摘要:
An method of making a porous asymmetric membrane involves dissolving a poly(phenylene ether), poly(phenylene ether) copolymer, polyethersulfone, polysulfone, polyphenylsulfone, polyimide, polyetherimide, polyvinylidene fluoride, or a combination thereof in a water-miscible polar aprotic solvent to provide a membrane-forming composition; and phase-inverting the membrane-forming composition in a first non-solvent composition composed of water, a water-miscible polar aprotic solvent, or a mixture thereof, and a polymer additive dissolved in the first non-solvent composition. The method can be a method of making a hollow fiber by coextrusion through a spinneret having an annulus and a bore, including coextruding the membrane-forming composition through the annulus, and the first non-solvent composition through the bore, into a second non-solvent composition composed of water, a water-miscible polar aprotic solvent, or a mixture thereof to form the hollow fiber.
摘要:
A porous asymmetric membrane comprises a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer; and a polymer additive. A separation module can be fabricated from the porous asymmetric membrane. A method of forming the porous asymmetric membrane comprises: dissolving a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer and, a polymer additive in a water-miscible polar aprotic solvent to form a porous asymmetric membrane-forming composition; and phase-inverting the porous asymmetric membrane forming-composition in a first non-solvent composition to form the porous asymmetric membrane. The polymer additive comprises hydrophilic functional groups, copolymerized hydrophilic monomers, or blocks of hydrophilic monomer repeat units. For example, the polymer additive can comprise a hydrophilic polymer or amphiphilic polymer. The porous asymmetric membrane can be a flat membrane or hollow fiber.
摘要:
A porous asymmetric membrane comprises a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer; and a polymer additive. A separation module can be fabricated from the porous asymmetric membrane. A method of forming the porous asymmetric membrane comprises: dissolving a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer and, a polymer additive in a water-miscible polar aprotic solvent to form a porous asymmetric membrane-forming composition; and phase-inverting the porous asymmetric membrane forming-composition in a first non-solvent composition to form the porous asymmetric membrane. The polymer additive comprises hydrophilic functional groups, copolymerized hydrophilic monomers, or blocks of hydrophilic monomer repeat units. For example, the polymer additive can comprise a hydrophilic polymer or amphiphilic polymer. The porous asymmetric membrane can be a flat membrane or hollow fiber.
摘要:
A polycarbonate composition includes: a continuous polycarbonate phase; discontinuous first domains distributed in the continuous phase, and comprising a core-shell silicone-(meth)acrylate impact modifier comprising a silicone elastomer core and a (meth)acrylate copolymer shell, wherein the first domains have an aspect ratio of at least 1.7, preferably at least 1.8; and discontinuous second domains distributed in the continuous phase, and comprising an alkenyl aromatic-olefin block copolymer impact modifier, wherein the second domains have an aspect ratio of at least 3, preferably at least 4, and a domain size of 6400 square nanometers or less, more preferably 5700 square nanometers or less. Optionally, the polycarbonate composition includes: a polycarbonate; a brominated polycarbonate different from the polycarbonate; a poly(carbonate-siloxane) comprising 30 to 70 weight percent of siloxane blocks; a core-shell silicone-(meth)acrylate impact modifier comprising a silicone elastomer core and an (meth)acrylate copolymer shell; and an alkenyl aromatic-olefin block copolymer impact modifier.
摘要:
An asymmetric membrane having a substantially non-porous surface layer is made by a method including: dissolving a poly(phenylene ether) copolymer in a solvent mixture including a first solvent and a second solvent to provide a membrane-forming composition; and phase-inverting the membrane forming composition in a first non-solvent to form the membrane comprising a substantially non-porous surface layer. The first solvent is a water-miscible polar aprotic solvent, and the second solvent is a polar solvent having two to eight carbon atoms.
摘要:
A porous membrane made from a poly(phenylene ether) copolymer has at least one of: a molecular weight cut off of less than 40 kilodaltons or a surface pore size of 0.001 to 0.1 micrometers. The porous membrane is made by dissolving the poly(phenylene ether) copolymer in a water-miscible polar aprotic solvent to form a porous membrane-forming composition; and phase-inverting the porous asymmetric membrane forming-composition in a first non-solvent composition to form the porous mem-brane. The porous membrane can be in the form of a sheet or a hollow fiber, and can be fabricated into separation modules.
摘要:
A porous membrane is made from a poly(phenylene ether) copolymer containing 10 to 40 mole percent repeat units derived from 2-methyl-6-phenylphenol and 60 to 90 mole percent repeat units derived from 2,6-dimethylphenol; and a block copolymer containing backbone or pendant blocks of poly(C2-4 alkylene oxide). The porous membrane is made by dissolving the poly(phenylene ether) copolymer in a water-miscible polar aprotic solvent to form a membrane-forming composition; and phase-inverting the membrane forming-composition in a first non-solvent composition to form the porous membrane. A method of making a hollow fiber by coextrusion through a spinneret having an annulus and a bore, includes coextruding the membrane-forming composition through the annulus, and a first non-solvent composition through the bore, into a second non-solvent composition to form the hollow fiber.
摘要:
The invention relates to a process for preparing a hydrocracking catalyst, comprising (i) contacting a shaped body comprising a zeolite and a binder with an aqueous solution of a hydrogenation metal compound which is a complex or a salt of a hydrogenation metal to deposit the hydrogenation metal onto the shaped body, wherein the aqueous solution comprises an ammonium salt and (ii) calcining the shaped body obtained by step (i).
摘要:
A porous asymmetric membrane comprises a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer; and a polymer additive. A separation module can be fabricated from the porous asymmetric membrane. A method of forming the porous asymmetric membrane comprises: dissolving a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer and, a polymer additive in a water-miscible polar aprotic solvent to form a porous asymmetric membrane-forming composition; and phase-inverting the porous asymmetric membrane forming-composition in a first non-solvent composition to form the porous asymmetric membrane. The polymer additive comprises hydrophilic functional groups, copolymerized hydrophilic monomers, or blocks of hydrophilic monomer repeat units. For example, the polymer additive can comprise a hydrophilic polymer or amphiphilic polymer. The porous asymmetric membrane can be a flat membrane or hollow fiber.
摘要:
A porous composite membrane includes a porous support layer of a poly(phenylene ether) or poly(phenylene ether) copolymer; and an amphiphilic copolymer having a hydrophobic block and a hydrophilic block or graft, wherein the hydrophobic block includes a polystyrene block, a poly(phenylene ether) block, or a poly(phenylene ether) copolymer block; and an ultrathin, cross-linked, water permeable layer, which is the reaction product of an electrophilic monomer and a nucleophilic monomer, in contact with a side of the porous support layer. The reaction product can be a polyamide that is the interfacial condensation product of: an aromatic, polyfunctional acyl halide comprising of 3 to 6 acyl halide groups per aromatic ring and an aromatic polyamine comprising at least two primary amine groups and a maximum number of primary amine groups that is less than or equal to the number of acyl halide groups on the polyfunctional acyl halide.