摘要:
Propylene copolymer composition comprising a propylene copolymer (A) having a comonomer content in the range of equal or more than 0.5 to equal or below 2.0 wt.-%, the comonomers are C5 to C12 α-olefins, and a propylene copolymer (B) having a comonomer content in the range of equal or more than 4.0 to equal or below 10.0 wt.-%, the comonomers are C5 to C12 α-olefins, wherein further the propylene copolymer composition has a comonomer content in the range of equal or more than 3.5 to equal or below 7.0 wt.-%, the comonomers are C5 to C12 α-olefins, and the weight ratio of the propylene copolymer (A) to the propylene copolymer (B) is in the range of 20/80 to below 55/45.
摘要:
Polypropylene composition comprising propylene homopolymer (H-PP) and a propylene copolymer (C-PP), said copolmyer comprises (a) a propylene copolymer fraction (A) having a comonomer content of equal or above 1.0 wt.-%, the comomers are C5 to C12 α-olefins, and (b) a propylene copolymer action (B) having a comonomer content of 4.0 to 20.0 wt-%, the comomers are C5 to C12 α-olefins, wherein further (i) the comonomer content in propylene copolymer fraction (A) is lower compared to the comonomer content in the propylene copolymer fraction (B), (ii) the propylene copolymer (C-PP) has a comonomer content of at least 2.0 wt.-%, the comomers are C5 to C12 α-olefins, (iii) the weight ratio [(A)/(B)] of the propylene copolymer fraction (A) to the propylene copolymer fraction (B) is in the range of 20/80 to 80/20, and (iv) the weight ratio [(C-PP)/(H-PP)] of the propylene copolymer (C-PP) to the propylene homopolymer (H-PP) is in the range of 95/5 to 75/25.
摘要:
A non-sealable, multi-layer polypropylene film which includes on top of a polypropylene base layer at least one top layer which includes a mixture of a propylene/butylene copolymer and an ethylene/propylene/butylene terpolymer, the mixture containing ethylene in an amount of about 0.1 to 7% by weight, propylene in an amount of about 68 to 95.9% by weight and butylene in an amount of about 4 to 25% by weight, relative to the total weight of the mixture. The layer thickness of the toplayer is not greater than 0.3 .mu.m. A process for producing the film is also described.
摘要:
The present invention relates to an olefin-based paint. The purpose of the present invention is to provide a paint with excellent organic solvent solubility or dispersibility, low paint viscosity, minimal coating irregularities even at high concentrations, excellent handling and storage stability, and excellent blocking resistance and coated film stability. In order to meet this purpose, an olefin-based paint is used that is characterized by containing a solution or dispersion obtained by dissolving or dispersing 0.1-55 parts by mass of a propylene-α-olefin copolymer (A) for 100 parts by mass of an organic solvent. The copolymer (A) is characterized by containing 60-90 mol % of propylene-derived constituent units (a) having a weight-average molecular weight (Mw), measured by GPC, in the range of 3,000 to 40,000, and 10-40 mol % of α-olefin-derived constituent units (b) having 4 or more carbon atoms [wherein (a)+(b)=100 mol %].
摘要:
Propylene copolymer composition (P) comprising (a) a propylene copolymer (A) having a comonomer content of at least 1.0 wt.-%, the comomers are C5 to C12 a-olefins, and (b) a propylene copolymer (B) having a comonomer content of 4.0 to 20.0 wt.-%, the comomers are C5 to C12 a-olefins, wherein further (i) the comonomer content in the propylene copolymer (A) is lower compared to the comonomer content in the propylene copolymer (B), (ii) the propylene copolymer composition (P) has a comonomer content of 2.0 to 10.0 wt.-%, the comomers are C5 to C12 a-olefins, (iii) the weight ratio of the propylene copolymer (A) to the propylene copolymer (B) is the range of 30/70 to 80/20.
摘要:
A process for tuft and filament bonding of unfinished carpet includes applying a coating composition which contains from 50% to 100% by weight of a substantially amorphous poly-null-olefin as a melt to the backside of a carpet material so as to obtain a coating weight of from 20 to 1,500 g/m2, the melt viscosity of the coating composition at 190null C. is in the range from 400 mPas to 10,000 mPas.
摘要翻译:未完成的地毯的毛簇和长丝粘合的方法包括将含有50重量%至100重量%的基本无定形聚-α-烯烃作为熔体的涂料组合物施用到地毯材料的背面,以获得涂层 重量为20至1,500g / m 2,涂层组合物在190℃下的熔体粘度在400mPas至10,000mPa·s的范围内。
摘要:
A coating composition comprising: an aqueous dispersion comprising: the melt-kneading product of (A) a base polymer which comprises one or more thermoplastic polymers, (B) a stabilizing agent which comprises at least one component selected from the group consisting of acrylic acid grafted ethylene-based polymers and maleic anhydride grafted polyolefins; (C) a neutralizing agent; and (D) water; wherein the aqueous dispersion has a volume average particle size of less than about 5 μm is provided.
摘要:
The invention relates to a novel halogen-free and acid-free, readily soluble priming bonding agent for polyolefins, said agent containing (meth)acrylate-grafted, amorphous polyolefins.
摘要:
The invention relates to a novel halogen-free and acid-free, readily soluble adhesion promoter for polyolefins, said promoter containing (meth)acrylate-grafted, amorphous polyolefins.
摘要:
The invention relates to a novel halogen-free and acid-free, readily soluble priming bonding agent for polyolefins, said agent containing (meth)acrylate-grafted, amorphous polyolefins.