GLASS FIBER-REINFORCED THERMOPLASTIC POLYMER COMPOSITION

    公开(公告)号:US20250066563A1

    公开(公告)日:2025-02-27

    申请号:US18724330

    申请日:2022-12-16

    Abstract: A glass fiber-reinforced thermoplastic polymer composition has a sheathed continuous multifilament strand including a core that extends in the longitudinal direction and a polymer sheath which intimately surrounds the core, wherein the core has an impregnated continuous multifilament strand having at least one continuous glass multifilament strand, wherein the at least one continuous glass multifilament strand is impregnated with an impregnating agent, the polymer sheath is a thermoplastic polymer composition including a thermoplastic polymer, wherein the thermoplastic polymer contains a polyester having a weight average molecular weight of 15,000 to 80,000 Daltons as measured by gel permeation chromatography (GPC) using polystyrene standard and as measured by differential scanning calorimetry with a heating rate of 20° C./minute on first heating according to ASTM D3418-08, at least one crystalline melting point (Tm) of 200 to 290° C.

    PROCESS OF MANUFACTURING GRAFT POLYMER COMPOSITIONS

    公开(公告)号:US20250051489A1

    公开(公告)日:2025-02-13

    申请号:US18723717

    申请日:2022-12-16

    Abstract: An emulsion polymerization process of manufacturing a graft polymer composition with a reduced residual monomer content includes feeding a vinyl aromatic monomer, an unsaturated nitrile, and a first portion of an initiator to a reactor having a temperature of 50 to 63° C., the reactor containing an initial reaction system comprising water and a diene emulsion. After 10% to 35% of the first portion of the initiator has been added, the reactor temperature is increased to 65 to 85° C. The polymerization reaction runs for 0 to 30 minutes, then a second portion of the initiator and a third monomer are added, and the reaction is allowed to proceed for a second non-charging reaction time to produce the graft polymer composition. In the process, the vinyl aromatic monomer and the unsaturated nitrile are fed to the reactor in 10 to 40 minutes. The process time can be less than 145 minutes.

    AUTOMOTIVE INTERIOR PART WITH LOW ODOR

    公开(公告)号:US20240425699A1

    公开(公告)日:2024-12-26

    申请号:US18211957

    申请日:2023-06-20

    Inventor: Sijun Li Xinjun Di

    Abstract: The present invention relates to an automotive interior article comprising or consisting of a thermoplastic composition, said composition comprising, based on the weight of the composition, (A) from 85-99 wt. % of aromatic polycarbonate, (B) from 1.0-10 wt. % of un-modified polyolefin elastomer, (C) from 0.1-5 wt. % of a copolymer comprising ethylene and glycidyl (meth)acrylate moieties, (D) from 0-5 wt. % of further component(s), wherein i) the sum of components (A)-(D) is 100 wt. %, ii) component (D) does not comprise polyester, iii) the thermoplastic composition is selected to have a sensory impression of smell determined in accordance with VDA 270-B3 of at most 3.0.

    METHOD FOR FLUSHING REACTOR
    10.
    发明申请

    公开(公告)号:US20240383019A1

    公开(公告)日:2024-11-21

    申请号:US18690000

    申请日:2022-09-06

    Abstract: The disclosure provides a flushing process for removing polymer fouling from a reactor including a gas distributor proximal to the bottom thereof and an internal condenser proximal to the top thereof, the method including, for a first flushing time period, injecting a flushing solvent into the reactor and withdrawing the flushing solvent from a reactor outlet proximal to the internal condenser to induce an upward movement of flushing solvent, the withdrawn flushing solvent containing a first polymer content. After the first flushing time period is complete, for a second flushing time period, the process includes injecting a flushing solvent into the reactor and withdrawing the flushing solvent from a reactor outlet proximal to the gas distributor to induce a downward movement of flushing solvent, the withdrawn flushing solvent containing a second polymer content.