve as a transitional layer between a (111) laminate and (100) MgO tunnel barrier. The laminated layer may be used as a reference layer, dipole layer, or free layer in a MTJ. Annealing between 300° C. and 400° C. may be used to further enhance PMA in the laminated layer.
摘要:
A MTJ for a spintronic device is disclosed and includes a thin seed layer that enhances perpendicular magnetic anisotropy (PMA) in an overlying laminated layer with a (Co/X)n or (CoX)n composition where n is from 2 to 30, X is one of V, Rh, Ir, Os, Ru, Au, Cr, Mo, Cu, Ti, Re, Mg, or Si, and CoX is a disordered alloy. A CoFeB layer may be formed between the laminated layer and a tunnel barrier layer to serve as a transitional layer between a (111) laminate and (100) MgO tunnel barrier. The laminated layer may be used as a reference layer, dipole layer, or free layer in a MTJ. Annealing between 300° C. and 400° C. may be used to further enhance PMA in the laminated layer.