摘要:
A first fine particle-containing solution is deposited on an appropriate substrate, and dried to form a first fine particle aggregate layer. Polymer particles are deposited on the first fine particle aggregate layer, and are supplied with a second fine particle-containing solution such that the polymer particles are immersed in the second fine particle-containing solution. The second fine particle-containing solution is dried to form a second fine particle aggregate layer containing a large number of the polymer particles embedded. A first structure precursor is completed at this stage. Then, the first structure precursor is separated from the substrate, and thermally treated. Thus, the production of a first solid electrolyte structure, which has a porous solid electrolyte portion and a dense solid electrolyte portion integrated, is completed.
摘要:
An all-solid-state cell contains a combination of an electrode active material and a solid electrolyte, and has a plate-shaped fired solid electrolyte body of a ceramic containing a solid electrolyte, a first electrode layer (e.g. a positive electrode) integrally formed on one surface of the fired solid electrolyte body by mixing and firing an electrode active material and a solid electrolyte, and a second electrode layer (e.g. a negative electrode) integrally formed on the other surface of the fired solid electrolyte body by mixing and firing an electrode active material and a solid electrolyte. The solid electrolyte materials added to the first electrode layer and the second electrode layer comprise an amorphous polyanion compound.
摘要:
The present invention provides a ceramic material allowing a pellet having higher density and satisfactory Li ion conduction to be obtained. The ceramic material contains Li, La, Zr, Al and O and has a garnet-type or garnet-like crystal structure, the ratio of the number of moles of Li with respect to La being 2.0 or greater to 2.5 or lower.
摘要:
An illuminated makeup mirror set includes: a mirror unit; a surface light source for illumination with adjustable color and adjustable brightness; a memory unit in which illumination conditions corresponding to a plurality of scenes are stored; a detection unit for detecting the color and brightness of ambient light at an installation position of the makeup mirror set; a selection unit for selecting one of the plurality of scenes according to an input operation; an acquisition unit for acquiring, from the memory unit, illumination conditions corresponding to the scene selected through the selection unit; and an adjustment unit for adjusting the color and brightness of the surface light source according to the color and brightness of the ambient light detected by the detection unit and the illumination conditions acquired by the acquisition unit.
摘要:
A base film for a dicing sheet is provided which can suppress dicing debris from generating during the dicing of a cut object without imparting physical energy, such as electron beam or γ ray. The base film for a dicing sheet comprises a resin layer. The resin layer comprises: a norbornene-based resin that is a thermoplastic resin having a norbornene-based compound as at least one type of monomer; and an olefin-based thermoplastic resin other than the norbornene-based resin. The norbornene-based resin in the resin layer has a content of more than 3.0 mass %. A dicing sheet is also provided which comprises: the base film for a dicing sheet; and a pressure-sensitive adhesive layer placed on a surface of the film at the resin layer side.
摘要:
A method for manufacturing an image display element including: a front panel; a back panel facing the front panel; plural pixels arranged in a matrix between the panels, and to be selected to be in a display or non-display state; and plural electrodes for controlling the pixels, the panels being bonded with the pixels and the electrodes interposed therebetween, and the electrodes being connected to a driving control circuit via metal wires, includes a first step of performing dicing from the back side of the opposing surface from the front panel, and forming a groove part such that electrode terminals connected to the electrodes are exposed between adjacent plural pixel lines, with the back panel bonded thereto, and a second step of forming the metal wires so as to be connected to the electrode terminals exposed at the groove part.
摘要:
A ceramic material according to the present invention mainly contains magnesium, aluminum, oxygen, and nitrogen, the ceramic material has the crystal phase of a MgO—AlN solid solution in which aluminum nitride is dissolved in magnesium oxide, the crystal phase serving as a main phase. Preferably, XRD peaks corresponding to the (200) and (220) planes of the MgO—AlN solid solution measured with CuKα radiation appear at 2θ=42.9 to 44.8° and 62.3 to 65.2°, respectively, the XRD peaks being located between peaks of cubic magnesium oxide and peaks of cubic aluminum nitride. More preferably, the XRD peak corresponding to the (111) plane appears at 2θ=36.9 to 39°, the XRD peak being located between a peak of cubic magnesium oxide and a peak of cubic aluminum nitride.
摘要:
A first selector receives a second input signal and a second reference voltage, and selects either one. A first buffer receives the output signal of the first selector, and outputs the signal thus received to a terminal of the first resistor, and to a terminal of the third resistor. A second selector receives a first input signal and a third input signal, and selects either one. A fourth selector receives, as input signals, the output signal of an operational amplifier, a signal that corresponds to the output signal of the second selector, and a signal that corresponds to the second input signal, and selects one signal selected from among the signals thus received.
摘要:
The present invention provides a mask blank which comprises a substrate made of a synthetic quartz glass and a light-shielding film laminated on a surface of the substrate and is for use in a semiconductor device production technique employing an exposure light wavelength of 200 nm or shorter, wherein the mask blank has a birefringence, as measured at a wavelength of 193 nm, of 1 nm or less per substrate thickness. According to the present invention, mask blanks suitable for use in the immersion exposure technique and the polarized illumination technique are provided.
摘要:
A method for manufacturing an image display element including: a front panel; a back panel facing the front panel; plural pixels arranged in a matrix between the panels, and to be selected to be in a display or non-display state; and plural electrodes for controlling the pixels, the panels being bonded with the pixels and the electrodes interposed therebetween, and the electrodes being connected to a driving control circuit via metal wires, includes a first step of performing dicing from the back side of the opposing surface from the front panel, and forming a groove part such that electrode terminals connected to the electrodes are exposed between adjacent plural pixel lines, with the back panel bonded thereto, and a second step of forming the metal wires so as to be connected to the electrode terminals exposed at the groove part.