摘要: A composite material includes polyimide and at least about 55 wt % non-carbonaceous filler. The composite material has a tensile strength at least about 44.9 MPa.
摘要翻译: 复合材料包括聚酰亚胺和至少约55重量%的非碳质填料。 该复合材料具有至少约44.9MPa的拉伸强度。
-
公开(公告)号:US20070152195A1
公开(公告)日:2007-07-05
申请号:US11324153
申请日:2005-12-30
申请人: Pawel Czubarow , Mark Beltz , Oh-Hun Kwon , Gwo Swei
发明人: Pawel Czubarow , Mark Beltz , Oh-Hun Kwon , Gwo Swei
IPC分类号: H01B1/12
CPC分类号: C08J3/20 , C08J2379/08 , C08K3/01 , C08K3/14 , C08K3/22 , H01L21/6833 , C08L79/08
摘要: A method of forming an electrostatic dissipative composite material includes preparing a mixture comprising a polyamic acid precursor and a non-carbonaceous resistivity modifier. The polyamic acid precursor reacts to form polyamic acid. The method also includes dehydrating the polyamic acid to form polyimide. The polyimide forms a polymer matrix in which the non-carbonaceous resistivity modifier is dispersed.
摘要翻译: 形成静电耗散复合材料的方法包括制备包含聚酰胺酸前体和非碳质电阻率改性剂的混合物。 聚酰胺酸前体反应形成聚酰胺酸。 该方法还包括使聚酰胺酸脱水以形成聚酰亚胺。 聚酰亚胺形成其中非碳质电阻率改性剂分散的聚合物基质。
-
公开(公告)号:US20080042107A1
公开(公告)日:2008-02-21
申请号:US11507062
申请日:2006-08-18
申请人: Pawel Czubarow , Gwo Swei , Oh-Hun Kwon
发明人: Pawel Czubarow , Gwo Swei , Oh-Hun Kwon
IPC分类号: H01B1/12
CPC分类号: H01B1/08 , H01B1/12 , Y10T428/13 , Y10T428/25 , Y10T428/26 , Y10T428/31504
摘要: A composite material including a thermoplastic polymer matrix and a non-carbonaceous resistivity modifier dispersed in the thermoplastic polymer matrix. The composite material has a surface resistivity of about 1.0×104 ohm/sq to about 1.0×1011 ohm/sq and at least a portion of a surface of the composite material has a surface roughness (Ra) not greater than about 500 nm.
摘要翻译: 一种复合材料,包括分散在热塑性聚合物基质中的热塑性聚合物基质和非碳质电阻率改性剂。 复合材料具有约1.0×10 4欧姆/平方至约1.0×10 11欧姆/平方的表面电阻率,复合材料表面的至少一部分具有 表面粗糙度(Ra)不大于约500nm。
-
公开(公告)号:US07476339B2
公开(公告)日:2009-01-13
申请号:US11507062
申请日:2006-08-18
申请人: Pawel Czubarow , Gwo Swei , Oh-Hun Kwon
发明人: Pawel Czubarow , Gwo Swei , Oh-Hun Kwon
CPC分类号: H01B1/08 , H01B1/12 , Y10T428/13 , Y10T428/25 , Y10T428/26 , Y10T428/31504
摘要: A composite material including a thermoplastic polymer matrix and a non-carbonaceous resistivity modifier dispersed in the thermoplastic polymer matrix. The composite material has a surface resistivity of about 1.0×104 ohm/sq to about 1.0×1011 ohm/sq and at least a portion of a surface of the composite material has a surface roughness (Ra) not greater than about 500 nm.
摘要翻译: 一种复合材料,包括分散在热塑性聚合物基质中的热塑性聚合物基质和非碳质电阻率改性剂。 复合材料具有约1.0×10 4欧姆/平方至约1.0×10 11欧姆/平方的表面电阻率,复合材料表面的至少一部分表面粗糙度(Ra)不大于约500nm。
-
公开(公告)号:US20070154717A1
公开(公告)日:2007-07-05
申请号:US11324022
申请日:2005-12-30
申请人: Mark Beltz , Gwo Swei , Pawel Czubarow
发明人: Mark Beltz , Gwo Swei , Pawel Czubarow
IPC分类号: B32B9/04
CPC分类号: C08G73/1067 , C08G73/105 , C08G73/1071 , C08K3/22 , C08K3/2279 , C08L79/08 , Y10T428/31504
摘要: A composite material includes polyimide and about 0.1 wt % to about 50.0 wt % metal oxide. The composite material has a thermal oxidative performance at least about 5% relative to the polyimide absent metal oxide, the thermal oxidative performance determined based on exposure to air at atmospheric pressure and a temperature of 371° C. for a period of 120 hours.
摘要翻译: 复合材料包括聚酰亚胺和约0.1重量%至约50.0重量%的金属氧化物。 该复合材料相对于不存在金属氧化物的聚酰亚胺具有至少约5%的热氧化性能,该热氧化性能基于在大气压下暴露于空气和371℃的温度下测定120小时。
-
公开(公告)号:US20070155949A1
公开(公告)日:2007-07-05
申请号:US11323979
申请日:2005-12-30
申请人: Mark Beltz , Gwo Swei , Pawel Czubarow
发明人: Mark Beltz , Gwo Swei , Pawel Czubarow
IPC分类号: C08G69/08
CPC分类号: C08G73/101
摘要: A composite material includes polyimide and an additive. The composite material has a glass transition temperature at least about 5% greater than the glass transition temperature of the polyimide absent the additive, the composite material has a thermal oxidative performance at least about 5% relative to the polyimide absent the additive, the thermal oxidative performance based on exposure to air at a temperature of 371° C. and at atmospheric pressure for a period of 120 hours.
摘要翻译: 复合材料包括聚酰亚胺和添加剂。 复合材料的玻璃化转变温度比不含添加剂的聚酰亚胺的玻璃化转变温度大至少约5%,复合材料的热氧化性能相对于不含添加剂的聚酰亚胺至少约5%,热氧化 基于在371℃的温度和大气压下暴露于空气120小时的性能。
-
公开(公告)号:US20230117290A1
公开(公告)日:2023-04-20
申请号:US18076845
申请日:2022-12-07
IPC分类号: H10N10/17 , B64D41/00 , H10N10/13 , H10N10/854
摘要: Methods of making various fibers are provided including co-axial fibers with oppositely doped cladding and core are provide; hollow core doped silicon carbide fibers are provided; and doubly clad PIN junction fibers are provided. Additionally methods are provided for forming direct PN junctions between oppositely doped fibers are provided. Various thermoelectric generators that incorporate the aforementioned fibers are provided.
-
公开(公告)号:US08344523B2
公开(公告)日:2013-01-01
申请号:US12512976
申请日:2009-07-30
申请人: Raymond L. Dietz , Maciej Patelka , Akito Yoshii , Pawel Czubarow , Takashi Sakamoto , Yukinari Abe
发明人: Raymond L. Dietz , Maciej Patelka , Akito Yoshii , Pawel Czubarow , Takashi Sakamoto , Yukinari Abe
IPC分类号: H01B1/22
CPC分类号: C09J9/02 , C08K3/08 , C08K7/18 , C09J11/04 , H01L24/29 , H01L24/83 , H01L2224/2919 , H01L2224/29311 , H01L2224/29339 , H01L2224/29344 , H01L2224/29347 , H01L2224/29364 , H01L2224/29369 , H01L2224/83801 , H01L2224/8384 , H01L2924/01005 , H01L2924/01006 , H01L2924/01011 , H01L2924/01029 , H01L2924/01033 , H01L2924/01046 , H01L2924/01047 , H01L2924/0105 , H01L2924/01074 , H01L2924/01078 , H01L2924/01079 , H01L2924/0665 , H01L2924/10253 , H01L2924/12044 , H01L2924/15787 , H01L2924/00
摘要: Conductive compositions which are useful as thermally conductive compositions and may also be useful as electrically conductive compositions are provided. The compositions include a conductive particle constituent in combination with a sintering aid which can, for example be a compound of the same metal in the nanometal, an organo-metallic, a metalorganic salt, mercaptan and/or resinate. In some embodiments the conductive particles include a small amount of nanoscale (
摘要翻译: 提供可用作导热组合物并且也可用作导电组合物的导电组合物。 组合物包括与烧结助剂组合的导电颗粒组分,其可以例如是纳米金属中相同金属的化合物,有机金属,金属有机盐,硫醇和/或树脂酸盐。 在一些实施方案中,导电颗粒包括少量的纳米级(<200nm)颗粒。 组合物表现出增加的导热性。
-
公开(公告)号:US06663704B2
公开(公告)日:2003-12-16
申请号:US09898942
申请日:2001-07-03
申请人: Jean L. Spencer , Pawel Czubarow , Yoojeong Kim
发明人: Jean L. Spencer , Pawel Czubarow , Yoojeong Kim
IPC分类号: C09D1100
摘要: Pearlescent inks are provided. The inks are suitable for use in writing instruments, and include a dispersion of a pearlescent pigment in a solvent. Some inks are erasable and/or shear-thinning.
-
10.
公开(公告)号:US6030681A
公开(公告)日:2000-02-29
申请号:US890912
申请日:1997-07-10
申请人: Pawel Czubarow , Karin M. Kinsman , Amy S. Chu , Christian Weber , Ryan Dupon , Anthony Evans
发明人: Pawel Czubarow , Karin M. Kinsman , Amy S. Chu , Christian Weber , Ryan Dupon , Anthony Evans
CPC分类号: C04B41/009 , C04B41/5098 , C04B41/52 , C04B41/85 , C04B41/89 , G11B5/8404 , C04B2111/00844 , Y10S428/90 , Y10T428/265
摘要: A method of forming an article having a cermet layer on a porcelain substrate, via the steps of (a) providing a substrate made a porcelain comprising one or more crystalline oxide phases dispersed in a glassy matrix, the glassy matrix containing 0.25 to 45.0 weight % of a reducible metal oxide having a reduction potential of between -1.0 and +3.5 E.degree./V; and (b) heating the substrate in a reducing atmosphere to form on at least one surface of the substrate a layer of cermet comprising elemental metal which is a reduction product of the reducible metal oxide. The article may be used as a substrate for magnetic recording disks.
摘要翻译: 一种通过以下步骤形成具有金属陶瓷层的制品的方法:(a)提供制备包含分散在玻璃状基质中的一种或多种结晶氧化物相的瓷的基材,所述玻璃质基质含有0.25〜45.0重量% 的还原电位在-1.0和+3.5E DEG / V之间的可还原金属氧化物; 和(b)在还原气氛中加热所述基材以在所述基材的至少一个表面上形成包含作为可还原金属氧化物的还原产物的元素金属的金属陶瓷层。 该物品可以用作磁记录盘的基片。
-
-
-
-
-
-
-
-
-