α+beta-type titanium alloy part and method of production of same
    1.
    发明授权
    α+beta-type titanium alloy part and method of production of same 有权
    α+β型钛合金零件及其制造方法

    公开(公告)号:US09187807B2

    公开(公告)日:2015-11-17

    申请号:US13513026

    申请日:2010-12-02

    IPC分类号: C22C14/00 C22F1/18

    摘要: A method of production of an α+β-type titanium alloy part for a motorcycle, car, or bicycle which has a high Young's modulus (rigidity) in the axial direction of the shaped product and a bolt, engine valve, or connecting rod made of an α+β-type titanium alloy and a method of production of the same, wherein an α+β-type titanium alloy is heated at the temperatures giving the β-single phase, then is uni-directionally hot rolled, the plate is machined so that a direction vertical to both the hot rolling direction and thickness direction (width direction) corresponds to the direction in which high rigidity is demanded in the finished part, that is, the axial direction of the bolt, engine valve, or connecting rod, and the X-ray diffraction intensities I(0002), I(10-10), and I(10-11), of the (0002) plane, (10-10) plane, and (10-11) plane of the titanium α-phase measured at the cross-sections vertical to the longitudinal axial direction of the parts satisfy I(0002)/[I(10-10)+I(10-11)]≧1.

    摘要翻译: 一种在成形制品的轴向上具有高杨氏模量(刚性)的摩托车,汽车或自行车的α+ / bgr型型钛合金部件的制造方法以及螺栓,发动机气门或连杆 由α+ / bgr型钛合金制成,其制造方法为α+ b型钛合金,在单相温度下加热,然后单向热轧 加工板,使得与热轧方向和厚度方向(宽度方向)垂直的方向对应于成品部件中要求高刚性的方向,即螺栓,发动机阀门的轴向方向 (10-10)面的X射线衍射强度I(0002),I(10-10)和I(10-11),(10-10)面和(10- 11)在垂直于部件的纵向轴向的横截面处测量的钛α相的面积满足I(0002)/ [I(10-10 )+ I(10-11)]≥1。

    Process for producing 2,3,3,3-tetrafluoropropene
    2.
    发明授权
    Process for producing 2,3,3,3-tetrafluoropropene 有权
    制备2,3,3,3-四氟丙烯的方法

    公开(公告)号:US09040760B2

    公开(公告)日:2015-05-26

    申请号:US13879668

    申请日:2011-10-27

    摘要: This invention provides a process for producing 2,3,3,3-tetrafluoropropene, the process comprising: (1) a first reaction step of reacting hydrogen fluoride with at least one chlorine-containing compound selected from the group consisting of a chloropropane represented by Formula (1): CClX2CHClCH2Cl, wherein each X is the same or different and is CI or F, a chloropropene represented by Formula (2): CClY2CCl═CH2, wherein each Y is the same or different and is CI or F, and a chloropropene represented by Formula (3): CZ2═CClCH2Cl, wherein each Z is the same or different and is CI or F in a gas phase in the absence of a catalyst while heating; and (2) a second reaction step of reacting hydrogen fluoride with a reaction product obtained in the first reaction step in a gas phase in the presence of a fluorination catalyst while heating. According to the process of this invention, 2,3,3,3-tetrafluoropropene (HFO-1234yf) can be obtained with high selectivity, and catalyst deterioration can be suppressed.

    摘要翻译: 本发明提供一种生产2,3,3,3-四氟丙烯的方法,该方法包括:(1)使氟化氢与至少一种选自以下的含氯化合物反应的第一反应步骤:选自由 式(1):CClX 2 CHClCH 2 Cl,其中每个X相同或不同,为Cl或F,式(2)表示的氯丙烯:CClY 2 CCl = CH 2,其中每个Y相同或不同,为Cl或F, 由式(3)表示的氯丙烯:CZ2 = CClCH2Cl,其中每个Z相同或不同,并且在加热时不存在催化剂的气相中为Cl或F; 和(2)在加热下在氟化催化剂存在下,在气相中使氟化氢与第一反应步骤中得到的反应产物反应的第二反应步骤。 根据本发明的方法,可以高选择性地获得2,3,3,3-四氟丙烯(HFO-1234yf),并且可以抑制催化剂劣化。

    Method for purifying 2,3,3,3-tetrafluoropropene
    3.
    发明授权
    Method for purifying 2,3,3,3-tetrafluoropropene 有权
    2,3,3,3-四氟丙烯的纯化方法

    公开(公告)号:US08975456B2

    公开(公告)日:2015-03-10

    申请号:US13505520

    申请日:2010-11-09

    IPC分类号: C07C17/25 C07C17/383

    CPC分类号: C07C17/383 C07C21/18

    摘要: The present invention provides a method for purifying HFO-1234yf, comprising the steps of (1) cooling a liquid mixture containing HFO-1234yf and HF to separate the mixture into a upper liquid phase having a high concentration of HF and a lower liquid phase having a high concentration of 2,3,3,3-tetrafluoropropene; and (2) subjecting the lower liquid phase obtained in step (1) to a distillation operation to withdraw a mixture containing HFO-1234yf and HF from a top of a distillation column, thereby obtaining substantially HF-free HFO-1234yf from a bottom of the distillation column. According to the present invention, HF and HFO-1234yf contained in a mixture containing HF and HFO-1234yf can be separated under simple and economically advantageous conditions.

    摘要翻译: 本发明提供了一种净化HFO-1234yf的方法,包括以下步骤:(1)冷却含有HFO-1234yf和HF的液体混合物,以将混合物分离成具有高浓度HF和较低液相的上液相, 高浓度的2,3,3,3-四氟丙烯; 和(2)将在步骤(1)中获得的下部液相进行蒸馏操作从蒸馏塔的顶部排出含有HFO-1234yf和HF的混合物,从而从底部获得基本上无HF的HFO-1234yf 蒸馏塔。 根据本发明,包含在含有HF和HFO-1234yf的混合物中的HF和HFO-1234yf可以在简单和经济上有利的条件下分离。

    Azeotropic or azeotrope-like composition and process for producing 2,3,3,3-tetrafluoropropene
    4.
    发明授权
    Azeotropic or azeotrope-like composition and process for producing 2,3,3,3-tetrafluoropropene 有权
    共沸或类共沸组合物和制备2,3,3,3-四氟丙烯的方法

    公开(公告)号:US08853473B2

    公开(公告)日:2014-10-07

    申请号:US13060869

    申请日:2009-08-21

    摘要: The present invention provides a process for producing 2,3,3,3-tetrafluoropropene, comprising distilling a mixture of water and 2,3,3,3-tetrafluoropropene to separate the mixture into a first stream and a second stream, the first stream containing 2,3,3,3-tetrafluoropropene with a water content higher than the original mixture, and the second stream containing 2,3,3,3-tetrafluoropropene with a water content lower than the original mixture; and obtaining 2,3,3,3-tetrafluoropropene with a reduced water content from the second stream. The process of the invention can efficiently remove water from 2,3,3,3-tetrafluoropropene (HFO-1234yf).

    摘要翻译: 本发明提供一种生产2,3,3,3-四氟丙烯的方法,包括蒸馏水和2,3,3,3-四氟丙烯的混合物以将混合物分离成第一流和第二料流,第一料流 含有水分高于原始混合物的2,3,3,3-四氟丙烯,第二料流含有水分低于原始混合物的2,3,3,3-四氟丙烯; 并从第二流中获得具有降低的水含量的2,3,3,3-四氟丙烯。 本发明的方法可以有效地从2,3,3,3-四氟丙烯(HFO-1234yf)中除去水。

    Liquid crystal display device
    5.
    发明授权
    Liquid crystal display device 有权
    液晶显示装置

    公开(公告)号:US08749726B2

    公开(公告)日:2014-06-10

    申请号:US13676566

    申请日:2012-11-14

    IPC分类号: G02F1/1343

    摘要: According to one embodiment, a liquid crystal display device includes a first substrate including a first storage capacitance line and a second storage capacitance line, a gate line located between the first storage capacitance line and the second storage capacitance line, a semiconductor layer located at a substantially central part of a pixel, a source line put in contact with the semiconductor layer, a drain electrode which is put in contact with the semiconductor layer and extends above the first storage capacitance line and the second storage capacitance line, and a pixel electrode including a first main pixel electrode opposed to the first storage capacitance line, and a second main pixel electrode opposed to the second storage capacitance line.

    摘要翻译: 根据一个实施例,液晶显示装置包括:第一基板,包括第一辅助电容线和第二辅助电容线;位于第一辅助电容线和第二辅助电容线之间的栅极线;位于 像素的大致中央部分,与半导体层接触的源极线,与半导体层接触并在第一辅助电容线和第二辅助电容线之上延伸的漏电极和包括 与第一辅助电容线相对的第一主像素电极和与第二辅助电容线相对的第二主像素电极。

    Half-duplex communication system, half-duplex communication device, communication content confirmation method, and its program
    6.
    发明授权
    Half-duplex communication system, half-duplex communication device, communication content confirmation method, and its program 有权
    半双工通信系统,半双工通信设备,通信内容确认方法及其程序

    公开(公告)号:US08570919B2

    公开(公告)日:2013-10-29

    申请号:US12600185

    申请日:2008-05-09

    IPC分类号: H04L5/16

    摘要: A half-duplex communication system that allows a user terminal to confirm past communication contents even during a series of half-duplex communications is provided. The system includes a communication record database in which all communication contents of half-duplex communications are stored together with identifiers thereof. A half-duplex communication device for controlling half-duplex communications includes a communication record control device which receives a communication content, transmits the communication content together with the identifier thereof to the communication record database so as to store it therein, and reads out the communication record therein. In response to a communication record readout request, the half-duplex communication device reads out a communication record in place of transmitting the communication content to a user terminal.

    摘要翻译: 提供了即使在一系列半双工通信期间也允许用户终端确认过去通信内容的半双工通信系统。 该系统包括通信记录数据库,其中半双工通信的所有通信内容与其标识符一起存储。 用于控制半双工通信的半双工通信设备包括:通信记录控制设备,其接收通信内容,将通信内容与其标识符一起发送到通信记录数据库,以便将其存储在其中,并读出通信 在其中记录。 响应于通信记录读出请求,半双工通信设备将用于发送通信内容的通信记录读出到用户终端。

    Image processing apparatus and image processing method
    7.
    发明授权
    Image processing apparatus and image processing method 有权
    图像处理装置和图像处理方法

    公开(公告)号:US08538247B2

    公开(公告)日:2013-09-17

    申请号:US13378459

    申请日:2010-07-01

    CPC分类号: H04N5/147

    摘要: A CPU divides a moving image file at a divided frame position, thereby generating a first divided moving image file including a first frame and another divided moving image file. The CPU detects a frame position where an object appears for the first time in the reproduction order from the other divided moving image file, and generates a file that describes the detected position as a new face information management file. The CPU controls a recording/reproduction control circuit to store the generated new face information management file in a recording medium in association with the other divided moving image file.

    摘要翻译: CPU在分割帧位置分割运动图像文件,从而生成包括第一帧和另一分割运动图像文件的第一分割运动图像文件。 CPU从另一个分割的运动图像文件以再现顺序检测对象第一次出现的帧位置,并且生成描述检测到的位置的文件作为新的面部信息管理文件。 CPU控制记录/再现控制电路,以将生成的新的面部信息管理文件与另一个分割的运动图像文件相关联地存储在记录介质中。

    PURIFICATION METHOD OF 2,3,3,3-TETRAFLUOROPROPENE
    8.
    发明申请
    PURIFICATION METHOD OF 2,3,3,3-TETRAFLUOROPROPENE 有权
    2,3,3,3-四氯丙烯的纯化方法

    公开(公告)号:US20130105296A1

    公开(公告)日:2013-05-02

    申请号:US13808358

    申请日:2011-07-21

    IPC分类号: C07C17/386

    摘要: This invention provides a method for purifying HFO-1234yf by removing HF from a mixture of HFO-1234yf and HF under simple and economically advantageous conditions. According to the present invention, this is a purification method for 2,3,3,3-tetrafluoropropene, (1) the purification method comprising the step of subjecting a mixture comprising 2,3,3,3-tetrafluoropropene and hydrogen fluoride to extractive distillation in a distillation column A using an extractant, thereby obtaining a fraction I that contains 2,3,3,3-tetrafluoropropene and has a lower ratio of hydrogen fluoride to 2,3,3,3-tetrafluoropropene than that of the mixture, while obtaining a fraction II that contains hydrogen fluoride and has a lower ratio of 2,3,3,3-tetrafluoropropene to hydrogen fluoride than that of the mixture; (2) the extractant comprising at least one member selected from the group consisting of: (i) alcohols represented by ROH, wherein R is a C1-5 alkyl group, (ii) ethers represented by ROR′, wherein R and R′ are the same or different, and each is a C1-4 alkyl group, (iii) fluorinated alcohols represented by RfOH, wherein Rf is a C1-3 fluoroalkyl group, (iv) ketones represented by RCOR′, wherein R and R′ are the same or different, and each is a C1-4 alkyl group, (v) esters represented by RCOOR′, wherein R and R′ are the same or different, and each is a C1-4 alkyl group, (vi) polyols represented by R(OH)n, wherein R is a C1-4 alkyl group, and n is an integer of 2 to 3, and (vii) ethylene glycols represented by R1O(CH2CH2O)nR2, wherein R1 and R2 are the same or different, and each is hydrogen or a C1-4 alkyl group, and n is an integer of 1 to 3.

    摘要翻译: 本发明提供了一种通过在简单且经济有利的条件下从HFO-1234yf和HF的混合物中除去HF来净化HFO-1234yf的方法。 根据本发明,这是2,3,3,3-四氟丙烯的纯化方法,(1)纯化方法,其包括将包含2,3,3,3-四氟丙烯和氟化氢的混合物进行萃取 在使用萃取剂的蒸馏塔A中进行蒸馏,从而获得含有2,3,3,3-四氟丙烯的馏分I,并且氟化氢与2,3,3,3-四氟丙烯的比例低于混合物, 同时获得含有氟化氢并且比2,3混合物具有较低的2,3,3,3-四氟丙烯与氟化氢的比例II; (2)萃取剂,其包含选自以下的至少一种:(i)由ROH表示的醇,其中R为C 1-5烷基,(ii)由ROR'表示的醚,其中R和R'为 相同或不同,各自为C1-4烷基,(iii)由RfOH表示的氟化醇,其中Rf为C1-3氟代烷基,(iv)由RCOR'表示的酮,其中R和R'为 相同或不同,并且各自为C 1-4烷基,(v)由RCOOR'表示的酯,其中R和R'相同或不同,并且各自为C 1-4烷基,(vi)由 R(OH)n,其中R是C 1-4烷基,n是2至3的整数,和(vii)由R 10(CH 2 CH 2 O)n R 2表示的乙二醇,其中R 1和R 2相同或不同, 各自为氢或C 1-4烷基,n为1〜3的整数。

    alpha+beta-TYPE TITANIUM ALLOY PART AND METHOD OF PRODUCTION OF SAME
    9.
    发明申请
    alpha+beta-TYPE TITANIUM ALLOY PART AND METHOD OF PRODUCTION OF SAME 有权
    α+β型钛合金部件及其制造方法

    公开(公告)号:US20120234066A1

    公开(公告)日:2012-09-20

    申请号:US13513026

    申请日:2010-12-02

    IPC分类号: B21B27/06 C22C14/00

    摘要: A method of production of an α+β-type titanium alloy part for a motorcycle, car, or bicycle which has a high Young's modulus (rigidity) in the axial direction of the shaped product and a bolt, engine valve, or connecting rod made of an α+β-type titanium alloy and a method of production of the same, wherein an α+β-type titanium alloy is heated at the temperatures giving the β-single phase, then is uni-directionally hot rolled, the plate is machined so that a direction vertical to both the hot rolling direction and thickness direction (width direction) corresponds to the direction in which high rigidity is demanded in the finished part, that is, the axial direction of the bolt, engine valve, or connecting rod, and the X-ray diffraction intensities I(0002), I(10-10), and I(10-11), of the (0002) plane, (10-10) plane, and (10-11) plane of the titanium α-phase measured at the cross-sections vertical to the longitudinal axial direction of the parts satisfy I(0002)/[I(10-10)+I(10-11)]≦1.

    摘要翻译: 一种在成形制品的轴向上具有高杨氏模量(刚性)的摩托车,汽车或自行车的α+ / bgr型型钛合金部件的制造方法以及螺栓,发动机气门或连杆 由α+ / bgr型钛合金制成,其制造方法为α+ b型钛合金,在单相温度下加热,然后单向热轧 加工板,使得与热轧方向和厚度方向(宽度方向)垂直的方向对应于成品部件中要求高刚性的方向,即螺栓,发动机阀门的轴向方向 (10-10)面的X射线衍射强度I(0002),I(10-10)和I(10-11),(10-10)面和(10- 11)在垂直于部件的纵向轴向的横截面处测量的钛α相的面积满足I(0002)/ [I(10-10 )+ I(10-11)]≦̸ 1。

    BETA-TYPE TITANIUM ALLOY
    10.
    发明申请
    BETA-TYPE TITANIUM ALLOY 有权
    BETA型钛合金

    公开(公告)号:US20120189487A1

    公开(公告)日:2012-07-26

    申请号:US13358483

    申请日:2012-01-25

    IPC分类号: C22C14/00

    CPC分类号: C22C14/00 C22F1/00 C22F1/18

    摘要: The present invention provides a β-type titanium alloy that includes, by mass %, when Al: 2 to 5%, 1) Fe: 2 to 4%, Cr: 6.2 to 11%, and V: 4 to 10%, 2) Fe: 2 to 4%, Cr: 5 to 11%, and Mo: 4 to 10%, or 3) Fe: 2 to 4%, Cr: 5.5 to 11%, and Mo+V (total of Mo and V): 4 to 10% in range, and a balance of substantially Ti. These include Zr added in amounts of 1 to 4 mass %. Furthermore, by making the oxygen equivalent Q 0.15 to 0.30 or leaving the alloy in the work hardened state or by applying both, the tensile strength before aging heat treatment can be further increased.