MECHANICALLY STABILIZED POLYAZOLES COMPRISING AT LEAST ONE POLYVINYL ALCOHOL
    6.
    发明申请
    MECHANICALLY STABILIZED POLYAZOLES COMPRISING AT LEAST ONE POLYVINYL ALCOHOL 有权
    包含至少一种聚乙烯醇的机械稳定聚对苯二甲酸

    公开(公告)号:US20120289654A1

    公开(公告)日:2012-11-15

    申请号:US13467485

    申请日:2012-05-09

    Abstract: A process for preparing mechanically stabilized polyazoles, comprising the following steps: I) treating at least one polyazole having at least one amino group in a repeat unit with a solution comprising (i) at least one strong acid and (ii) at least one stabilizing reagent, the total content of stabilizing reagents in the solution being in the range from 0.01 to 30% by weight, II) performing the stabilization reaction directly and/or in a subsequent processing step by heating to a temperature greater than 25° C., the stabilizing reagent used being at least one polyvinyl alcohol. The polyazoles thus obtainable are notable especially for a high conductivity and a very good mechanical stability. They are therefore especially suitable for applications in fuel cells.

    Abstract translation: 一种制备机械稳定化的多唑的方法,包括以下步骤:I)用包含(i)至少一种强酸和(ii)至少一种稳定的酸的溶液,在重复单元中处理至少一种具有至少一个氨基的聚唑 试剂,溶液中稳定试剂的总含量在0.01至30重量%的范围内,II)直接和/或在随后的加工步骤中通过加热至大于25℃的温度进行稳定化反应, 使用的稳定剂为至少一种聚乙烯醇。 因此获得的聚唑特别是对于高导电性和非常好的机械稳定性而言尤其如此。 因此,它们特别适用于燃料电池中的应用。

    METHOD FOR THE SYNTHESIS OF A POLYOXADIAZOLE POLYMER
    9.
    发明申请
    METHOD FOR THE SYNTHESIS OF A POLYOXADIAZOLE POLYMER 失效
    合成聚氧杂二唑聚合物的方法

    公开(公告)号:US20090203870A1

    公开(公告)日:2009-08-13

    申请号:US12369133

    申请日:2009-02-11

    Abstract: A polyoxadiazole polymer is synthesized by heating polyphosphoric acid to a temperature of at least about 160° C. and making a solution by mixing hydrazine sulfate salt with one or more dicarboxylic acids or their derivatives in the heated polyphosphoric acid. The solution is heated under an inert gas atmosphere and the polymer is precipitated in a basic solution. The polyoxadiazole polymer can be produced as a homopolymer or copolymer, and may be used to produce a membrane or fibers.

    Abstract translation: 通过将多磷酸加热到至少约160℃的温度并通过将肼硫酸盐与一种或多种二羧酸或其衍生物在加热的多磷酸中混合而制备溶液来合成聚恶二唑聚合物。 将溶液在惰性气体气氛下加热,并将聚合物在碱性溶液中沉淀。 聚二恶唑聚合物可以作为均聚物或共聚物制备,并且可用于制备膜或纤维。

    POLYBENZOXAZOLE-FILLED NITRILE BUTADIENE RUBBER COMPOSITIONS, ARTICLES INCORPORATING THE SAME, AND A METHOD OF INSULATING A ROCKET MOTOR WITH THE SAME
    10.
    发明申请
    POLYBENZOXAZOLE-FILLED NITRILE BUTADIENE RUBBER COMPOSITIONS, ARTICLES INCORPORATING THE SAME, AND A METHOD OF INSULATING A ROCKET MOTOR WITH THE SAME 失效
    聚苯并噻唑填充的丁二烯橡胶组合物,包含它们的制品以及使用该绝缘材料绝缘的电动机的方法

    公开(公告)号:US20070254988A1

    公开(公告)日:2007-11-01

    申请号:US11207855

    申请日:2005-08-18

    CPC classification number: C08L9/02 C08K7/02 C08L79/06 C08L2666/20

    Abstract: An insulation composition that comprises at least one nitrile butadiene rubber (“NBR”) having an acrylonitrile content that ranges from approximately 26% by weight to approximately 35% by weight and polybenzoxazole (“PBO”) fibers. The NBR may be a copolymer of acrylonitrile and butadiene and may be present in the insulation composition in a range of from approximately 45% by weight to approximately 56% by weight of a total weight of the insulation composition. The PBO fibers may be present in a range of from approximately 3% by weight to approximately 10% by weight of a total weight of the insulation composition. A rocket motor including the insulation composition and a method of insulating a rocket motor are also disclosed.

    Abstract translation: 一种绝缘组合物,其包含至少一种丙烯腈含量为约26重量%至约35重量%的丁腈橡胶(“NBR”)和聚苯并恶唑(“PBO”)纤维。 NBR可以是丙烯腈和丁二烯的共聚物,并且可以以绝热组合物的总重量的约45重量%至约56重量%的范围存在于绝缘组合物中。 PBO纤维可以以绝热组合物的总重量的约3重量%至约10重量%的范围存在。 还公开了包括绝缘组合物的火箭发动机和绝热火箭发动机的方法。

Patent Agency Ranking