摘要:
The invention relates to compositions containing polycarbonate and defined quantities of a triazine, and to the production and use thereof for producing moulded parts, in particular optical quality sheets and tubes, according to an extrusion method
摘要:
A process for extracting phenol from a phenol-containing aqueous solution is disclosed. The process entails contacting the aqueous solution with an extracting agent that comprise a mixture of 60 to 99% of methyl isobutyl ketone, 1 to 40% of anisole and 0 to 20% of mesitylene.
摘要:
The present invention relates to compositions containing flame retardant polycarbonate, which are suitable for producing flame-resistant milk-white colored plates. The composition contains polycarbonate, 0.10 to 4.00 weight percent of an acrylate-based scattering additive, 0.50 to 5.00 weight percent of an aromatic-aliphatic polyester, and 0.50 to 8.00 weight percent of a phosphorus-based flame retardant.
摘要:
A sheet containing a base layer containing polycarbonate and a flame retardant, wherein the flame retardant contains a compound of formula 1 wherein R1, R2, R3 and R4, represents an optionally halogen-substituted C1-C8 alkyl, C5-C6 cycloalkyl, C6-C10 aryl or C7-C12 aralkyl, R5 and R6, represents a C1-C4 alkyl, and Y represents a C1-C7 alkylidene, C1-C7 alkylene, C5-C12 cycloalkylidene, —O—, —S—, —SO—, —SO2—, —CO— or a residue of formula (2) or (3) wherein Z represents carbon and R21 and R22 can be selected for each Z individually and, represent hydrogen or C1-C6 alkyl, with the proviso that, on at least one Z atom, R21 and R22 are simultaneously alkyl and wherein the polycarbonate comprises a mixture of linear and branched polycarbonate and wherein the linear polycarbonate content is at least 40 wt. %, based on the total polycarbonate weight.
摘要:
The present invention relates to a polymer composition containing polycarbonate with a weight-average molecular weight Mw of from 24,000 to 33,000 and 5.0 wt. % to 20.0 wt. % (based on the total amount of the composition) of glass hollow spheres with an alkalinity of less than 1.0 meq/g. The present invention furthermore provides coextruded sheets in which the coextruded layer contains this polymer composition, and shaped articles produced therefrom, in particular containers and pieces of luggage, very particularly suitcases. Sheets which are obtainable with the polymer composition according to the invention have a high mechanical stability, a high scratch resistance, pleasant haptic properties and an excellent homogeneous external visual impression. The present invention furthermore relates to a process for the preparation of these polymer compositions and a process for production of the sheets according to the invention.
摘要:
Disclosed is a composition comprising polycarbonate and from 0.0001 weight % to 0.1000 weight % of 2-(2,4-dihydroxy)phenyl-4,6-di(4-phenyl)phenyl-1,3,5-triazine.
摘要:
The present invention relates to compositions containing flame retardant polycarbonate, which are suitable for producing flame-resistant milk-white coloured plates.
摘要:
The present invention relates to compositions which contain flame-retardant polycarbonate and are suitable for the production of flame-resistant and milky-white sheets.
摘要:
The invention describes a process for producing bisphenol with a content of less than 15 wt. % of phenol, wherein a suspension crystallisation of a product mixture containing bisphenol A, minor components and phenol is performed in a crystalliser, the product mixture being pumped through a heat exchanger. Due to deposition (fouling, i.e. crystallisation and deposition on the surface of the heat exchangers) in the heat exchanger, the pressure difference increases from 0.5 to 3 bar across the heat exchanger. The resulting reduced flow rate, which would lead to increased fouling in the crystalliser, is offset by continuously increasing the speed of the pump, the pump speed being regulated in such a way that the current consumption of the pump is maintained such that it fluctuates by a maximum of 5%.
摘要:
A process for the preparation of high purity bisphenol A is disclosed. The multi-step process entails a process whereby bisphenol A of a purity of preferably at least 99.8% can be obtained.