HIGH LIQUIDUS VISCOSITY BIOACTIVE GLASS

    公开(公告)号:US20220298058A1

    公开(公告)日:2022-09-22

    申请号:US17832208

    申请日:2022-06-03

    Abstract: Methods of making a bioactive glass fiber include forming a melt of a glass composition including: 50 to 70% SiO2; 0.1 to 10% Al2O3, 5 to 30% Na2O, 0.1 to 15% K2O, 0.1 to 15% MgO, 0.1 to 20% CaO, and 5 to 10% P2O5, based on a 100 wt % of the glass composition. The melt has a viscosity of from 200 Poise to 2,000 Poise. Methods include drawing the melt into a drawn glass fiber. Bioactive glass compositions include: 60 to 70% SiO2; 15 to 30% Na2O, 5 to 15% K2O, 1 to 10% CaO, and 5 to 10% P2O5, based on a 100 wt % of the glass composition.