摘要:
Melt-blown webs having no shots and improved barrier properties, whereby the melt-blown webs are made out of a so-called “controlled rheology” propylene (CR-PP), which was visbroken without any peroxide.
摘要:
The present invention relates to a polypropylene composition comprising —10 to 50 wt. % of recycled polypropylene (R-PP) and/or linear polypropylene (L-PP); —40 to 89.95 wt. % of a high melt strength polypropylene (HMS-PP) having an F30 melt strength of more than 25.0 cN and a v30 melt extensibility of more than 205 mm/s, wherein the F30 melt strength and the v30 melt extensibility are determined according to ISO 16790:2005; and —0.05 to 10 wt. % of a nucleating agent (NA); a foamed sheet formed from the polypropylene composition; an article comprising the foamed sheet and a process comprising the step of forming the polypropylene composition. Furthermore, the invention is further directed to the usage of the polypropylene composition for the formation of foamed sheets.
摘要:
The present invention relates to a foamed sheet consisting of a polypropylene composition comprising at least 85 wt. %, e.g. from 85 to 99.5 wt.-%, of a high melt strength polypropylene (HMS-PP) and 0.5 to 15 wt. % of a nucleating agent (NA), wherein the foamed sheet has a thickness of below 0.5 mm or a thickness of 2.0 mm or more. The present invention further relates to a foamed material consisting of a polypropylene composition as well as the use of a polypropylene composition comprising at least 85 wt. %, e.g. from 85 to 99.5 wt.-%, of a high melt strength polypropylene (HMS-PP) and 0.5 to 15 wt. % of a nucleating agent (NA) for producing foamed material.
摘要:
The present invention relates to pellets comprising a polyethylene composition, a pipe or pipe system comprising the pellets as well as a process for the preparation of such a pipe or pipe system.
摘要:
The present invention relates to a polyethylene composition comprising-a base resin comprising (A) a first ethylene homo- or copolymer component having a melt flow rate MFR2 (2.16 kg, 190° C.) of equal to or more than 150 g/10 min to equal to or less than 300 g/10 min, determined according to ISO 1133, and (B) a second ethylene homo- or copolymer component, -optional carbon black, -optional further polymer component(s) different to the first ethylene homo- or copolymer components (A) and (B), and -optional additive(s); wherein the first ethylene homo- or copolymer component (A) has a lower weight average molecular weight as the second ethylene homo- or copolymer component (B), and the weight ratio of the first ethylene homo- or copolymer component (A) to the second ethylene homo- or copolymer component (B) is from 40:60 to 47:53; the polyethylene composition has a melt flow rate MFRS (5 kg, 190° C.) of equal to or more than 0.35 g/10 min to equal to or less than 0.60 g/10 min, determined according to ISO 1133. The invention further relates to a process for the production of such a polyethylene composition, an article, such as a pipe or pipe fitting comprising such a polyethylene composition and the use of such a polyethylene composition for the production of such an article.
摘要:
The present invention is directed to a foamable polyolefin composition which is crosslinkable by silane groups, to a crosslinked foam obtained from such a foamable polyolefin composition, and to a process for producing a crosslinked foam based on the foamable polyolefin composition. The foamable polyolefin composition comprises a polyethylene bearing hydrolysable silane groups and comonomer units comprising a polar group selected from the group consisting of acrylic acid, methacrylic acid, acrylates, methacrylates, vinyl esters, and mixtures thereof, a silanol condensation catalyst, a physical blowing agent, and a cell nucleating agent.
摘要:
The present invention relates to a polyethylene composition comprising, a base resin (A) comprising a copolymer of ethylene and at least one comonomer selected from alpha-olefins having from three to twelve carbon atoms, wherein the ethylene copolymer comprises a low molecular weight component (A-1) and a high molecular weight component (A-2) with the low molecular weight component (A-1) having a lower weight average molecular weight than the high molecular weight component (A-2), (B) carbon black in an amount of 1.0 to 10 wt % based on the total amount of the polyethylene composition, and (C) optional further additives other than carbon black; wherein the low molecular weight component (A-1) has a melt flow rate MFR2 (190° C., 2.16 kg) of equal to or more than 150 g/10 min to equal to or less than 400 g/10 min, determined according to ISO 1133, the base resin (A) has a density of equal to or more than 943 kg/m3 to equal to or less than 957 kg/m3, determined according to ISO 1183, and the composition has a melt flow rate MFR5 (190° C., 5 kg) of equal to or more than 0.14 g/10 min to equal to or less than 0.30 g/10 min, determined according to ISO 1133, a viscosity at a constant shear stress of 747 Pa, eta747, of equal to or more than 800 kPa*s to equal to or less than 1300 kPa*s, and complies with the in-equation (I) eta747>−1800×MFR5+1200 (I), a process for producing said polyethylene composition and an article comprising said polyethylene composition.
摘要:
The present invention relates to a polyethylene composition comprising—a base resin comprising (A) a first ethylene homo- or copolymer component having a melt flow rate MFR2 (2.16 kg, 190° C.) of equal to or more than 150 g/10 min to equal to or less than 300 g/10 min, determined according to ISO 1133, and (B) a second ethylene homo- or copolymer component, —optional carbon black, —optional further polymer component(s) different to the first ethylene homo- or copolymer components (A) and (B), and —optional additive(s); wherein the first ethylene homo- or copolymer component (A) has a lower weight average molecular weight as the second ethylene homo- or copolymer component (B), and the weight ratio of the first ethylene homo- or copolymer component (A) to the second ethylene homo- or copolymer component (B) is from 40:60 to 47:53; the polyethylene composition has a melt flow rate MFR5 (5 kg, 190° C.) of equal to or more than 0.35 g/10 min to equal to or less than 0.60 g/10 min, determined according to ISO 1133. The invention further relates to a process for the production of such a polyethylene composition, an article, such as a pipe or pipe fitting comprising such a polyethylene composition and the use of such a polyethylene composition for the production of such an article.
摘要:
The present invention relates to the use of a combination of additives comprising at least two of the following compounds: an antioxidant (A) according to formula (I): wherein R1, R2, R3, R4 and R5 independently are H, or non-substituted or substituted aliphatic or aromatic hydrocarbyl radicals which may comprise heteroatoms, an antioxidant (B) according to formula (II): wherein o R6, R7 and R8 independently are non-substituted or substituted aliphatic or aromatic hydrocarbyl radicals which may comprise OH-groups; o X1, X2, and X3 independently are H or OH, with the provisio that at least one of X1, X2 and X3 is OH; and o the entire molecule does not comprise an ester group; carbon black; reducing taste and/or odour in a polyolefin composition.
摘要:
The present invention relates to a multilayer sheet comprising at least two layers (A) and (B) in adherent contact with each other, wherein layer (A) is a foamed sheet comprising a high melt strength polypropylene composition and layer (B) is a coated non-foamed layer, which comprises a polypropylene composition, a process for producing said multilayer sheet, an article comprising said multilayer sheet and the use of said multilayer sheet for the production of an article with improved water vapor transmission and oxygen transmission properties.