摘要:
This disclosure describes a process for strengthening, by ion-exchange, the edges of an article separated from a large glass sheet after the sheet has been ion-exchanged to strengthen by exposing only the one or a plurality of the edges of the separated article to an ion-exchange medium (for example without limitation, a salt, paste, frit, glass) while the glass surface is maintained at temperatures less than 200° C.
摘要:
Tungsten-titanium-phosphate materials and methods of making and using the same. The Tungsten-titanium-phosphate materials comprise about 20 to 60 actual mol % WO3, about 10 to 40 actual mol % TiO2, and about 15 to 40 actual mol % P2O5
摘要:
This disclosure describes a process for strengthening, by ion-exchange, the edges of an article separated from a large glass sheet after the sheet has been ion-exchanged to strengthen by exposing only the one or a plurality of the edges of the separated article to an ion-exchange medium (for example without limitation, a salt, paste, frit, glass) while the glass surface is maintained at temperatures less than 200° C.
摘要:
An optical member comprising OD-doped silica glass, optionally doped with fluorine. The optical member is particularly advantageous for use in connection with radiation having a wavelength shorter than about 248 nm. In certain embodiments the optical member can be advantageously used for wavelength as short as about 157 nm.
摘要:
Disclosed are high purity synthetic silica material having an internal transmission at 193 nm of at least 99.65%/cm and method of preparing such material. The material is also featured by a high compositional homogeneity in a plane transverse to the intended optical axis. The soot-to-glass process for making the material includes a step of consolidating the soot preform in the presence of H2O and/or O2.
摘要翻译:公开了具有193nm以上的内透射率为至少99.65%/ cm 3的高纯度合成二氧化硅材料及其制备方法。 该材料的特征还在于横向于预期光轴的平面中具有高的组成均匀性。 用于制造该材料的烟灰 - 玻璃工艺包括在H 2 O和/或O 2存在下固化烟灰预制件的步骤。
摘要:
An optical member comprising OD-doped silica glass, optionally doped with fluorine. The optical member is particularly advantageous for use in connection with radiation having a wavelength shorter than about 248 nm. In certain embodiments the optical member can be advantageously used for wavelength as short as about 157 nm.
摘要:
The present invention is a method of making a lithography photomask and photomask blank. The method of making the lithography photomask and photomask blank includes providing a silicon oxyfluoride glass tube having an OH content less than 50 ppm. The method further includes cutting the silicon oxyfluoride glass tube, flattening the silicon oxyfluoride glass tube, and forming the flattened cut silicon oxyfluoride glass tube into a photomask blank having a planar surface. The present invention includes a glass lithography mask preform. The glass lithography mask preform is a longitudinal silicon oxyfluoride glass tube that has an OH content ≦10 ppm, a F wt. % concentration ≧0.5 wt. %.
摘要:
Glass interposer panels and methods for forming the same are described herein. The interposer panels include a glass substrate core formed from an ion-exchangeable glass. A first layer of compressive stress may extend from a first surface of the glass substrate into the thickness T of the glass substrate core to a first depth of layer D1. A second layer of compressive stress may be spaced apart from the first layer of compressive stress and extending from a second surface of the glass substrate core into the thickness T of the glass substrate core to a second depth of layer D2. A plurality of through-vias may extend through the thickness T of the glass substrate core. Each through-via is surrounded by an intermediate zone of compressive stress that extends from the first layer of compressive stress to the second layer of compressive stress adjacent to a sidewall of each through-via.
摘要:
Strengthened glass substrate sheets and methods of fabricating glass panels from glass substrate sheets are disclosed. In one embodiment, a method includes forming at least one series of holes through a thickness of the glass substrate sheet, wherein the at least one series of holes defines a perimeter of the glass panel to be separated from the glass substrate sheet. The method further includes strengthening the glass substrate sheet by a strengthening process, and separating the glass panel from the glass substrate sheet along the at least one series of holes. At least a portion of one or more edges of the glass panel has an associated edge compressive layer. In another embodiment, a strengthened glass substrate sheet includes at least one series of holes that defines a perimeter of one or more glass panels to be separated from the strengthened glass substrate sheet.
摘要:
A fused silica glass having a refractive index homogeneity of less or equal to about 5 ppm over an aperture area of at least about 50 cm2. The fused silica glass is also substantially free of halogens and has an adsorption edge of less than about 160 nm. The glass is dried by exposing a silica soot blank to carbon monoxide before consolidation, reducing the combined concentration of hydroxyl (i.e., OH, where H is protium (11H) and deuteroxyl (OD), where D is deuterium (12H)) of less than about 20 ppm by weight in one embodiment, less than about 5 ppm by weight in another embodiment, and less than about 1 ppm by weight in a third embodiment.