摘要:
This method for estimating the depth of latent scratches in SiC substrates includes an etching step, a measurement step, and an estimation step. In the etching step, a SiC substrate in which at least the surface is formed from single crystal SiC, and which has been subjected to machining, is subjected to heat treatment under Si atmosphere to etch the surface of the SiC substrate. In the measurement step, the surface roughness or the residual stress of the SiC substrate which has been subjected to the etching step is measured. In the estimation step, the depth of latent scratches or the presence or absence of latent scratches in the SiC substrate before the etching step are estimated on the basis of the results obtained in the measurement step.
摘要:
The present invention is to provide a storing container wherein Si does not drop onto a single crystal SiC substrate, and Si pressure distribution in an internal space can be made uniform. This storing container stores therein a single crystal SiC substrate to be etched by means of a heat treatment under Si vapor pressure. The storing container is formed of a tantalum metal, and has a tantalum carbide layer provided on an internal space side, and a tantalum silicide layer provided on the side further toward the internal space side than the tantalum carbide layer. The tantalum silicide layer supplies Si to the internal space. Furthermore, the tantalum silicide layer is different from adhered Si, and does not melt and drop.
摘要:
This method for estimating the depth of latent scratches in SiC substrates includes an etching step, a measurement step, and an estimation step. In the etching step, a SiC substrate in which at least the surface is formed from single crystal SiC, and which has been subjected to machining, is subjected to heat treatment under Si atmosphere to etch the surface of the SiC substrate. In the measurement step, the surface roughness or the residual stress of the SiC substrate which has been subjected to the etching step is measured. In the estimation step, the depth of latent scratches or the presence or absence of latent scratches in the SiC substrate before the etching step are estimated on the basis of the results obtained in the measurement step.
摘要:
In a method for manufacturing a reformed SiC wafer 41 (a surface treatment method for a SiC wafer) having its surface that is reformed by processing an untreated SiC wafer 40 before formation of an epitaxial layer 42, the method includes a surface reforming step as described below. That is, the untreated SiC wafer 40 includes BPDs as dislocations parallel to an inside of a (0001) face, and TEDs. Property of the surface of the untreated SiC wafer 40 is changed so as to have higher rate in which portions having BPDs on the surface of the untreated SiC wafer 40 propagate as TEDs at a time of forming the epitaxial layer 42.
摘要:
Provided is a surface treatment method for a SiC substrate (40), the method being capable of controlling whether to generate a step bunching or the type of step bunching that is generated. In the surface treatment method in which the surface of the SiC substrate (40) is etched by heating the SiC substrate (40) under Si vapor pressure, an etching mode and an etching depth which are determined at least on the basis of an etching rate, are controlled to etch the SiC substrate (40), so that a surface pattern of the SiC substrate (40) after etching treatment is controlled.
摘要:
When a SiC substrate (40) after performing mechanical treatment is heat-treated under SiC atmosphere to etch the SiC substrate (40), the etching rate is controlled by adjusting the inert gas pressure around the periphery of the SiC substrate (40). As a result, when latent scratches or the like exist in the SiC substrate (40), the latent scratches or the like can be removed. Accordingly, the surface of the SiC substrate (40) does not become rough, even if epitaxial growth and heat treatment and the like are performed. This can manufacture high-quality SiC substrates.
摘要:
The present application aims to provide a surface treatment method that is able to accurately control the rate of etching a single crystal SiC substrate and thereby enables correct understanding of the amount of etching. In the surface treatment method, the single crystal SiC substrate is etched by a heat treatment performed under Si vapor pressure. At a time of the etching, inert gas pressure in an atmosphere around the single crystal SiC substrate is adjusted to control the rate of etching. Accordingly, correct understanding of the amount of etching is obtained.
摘要:
The present invention is to provide a storing container wherein Si does not drop onto a single crystal SiC substrate, and Si pressure distribution in an internal space can be made uniform. This storing container stores therein a single crystal SiC substrate to be etched by means of a heat treatment under Si vapor pressure. The storing container is formed of a tantalum metal, and has a tantalum carbide layer provided on an internal space side, and a tantalum silicide layer provided on the side further toward the internal space side than the tantalum carbide layer. The tantalum silicide layer supplies Si to the internal space. Furthermore, the tantalum silicide layer is different from adhered Si, and does not melt and drop.
摘要:
To provide a technique capable of improving performance and reliability of a semiconductor device. An n−-type epitaxial layer (12) is formed on an n-type semiconductor substrate (11), and a p+-type body region (14), n+-type current spreading regions (16, 17), and a trench. TR are formed in the n−-type epitaxial layer (12). A bottom surface B1 of the trench TR is located in the p+-type body region (14), a side surface S1 of the trench TR is in contact with the n+-type current spreading region (17), and a side surface S2 of the trench TR is in contact with the n+-type current spreading region (16). Here, a ratio of silicon is higher than a ratio of carbon in an upper surface T1 of the n−-type epitaxial layer (12), and the bottom surface B1, the side surface S1, and the side surface 32 of the trench. Furthermore, an angle θ1 at which the upper surface T1 of the n−-type epitaxial layer (12) is inclined with respect to the side surface S1 is smaller than an angle θ2 at which the upper surface T1 of the n−-type epitaxial layer (12) is inclined with respect to the side surface S2.
摘要:
A heat treatment container (1) is provided with support members (6) for supporting a disc-shaped SiC substrate (2), which is an object, at a time of an etching treatment of the SiC substrate (2). Each of the support members (6) has an inclined surface (6F) for supporting a lower surface end (2E) of the SiC substrate (2), the inclined surface being inclined so as to increasingly approach the centerline of the SiC substrate (2) going downward. More specifically, each of the support members (6) is formed in a conical shape with a diameter that increases going downward, and a conical surface which is the peripheral surface of each supporting member forms the inclined surface (6F). A vertically-middle section of the inclined surface (6F) contacts the lower surface end (2E) of the SiC substrate (2).