Abstract:
The present disclosure relates to novel procatalyst compositions including a titanium moiety, a magnesium halide support, a hydrocarbon solution in which the magnesium halide support is formed, and an electron donor modifier having the formula (I). The present disclosure further relates to a one-pot process for preparing the novel procatalyst compositions, as well as use of the novel procatalyst compositions in solution processes for polymerization of ethylene and at least one additional polymerizable monomer to form a polymer composition.
Abstract:
Mono- and multi-layer films comprising a polyethylene composition which comprises the reaction product of ethylene and optionally one or more alpha olefin comonomers in the presence of a catalyst composition comprising a multi-metallic procatalyst via a solution polymerization process in at least one reactor; wherein said polyethylene composition is characterized by one or more of the following properties: a melt index, I2, measured according to ASTM D 1238 (2.16 kg @ 190° C.), from 0.1 to 5 g/10 min; density, measured according to ASTM D-792, from 0.910 to 0.935 g/cc; melt flow ratio, I10/I2, wherein I10 is measured according to ASTM D1238 (10 kg @ 190° C.), from 6 to 7.4; and molecular weight distribution, (Mw/Mn) from 2.5 to 3.5 are provided. Also provided are articles made from the mono- and/or multi-layer films.
Abstract:
The invention provides a composition comprising the following: A) a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)
Abstract:
Embodiments disclosed herein include multilayer cast films having a first outer layer, a core layer, and a second outer layer, wherein the first outer layer comprises (a) a linear low density polyethylene (LLDPE), ultra-low density polyethylene (ULDPE), a first polyethylene composition, or combinations of two or more thereof, and (b) polyisobutylene, and the core layer comprises a core layer polyethylene composition.
Abstract:
Disclosed herein is a blown film comprising at least 50 wt. % of a polyethylene composition comprising the reaction product of ethylene and optionally, one or more alpha-olefin comonomers, wherein the polyethylene composition is characterized by the following properties: a melt index, I2, of from 0.1 to 2 g/10 min; a density of from 0.940 to 0.970 g/cm3; a melt flow ratio, I10/I2, of from 5.5 to 7.2; and a molecular weight distribution (Mw/Mn) of from 2.2 to 3.5.
Abstract:
Functionalized ethylene-based polymers are prepared by a process comprising the step of reacting a first composition comprising an ethylene-based polymer with at least the following: (A) at least one carbon-carbon (C—C) free radical initiator of Structure I: wherein R1, R2, R3, R4, R5 and R6 are each, independently, hydrogen or a hydrocarbyl group; and wherein, optionally, two or more R groups (R1, R2, R3, R4, R5 and R6) form a ring structure; and with the provisos that (i) at least one of R2 and R5 is a hydrocarbyl group of at least two carbon atoms, and (ii) at least one of R3 and R6 is a hydrocarbyl group of at least two carbon atoms; and (B) at least one free radical initiator other than the carbon-carbon (C—C) free radical initiator of Structure I (a non-C—C free radical initiator), e.g., a peroxide; and (C) at least one functionalization agent, e.g., maleic anhydride.
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)
Abstract:
The invention provides an ethylene-based polymer comprising the following properties: a) weight fraction (w) of molecular weight above 5*106 g/mol, w>A−B*I2, where A=0.4 wt %, and B is 0.02 wt %/(dg/min), and w D−E*log(I2), where D=162 Pa and E=52 Pa/log(dg/min).
Abstract:
The invention provides an ethylene-based polymer comprising the following properties: a) weight fraction (w) of molecular weight above 5*106 g/mol, w>A−B*I2, where A=0.4 wt %, and B is 0.02 wt %/(dg/min), and w D−E*log(I2), where D=162 Pa and E=52 Pa/log(dg/min).
Abstract:
The invention provides a process to form an ethylene-based polymer, said process comprising polymerizing ethylene in presence of at least the following: A) a free-radical agent; B) an alkylated phenol selected from Formula (I), wherein R1, R2,R3, R4 and R5 are each, independently, hydrogen or an alkyl; and C) a “metal alkyl-containing compound” selected from the group consisting of the following: i) at least one “Group II metal alkyl-containing compound,” ii) at least one “Group III metal alkyl-containing compound,” and iii) a combination of i) and ii).