Abstract:
A birefringent film with excellent uniformity in in-plane retardation, retardation in the thickness direction, and alignment axis is provided. The birefringent film is produced in such a manner that, in the step of stretching a polymer film, the polymer film is stretched in a width direction while being shrunk in a longitudinal direction, and assuming that lengths in the width direction and the longitudinal direction of the polymer film before being stretched are 1, a change ratio (STD) of the length in the width direction of the polymer film resulting from the stretching and a change ratio (SMD) of the length in the longitudinal direction of the polymer film resulting from the shrinking satisfy the following formula (1). (1/STD)1/2≦SMD
Abstract:
The method of cleaning a coated sheet according to the present invention is characterized in that dry wind is brown along the traveling direction of a film onto the surface of a coating layer wherein the solid content and the viscosity of the coating solution are within specified ranges. By this method, the thickness precision of the coating film can be improved in its large area, and the evenness of its in-plane optically functional property can be made even therein. The speed of the dry wind, the temperature of the wind, and the thickness of the dried coating film are preferably within specified ranges. In particular, the coated sheet is very useful as an optical material having good properties in an optically functional layer which is frequently used as a large-area coated sheet, an optical device having such an optically functional layer, an optically compensating layer, or an optically compensating plate. The coated sheet is particularly effective for an image display on which they are mounted.
Abstract:
A transparent protective film for polarizing plate being provided via an adhesive layer on at least one surface of a polarizer, wherein a ratio of constituent elements (oxygen ratio/carbon ratio) on the polarizer-adhering surface of the transparent protective film for polarizing plate, which is determined by X-ray photoelectron spectrometry, is larger than 0.75 has facilitate adhesion surface and no deformation without problems attributable to saponification.
Abstract:
A polarizing film comprising a polarizer (A) and a protection film (B) prepared on at least one face of the polarizer (A), wherein the protection film (B) is adhered to the polarizer (A) without using adhesives, is induced problems by use of adhesives.
Abstract:
An oriented film of polyvinyl alcohol derived film with reduced stretch irregularity and uniform orientation in a wide range of a stretching ratio is obtained by a manufacturing method for an oriented film, comprising the steps of: contacting a non-stretched film, comprising polyvinyl alcohols or derivatives thereof, with moisture percentage adjusted to no more than 10%, to at least one heating roll currently driven and heating the film at no less than 70° C.; subsequently giving a tension and stretching using a peripheral velocity difference between the heating roll concerned and a stretch roll in a position ahead of said heating roll in a running direction of the film.
Abstract:
A polarizer comprising a polyvinyl alcohol based film being dyed by iodine and treated with potassium iodide, wherein an element content ratio (K/I) of iodine (I) and potassium (K) is 0.05 through 0.24, show an effect controlling coloring and satisfying high durability under conditions of high temperature.
Abstract:
A thin polarizing plate is disclosed that includes a polarizer, a protective layer formed on at least one side of the polarizer, and a pressure sensitive adhesive layer formed on the protective layer, wherein the thickness A of the polarizer, the thickness B of the protective layer, the modulus of elasticity C of a pressure sensitive adhesive of the pressure sensitive adhesive layer, a numerical value 1 and a numerical value 2 satisfy the following relationships: (numerical value 1)=B/A
Abstract translation:公开了一种薄偏振片,其包括偏振器,形成在偏振器的至少一侧上的保护层和形成在保护层上的压敏粘合剂层,其中偏振器的厚度A,保护层的厚度B 层数,压敏粘合剂层的压敏粘合剂的弹性模量C,数值1和数值2满足以下关系:(数值1)= B / A <2.0(数值2)= (数值1)/℃<20,通过提供薄且轻的偏振片。 还公开了使用所述偏振片的薄且轻的液晶显示器。
Abstract:
The present invention pertains to a method of fabricating a polarizing film by uniaxially stretching a resin film such as a polyvinyl alcohol-based film in a fabrication process including a swelling step and a dyeing step following the swelling step, comprising the steps of immersing a resin film in bath liquids in at least two or more swelling baths in sequence in the above-mentioned swelling step, wherein at least a bath temperature of a swelling bath located at a Nth position from the front-stage side is set at a temperature which is higher than a bath temperature of a swelling bath located at a (N+M)th position by 3° C. or more (both N and M are specified positive integers).
Abstract:
A method for producing a multilayer laminated film comprising: laminating a resin film having a moisture percentage of 10% by weight to 60% by weight with a first transparent film and a second transparent film each having a moisture percentage of 0.5% by weight to 5% by weight to be bonded to both sides of the resin film through an adhesive or pressure-sensitive adhesive layer interposed therebetween; wherein the laminating comprising steps of: passing the resin film and the first transparent film between a pair of a first metal roll and a first elastic roll in such a manner that the first transparent film is placed on the first metal roll side so that they are bonded to each other under pressure to form a laminated film; and then, using the laminated film without winding up it and passing the laminated film and the second transparent film between a pair of a second metal roll and a second elastic roll in such a manner that the second transparent film is placed on the second metal roll side so that they are bonded to each other under pressure to form a multilayer laminated film. The method can prevent bubbles from being formed between the resin film and the transparent film.
Abstract:
A method for manufacturing a coated sheet that may form a coated layer having a uniform film thickness by a coating liquid even when a substrate has a large area is provided.A method for manufacturing a coated sheet to form a coated layer by a process including a process (1) for coating a coating liquid including a resin material and a solvent on a substrate, and a drying process (2) for drying a coated liquid, wherein a drying is performed under drying wind flow having an average wind speed of 10 m/s or less until a viscosity of the coated liquid in the drying process (2) reaches at least 50 [mPa·s] at drying temperatures.