LIGHT EMITTING DEVICE
    2.
    发明公开

    公开(公告)号:US20230369547A1

    公开(公告)日:2023-11-16

    申请号:US18245334

    申请日:2021-08-20

    CPC classification number: H01L33/504 C09K11/646 C09K11/643 C09K11/0855

    Abstract: A light emitting device includes a light emitting element, and a fluorescent member including a phosphor. The light emitting device satisfies any of Condition (A): a correlated color temperature of light emission of the light emitting device is within a range of 4500 K or more and 7500 K or less, a content of a first phosphor is within a range of 29 mass % or more and 90 mass % or less, and a melanopic ratio is within a range of 1.0 or more and 1.4 or less; Condition (B): a correlated color temperature of light emission of the light emitting device is within a range of 2500 K or more and less than 4500 K, a content of a first phosphor is within a range of 25 mass % or more and 90 mass % or less, and a melanopic ratio is within a range of 0.7 or more and 1.1 or less; and Condition (C): a correlated color temperature of light emission of the light emitting device is within a range of 2500 K or more and 3000 K or less, a content of a first phosphor is within a range of 20 mass % or more and 90 mass % or less, and a melanopic ratio is within a range of 0.48 or more and 1.10 or less.

    Yellow light emitting phosphor and light emitting device package using the same
    6.
    发明授权
    Yellow light emitting phosphor and light emitting device package using the same 有权
    黄色发光荧光体和使用其的发光器件封装

    公开(公告)号:US09475987B2

    公开(公告)日:2016-10-25

    申请号:US14705620

    申请日:2015-05-06

    Abstract: Disclosed are phosphors and, more particularly, yellow light emitting phosphors and light emitting device packages using the same. The yellow light emitting phosphor includes a first phosphor including at least one of Lu3Al5O12:Ce, SrSi2O2N2, and β-type SiAlON and a second phosphor mixed with the first phosphor to form a mixture, the second phosphor including α-type SiAlON(Li-α-SiAlON) containing Li as a metal component, wherein the second phosphor emits light having a central wavelength in a range of 550 nm to 590 nm by being excited by near ultraviolet (UV) or blue light, The mixture of the first phosphor and the second phosphor is excited by the near UV or blue light to emit yellow light.

    Abstract translation: 公开了荧光体,更具体地,涉及使用其的黄色发光荧光体和发光器件封装。 黄色发光荧光体包括:包含Lu3Al5O12:Ce,SrSi2O2N2和β型SiAlON中的至少一种的第一荧光体和与第一荧光体混合形成混合物的第二荧光体,第二荧光体包括α型SiAlON(Li- α-SiAlON),其中第二荧光体通过被近紫外(UV)或蓝光激发而发射中心波长在550nm至590nm范围内的光。第一荧光体和 第二个磷光体被近紫外或蓝光激发,发出黄光。

    LIGHT-EMITTING DEVICE
    7.
    发明申请
    LIGHT-EMITTING DEVICE 审中-公开
    发光装置

    公开(公告)号:US20160149095A1

    公开(公告)日:2016-05-26

    申请号:US14899748

    申请日:2014-06-16

    Abstract: A light-emitting device (1) includes a substrate (2); a wiring pattern (3), an electrode land (4), a sealing resin layer (5), a wire (7), and a resin dam (9) that are disposed on the substrate (2); at least one light-emitting element (6) that emits light having a peak emission wavelength in a wavelength range of 430 to 480 nm; a green phosphor (10) that is excited by primary light emitted from the light-emitting element (6) to emit light having a peak emission wavelength in a green region; and a first red phosphor (11) that is excited by the primary light to emit light having a peak emission wavelength in a red region. The first red phosphor (11) emits no light in a wavelength range of 700 nm or more and absorbs no light in a wavelength range of 550 to 600 nm.

    Abstract translation: 发光装置(1)包括基板(2); 设置在基板(2)上的布线图案(3),电极接合区(4),密封树脂层(5),电线(7)和树脂阻挡件(9)。 发射波长范围为430〜480nm的峰值发光波长的光的至少一个发光元件(6); 绿色荧光体(10),其由从所述发光元件(6)发射的初级光激发,以发射具有绿色区域中的峰值发射波长的光; 以及由初级光激发以发射具有红色区域中的峰值发射波长的光的第一红色荧光体(11)。 第一红色荧光体(11)在700nm以上的波长范围内不发光,并且在550〜600nm的波长范围内不吸收光。

    METHOD FOR PRODUCING PHOSPHOR
    9.
    发明申请
    METHOD FOR PRODUCING PHOSPHOR 有权
    生产磷光体的方法

    公开(公告)号:US20150307353A1

    公开(公告)日:2015-10-29

    申请号:US14434162

    申请日:2013-02-22

    Abstract: Provided is a method for producing a phosphor, using a nitride raw material, that gives a high-reliability (Sr,Ca)AlSiN3-based nitride phosphor at a productivity higher than before.The method comprises a mixing step of mixing raw materials and a calcining step of calcining the mixture obtained in the mixing step and, in producing the phosphor having a crystalline structure substantially identical with that of (Sr,Ca)AlSiN3 crystal as the host crystal, a strontium nitride containing SrN, Sr2N, or the mixture thereof as the main crystalline phase, as determined by crystalline phase analysis by powder X-ray diffractometry, and having a nitrogen content of 5 to 12 mass % is used as part of the raw materials.

    Abstract translation: 提供一种使用氮化物原料制造以高于以前的生产率提供高可靠性(Sr,Ca)AlSiN 3的氮化物荧光体的荧光体的方法。 该方法包括混合原料的混合步​​骤和煅烧在混合步骤中获得的混合物的煅烧步骤,并且在制备具有与作为主晶体的(Sr,Ca)AlSiN 3晶体基本相同的晶体结构的荧光体时, 使用通过粉末X射线衍射的结晶相分析测定的含有5〜12质量%的氮含量的SrN,Sr 2 N或其混合物作为主要结晶相,作为原料的一部分 。