摘要:
The present disclosure provides for a bicomponent fiber that includes a first region formed of a condensation polymer and a second region formed from a polyethylene blend. The polyethylene blend includes (i) an ethylene-based polymer having a density of 0.920 g/cm3 to 0.970 g/cm3 and a melt index, I2, as determined by ASTM D1238 at 190° C. and 2.16 kg of 0.5 to 150 g/10 minutes; (ii) a maleic anhydride-grafted polyethylene; and (iii) an inorganic Brønsted-Lowry acid having an acid strength pKa value at 25° C. of 1 to 6.5, wherein the polyethylene blend has a 0.03 to 0.5 weight percent of grafted maleic anhydride based on the total weight of the polyethylene blend. The first region is a core region of the bicomponent fiber and the second region is a sheath region of the bicomponent fiber, where the sheath region surrounds the core region.
摘要:
The present invention is directed to a polypropylene composition (P) comprising a bimodal copolymer of propylene and 1-hexene prepared in the presence of a metallocene catalyst, said bimodal copolymer having a melt flow rate MFR2 in the range of 4.0 to 20.0 g/10 min. Further, the present invention is directed to a method for preparing the copolymer (C) and an article comprising said polypropylene composition (P).
摘要:
In an embodiment, a thermoplastic vulcanizate (TPV) composition is provided. The TPV composition includes a thermoplastic polyolefin; and an ethylene based copolymer rubber, wherein the ethylene based copolymer rubber has: a Mw of from 500,000 g/mol to 3,000,000 g/mol, a Mw/Mn of 4.0 or lower, and a g′vis of 0.90 or greater. In another embodiment, a TPV composition includes a thermoplastic phase and an ethylene-propylene-diene terpolymer, wherein the thermoplastic vulcanizate composition has: a hardness of from 20 Shore A to 60 Shore D; and a stress relaxation slope of −1 to −5 (l/min) as measured by an Elastocon stress relaxation instrument.
摘要:
A composition for foam molding including: a component (A): an olefin-based polymer; a component (B): a styrene block copolymer having no chemical-bond cross-linking moiety; a component (C): a process oil; and a component (D): a foaming agent, wherein a content of the component (A) relative to a total mass of the component (A) and the component (B) is 5 to 36% by mass, and a content of the component (C) relative to 100 parts by mass of the total mass of the component (A) and the component (B) is 160 to 350 parts by mass.
摘要:
A thermoplastic starch composition acquired from compounding a mixture comprises starch-containing agricultural waste in 45 to 70% by weight of total composition that the agricultural waste contains starch content less than 50% in dry weight; thermoplastic synthetic polymer in 25 to 50% by weight of total composition; plasticizer in 1 to 10% by weight of total composition; and coupling agent in 1 to 5% by weight of total composition; wherein the compounding is performed at a first temperature which is higher than room temperature.
摘要:
Provided is a pneumatic tire which has low air permeability and undergoes a small change in air permeability due to fatigue. A pneumatic tire of the present invention contains a layer which is formed of a thermoplastic elastomer composition that is composed of (A) a modified ethylene-vinyl alcohol copolymer to which an aliphatic polyester is grafted, (B) a polyamide resin and (C) a modified rubber having an acid anhydride group or an epoxy group.
摘要:
Embodiments of the present invention are directed to compositions and methods for a thermoplastic paving composition including an asphalt rubber binder and a polyethylene polymer additive.
摘要:
A thermoplastic starch composition acquired from compounding a mixture comprising starch-containing agricultural byproducts in 45 to 70% by weight of total composition, the agricultural byproducts having a starch content less than 50% dry weight; thermoplastic synthetic polymer in 25 to 50% by weight of total composition; plasticizer in 1 to 10% by weight of total composition; and coupling agent in 1 to 5% by weight of total composition; the compounding performed at a first temperature which is higher than room temperature.
摘要:
An adhesion composition comprising a) a first polymer that is selected from the group consisting of acrylic polymers, acrylonitrile butadiene, butyl rubber, cellulose acetate, cellulose butyrate, epoxy resins, ethylene vinyl acetate, natural rubber, neoprene, phenolic polymers, polyurethanes, polyvinyl acetate, polyvinyl alcohol, styrene butadiene rubber, casein, dextrin, starch, copolymers thereof and combinations thereof; b) a second polymer selected from the group consisting of ethylene-acrylic acid copolymer, oxidized polyethylene, oxidized ethylene-vinyl acetate copolymer, maleated polyolefin and combinations thereof; and c) a surfactant; where the composition is water-based, having a solids content of greater than about 30% based on the total weight of the composition, with a particle size of about 10 nm to about 2000 nm, and is adapted for adhesion to substrates; and where the first and second polymers are different. The adhesion composition can also comprise a tackifier resin selected from the group consisting of rosin ester resin, rosin acid resin, synthetic hydrocarbon resin, synthetic terpenic resin and combinations thereof. Applications of the composition are also disclosed.
摘要:
A phenol resin molding material of the present invention includes a modified olefin-based polymer particle (I) and a phenol resin (II). Furthermore, it is preferable that the above-described modified olefin-based polymer particle (I) satisfy at least one of the following requirements (A), (B), and (C). (A) Inclusion of at least one element selected from a group consisting of a group 15 element, a group 16 element, and a group 17 element of the periodic table. (B) When the whole of the above-described olefin-based polymer particle (I) is set as 100 wt %, the content of the above-described elements is greater than or equal to 0.05 wt % and less than or equal to 50 wt %. (C) MFR which is measured under the conditions of 190° C. and 2.16 kgf based on JIS K 7210 is greater than or equal to 0.001 g/10 minutes and less than 3 g/10 minutes.