摘要:
In a process for preparing a supported hydrogenation catalyst with increased hydrogenation activity, which comprises a hydrogenating metal and/or an oxide of a hydrogenating metal on an Al2O3-containing support material, said calcined supported hydrogenation catalyst is treated before or after the final shaping thereof and before use thereof in the hydrogenation with a base solution having a pH of >10 at a temperature in the range from 20 to 120° C. for 1 to 300 hours.
摘要翻译:在含有Al 2 O 3的载体材料上制备含氢化金属和/或氢化金属的氢化物的氢化活性增加的负载型氢化催化剂的方法中,所述煅烧的负载氢化催化剂在其最终成型之前或之后进行处理 并且在使用之前,在温度为20〜120℃的pH为> 10的碱溶液中氢化1〜300小时。
摘要:
The present invention relates to a process for separating off solvents from solvent-comprising hydrogenation outputs from a catalytic hydrogenation process, which comprise at least one water-soluble hydrogenation product having at least one alcohol, lactone, ether, lactam or amino group in a solvent which is immiscible or not completely miscible with water and has a boiling point below 100° C., wherein water is added to the hydrogenation output, the solvent-comprising phase is separated off and recirculated to the hydrogenation.
摘要:
The invention relates to a process for the regeneration of a copper-, zinc- and zirconium oxide-comprising adsorption composition after use thereof for the adsorptive removal of carbon monoxide from substance streams comprising carbon monoxide and at least one olefin, in which the adsorption composition is heated to a temperature in the range from 160 to 400° C. and a regeneration gas is passed through the adsorption composition, wherein the regeneration gas comprises 1000 to 3000 ppm of oxygen in an inert carrier gas.
摘要:
The present invention relates to a process for preparing 1,2-propanediol, in which a glycerol-containing stream, especially a stream obtained on the industrial scale in the production of biodiesel, is subjected to a hydrogenation in a two-stage reactor cascade.
摘要:
The invention relates to a process for the regeneration of a copper-, zinc- and zirconium oxide-comprising adsorption composition after use thereof for the adsorptive removal of carbon monoxide from substance streams comprising carbon monoxide and at least one olefin, in which the adsorption composition is heated to a temperature in the range from 160 to 400° C. and a regeneration gas is passed through the adsorption composition, wherein the regeneration gas comprises 1000 to 3000 ppm of oxygen in an inert carrier gas.
摘要:
Method of reducing the concentration of sulfur and/or a sulfur-containing compound in a biochemically prepared organic compound by bringing the respective organic compound into contact with an adsorbent, wherein the adsorbent is a clay doped with silver and/or a silver compound.
摘要:
Carbon monoxide is removed from streams by adsorption on an adsorption composition which comprises copper, zinc and zirconium oxides and whose copper-comprising component has a degree of reduction, expressed as weight ratio of metallic copper to the sum of metallic copper and copper oxides, calculated as CuO, of at least 45% and not more than 75%.
摘要:
The present invention relates to a process for preparing optically active hydroxy-, alkoxy-, amino-, alkyl-, aryl- or chlorine-substituted alcohols or hydroxy carboxylic acids having from 3 to 25 carbon atoms or their acid derivatives or cyclization products by hydrogenating the correspondingly substituted optically active mono- or dicarboxylic acids or their acid derivatives in the presence of a catalyst whose active component consists of rhenium or of rhenium and comprises at least one further element having an atomic number of from 22 to 83, with the provisos that a. the at least one further element having an atomic number of from 22 to 83 is not ruthenium and b. in the case of the preparation of optically active 2-amino-, 2-chloro-, 2-hydroxy- and 2-alkoxy-1-alkanols by catalytically hydrogenating corresponding optically active 2-aminocarboxylic acids, 2-chlorocarboxylic acids, 2-hydroxycarboxylic acids and 2-alkoxycarboxylic acids or their acid derivatives, the at least one further element having an atomic number of from 22 to 83 is not palladium or platinum.
摘要:
The invention relates to a process for regenerating a hydrogen chloride oxidation catalyst comprising ruthenium oxide on a support material, which comprises the steps a) reduction of the catalyst in a gas stream comprising hydrogen chloride and optionally an inert gas at a temperature of from 100 to 800° C., b) recalcination of the catalyst in an oxygen-comprising gas stream at a temperature of from 150 to 800° C.
摘要:
In a process for preparing a supported hydrogenation catalyst with increased hydrogenation activity, which comprises a hydrogenating metal and/or an oxide of a hydrogenating metal on an Al2O3-containing support material, said calcined supported hydrogenation catalyst is treated before or after the final shaping thereof and before use thereof in the hydrogenation with a base solution having a pH of >10 at a temperature in the range from 20 to 120° C. for 1 to 300 hours.
摘要翻译:在含有Al 2 O 3的载体材料上制备含氢化金属和/或氢化金属的氢化物的氢化活性增加的负载型氢化催化剂的方法中,所述煅烧的负载氢化催化剂在其最终成型之前或之后进行处理 并且在使用之前,在温度为20〜120℃的pH为> 10的碱溶液中氢化1〜300小时。