摘要:
A ceramic material powder for a translucent ceramic is molded with a binder, and the resulting green compact is embedded in a ceramic powder having the same composition with the ceramic material powder. After removing the binder, the green compact embedded in the ceramic powder is fired in an atmosphere having an oxygen concentration higher than that in the removal procedure of the binder and thereby yields a translucent ceramic represented by Formula I: Ba{(SnuZr1-u)xMgyTaz}vOw, Formula II: Ba(ZrxMgyTaz)vOw or Formula III: Ba{(SnuZr1-u)xZntMg1-t)yNbz}vOw. The translucent ceramic has a refractive index of 1.9 or more and is paraelectric.
摘要翻译:用粘合剂将用于半透明陶瓷的陶瓷材料粉末模制,并将所得的生坯压坯与陶瓷材料粉末嵌入具有相同组成的陶瓷粉末中。 在除去粘合剂之后,将包埋在陶瓷粉末中的生坯在氧浓度高于粘合剂的除去程度的气氛中焙烧,从而得到由式I表示的半透明陶瓷:Ba {(Sn u 1 1 1 x u> 式II:Ba(Zr x Si y Ta z z)z H z, 或者式III:Ba({(Sn≡Z1)≡Z> w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w w SUB>。 半透明陶瓷的折射率为1.9以上,为顺电性。
摘要:
A piezoelectric ceramic composition that is based on a layered bismuth compound composed of Sr, Bi, Nb, oxygen, contains an additional monovalent metallic element. The piezoelectric ceramic composition has an elevated Curie point, is highly reliable at higher temperatures, that is, minimizes the reduction in the piezoelectric effect, and is useful as a material for piezoelectric ceramic devices that contain little or no lead or lead compounds. The layered bismuth compound contains not more than about 0.125 mol and more than 0 mol of the monovalent metallic element for 1 mol of Nb.
摘要:
A laminated sintered body is produced having a ceramic porous body 8 having a thickness of 300 nullm or larger and a ceramic dense body 9 having a thickness of 25 nullm or smaller. A green body 5 for the porous body and a green body 3 for the dense body is laminated to obtain a laminate, which is then subjected to pressure molding by cold isostatic pressing to obtain a pressure molded body 6. The pressure molded body 6 is sintered to obtain a laminated sintered body. Alternatively, it is provided a laminated sintered body has a ceramic porous body having a thickness of 300 nullm or larger and a ceramic dense body having a thickness of 25 nullm or smaller. By reducing the leakage rate of helium gas of the laminated sintered body to 10null6 Panullm3/s or lower, the operational efficiency of the cell can be improved, and the deterioration of the cell can be prevented to improve an output after the cell is subjected to initiation and termination cycle test of operation.
摘要翻译:制造具有厚度为300μm以上的陶瓷多孔体8和厚度为25μm以下的陶瓷致密体9的层叠烧结体。 将用于多孔体的生坯体5和用于致密体的生坯体3层压以获得层压体,然后通过冷等静压进行加压成型,得到加压成形体6.将加压成形体6烧结 得到层叠烧结体。 或者,提供一种层叠烧结体,其具有厚度为300μm以上的陶瓷多孔体和厚度为25μm以下的陶瓷致密体。 通过将层叠烧结体的氦气的泄漏率降低至10 -6 Pa / m 3以上,能够提高电池的运转效率,能够防止电池的劣化 在电池进行启动和终止循环测试后,改善输出。
摘要:
A method of manufacturing a joint between metal and a ceramic substrate for a high temperature sensor. First, a predetermined hole is formed in the ceramic substrate to serve as a joint portion. A bonding layer is preferably disposed on the ceramic substrate to form on the inner surface and the surrounding portion of the hole. Next, the hole is filled with a supporting metal. Then, a conductive layer is formed on the supporting metal and the bonding layer. A metal signal conductive frame is then formed on the conductive layer. Next, a welding spot is formed through the metal signal conductive frame, the conductive layer and the supporting metal at the joint portion by a welding process.
摘要:
A ceramic material powder for a translucent ceramic is molded with a binder, and the resulting green compact is embedded in a ceramic powder having the same composition with the ceramic material powder. After removing the binder, the green compact embedded in the ceramic powder is fired in an atmosphere having an oxygen concentration higher than that in the removal procedure of the binder and thereby yields a translucent ceramic represented by Formula I: Banull(SnuZr1-u)xMgyTaznullvOw, Formula II: Ba(ZrxMgyTaz)vOw or Formula III: Banull(SnuZr1-u)xZntMg1-t)yNbznullvOw. The translucent ceramic has a refractive index of 1.9 or more and is paraelectric.
摘要:
A multilayered microfluidic device having a substantially monolithic structure is formed by sintering together a plurality of green-sheet layers. The substantially monolithic structure has an inlet port for receiving fluid, an outlet port for releasing fluid, and an interconnection between the inlet port and the outlet port. The substantially monolithic structure may also include a variety of components to enable useful interaction with the fluid, such as electrically conductive pathways, heaters, fluid sensors, fluid motion transducers, and optically transmissive portions. The components are preferably fabricated using thick-film or green-sheet technology and are preferably co-fired with and sintered to the green-sheet layers to become integral with the substantially monolithic structure.
摘要:
A micro-gas chromatograph column is formed by texturing a channel into a plurality of green-sheet layers, which are then sintered together to form a substantially monolithic structure. A thick-film paste may be added to the channel textured in the green-sheet layers to provide a porous plug sintered in the micro-gas chromatograph column in the substantially monolithic. A thermal conductivity detector is formed in the substantially monolithic structure by depositing a conductive thick-film paste on the surface of one of the green-sheet layers to define a resistor in an exit channel of the micro-gas chromatograph column.
摘要:
A motor (17a, 17b) opens and closes a shutter turnably mounted so as to open and close a discharge port relevant to a hopper, and generates a torque against a load in a gravity direction of materials dropped from a material supply mechanism to the hopper. A shutter control portion (19a, 19b, . . . 19h) sets a hold current applied to the motor from the start of loading relevant to the shutter caused by the materials to be dropped to a predetermined period, to a first hold current value for applying to the shutter a torque sufficient to bear the shock during charge of the materials. In addition, the control portion sets a hold current applied to the motor from an elapse of the predetermined period after reception of the materials by the hopper to the start of discharging the materials from a discharge port of the hopper, to a second hold current value that is smaller than the first hold current value, the second hold current value applying to the shutter a torque against a force released downwardly under a load in the gravity direction of the materials.
摘要:
An extended life fluorescent polyvinyl chloride sheeting and a method for forming the sheeting are disclosed. The sheeting includes a polyvinyl chloride film having a fluorescent colorant incorporated therein. A protective polymer layer is attached to the polyvinyl chloride film. A light filtering agent is incorporated into the protective layer, wherein the filter agent blocks the 425 nm and lower wavelengths of the visible spectrum.
摘要:
An extended life fluorescent polyvinyl chloride sheeting and a method for forming the sheeting are disclosed. The sheeting includes a polyvinyl chloride film having a fluorescent colorant incorporated therein. A protective polymer layer is attached to the polyvinyl chloride film. A light filtering agent is incorporated into the protective layer, wherein the filter agent blocks the 425 nm and lower wavelengths of the visible spectrum.