摘要:
The present invention is a piezoelectric composition and a piezoelectric element using the piezoelectric composition, the composition being characterized by: having a Perovskite structure represented by general formula ABO3; being represented by composition formula x(Bi0.5K0.5)TiO3-yBi(Mg0.5Ti0.5)O3-zBiFeO3, x+y+z=1 in the composition formula above; and in a triangular coordinate using x, y and z in the composition formula above, having a composition represented by a region which is surrounded by a pentagon ABCDE with apexes of point A (1, 0, 0), point B (0.7, 0.3, 0), point C (0.1, 0.3, 0.6), point D (0.1, 0.1, 0.8) and point E (0.2, 0, 0.8) and which does not include the line segment AE that connects point A (1, 0, 0) and point E (0.2, 0, 0.8).
摘要:
To produce a ferroelectric film formed of a lead-free material. The ferroelectric film according to an aspect of the present invention includes a (K1-XNaX)NbO3 film or a BiFeO3 film having a perovskite structure and a crystalline oxide preferentially oriented to (001) formed on at least one of the upper side and lower side of the (K1-XNaX)NbO3 film or BiFeO3 film, and X satisfies the formula below 0.3≦X≦0.7.
摘要:
A lead-free piezoelectric ceramic material has the general chemical formula xBiCoO3-y(Bi0.5Na0.5)TiO3-z(Bi0.5K0.5)TiO3, xBiCoO3-y(Bi0.5Na0.5)TiO3-zNaN-bO3, xBiCoO3-y(Bi0.5Na0.5)TiO3-zKNbO3, xBiCoO3-yBi(Mg0.5Ti0.5)O3-z(Bi0.5Na0.5)TiO3, xBiCoO3-yBa-TiO3-z(Bi0.5Na0.5)TiO3, or xBiCoO3-yNaNbO3-zKNbO3; wherein x+y+z=1, and x, y, z≠0.
摘要:
A piezoelectric material is expressed as a mixed crystal including a complex oxide having a perovskite structure and a rhombohedral structure and a complex oxide having a perovskite structure and a tetragonal structure, and the molar ratio of the complex oxide having a rhombohedral structure to the complex oxide having a tetragonal structure (rhombohedral crystal/tetragonal crystal) is 0.54 to less than 1.20.
摘要:
Provided is a piezoelectric element comprising a first electrode; a piezoelectric body layer provided on the first electrode, the piezoelectric body layer including 50 mol % or more of at least bismuth and iron, and the piezoelectric body layer having a current density-time curve obtained by applying a voltage to the first electrode and the second electrode including a plurality of inflection points; and a second electrode provided on the piezoelectric body layer.
摘要:
A piezoelectric element which includes an adhesion layer made of composite oxide having perovskite structure including at least one of bismuth, manganese, iron, and titanium; a first electrode provided on the adhesion layer and made of metal preferentially oriented in a (100) face; a piezoelectric body layer provided on the first electrode and made of composite oxide having perovskite structure preferentially oriented in the (100) face; and a second electrode provided on the piezoelectric body layer.
摘要:
A piezoelectric material contains a first component that is a rhombohedral crystal and that is configured to have a complex oxide with a perovskite structure and Curie temperature Tc1, a second component that is a crystal other than a rhombohedral crystal and that is configured to have a complex oxide with a perovskite structure and Curie temperature e Tc2, and a third component that is a rhombohedral crystal and that is configured to have a complex oxide with a perovskite structure and Curie temperature Tc3 different from the first component, and in which Tc2 is higher than Tc1, Tc3 is equal to or higher than Tc2, and a value of (0.1×Tc1+0.9×Tc2) is equal to or lower than 280° C.
摘要:
Provided is a piezoelectric material that achieves both high piezoelectric performance and high Curie temperature. In addition, provided are a piezoelectric element, a liquid discharge head, an ultrasonic motor, and a dust removing device, which use the piezoelectric material. The piezoelectric material includes a perovskite-type metal oxide that is expressed by the following general formula (1): xBaTiO3-yBiFeO3-zBi(M0.5Ti0.5)O3 (1), where M represents at least one type of element selected from the group consisting of Mg and Ni, x satisfies 0.25≦x≦0.75, y satisfies 0.15≦y≦0.70, z satisfies 0.05≦z≦0.60, and x+y+z=1 is satisfied.
摘要翻译:提供一种能够实现高压电性能和高居里温度的压电材料。 此外,提供了使用压电材料的压电元件,排液头,超声波马达和除尘装置。 压电材料包括由以下通式(1)表示的钙钛矿型金属氧化物:xBaTiO3-yBiFeO3-zBi(M0.5Ti0.5)O3(1),其中M表示至少一种选自 由Mg和Ni组成的组x满足0.25≦̸ x≦̸ 0.75,y满足0.15≦̸ y≦̸ 0.70,z满足0.05≦̸ z≦̸ 0.60,x + y + z = 1。
摘要:
A piezoelectric element 300 includes a first electrode 60, a piezoelectric layer 70 which is provided on the first electrode, and a second electrode 80 which is provided on the piezoelectric layer, and the piezoelectric layer is made of a piezoelectric material expressed as a mixed crystal including a first component formed of a complex oxide containing Bi and Fe and having a rhombohedral perovskite structure and a complex oxide containing Ba and Ti and having a tetragonal perovskite structure, a second component formed of a complex oxide containing Bi, K, and Ti and having a tetragonal perovskite structure, and a third component formed of a complex oxide containing Bi, Mg, and Ti and having a rhombohedral perovskite structure.
摘要:
A piezoelectric material is expressed as a mixed crystal including a complex oxide having a perovskite structure and a rhombohedral structure and a complex oxide having a perovskite structure and a tetragonal structure, and the molar ratio of the complex oxide having a rhombohedral structure to the complex oxide having a tetragonal structure (rhombohedral crystal/tetragonal crystal) is 0.54 to less than 1.20.