公开(公告)号:US20170081481A1
公开(公告)日:2017-03-23
申请号:US15119857
申请日:2015-02-16
申请人: BASF SE
发明人: Joerg ERBES , Gerhard LANGE , Tobias KORTEKAMP , Bernhard LINNER , Cecile SCHNEIDER , Angela ULZHOEFER , Robert KEINZ , Michael Klemens MUELLER
CPC分类号: C08J3/14 , B29B13/065 , C08J3/12 , C08J2381/06 , F26B3/08 , F26B5/14 , F26B2200/08
摘要: The present invention relates to a process for drying particulate polymers, comprising the steps of: a) providing a particulate polymer comprising from 60 wt % to 90 wt % of at least one solvent based on the total weight of particulate polymer and solvent, b) mechanically predrying the particulate polymer to a content of the at least one solvent of from 20 wt % to 50 wt % based on the total weight of particulate polymer and solvent, wherein the mechanical predrying in step b) is carried out with a roller press, and c) end-drying the particulate polymer to a content of the at least one solvent of from 0 wt % to 15 wt % based on the total weight of particulate polymer and solvent, wherein the particulate polymer is a polymer comprising repeating units of formulae I, II and/or III The present invention further relates to a process for working up particulate polymers.
-
公开(公告)号:US20160215105A1
公开(公告)日:2016-07-28
申请号:US14904610
申请日:2014-07-16
申请人: BASF SE
发明人: Joerg ERBES , Gerhard LANGE , Tobias KORTEKAMP , Cecile SCHNEIDER
CPC分类号: C08J3/14 , C08G65/46 , C08G75/23 , C08J2371/10 , C08J2381/06
摘要: Process for producing polyarylene ether beads from a polyarylene ether solution, comprising the steps of i) dividing the polyarylene ether solution into droplets, ii) transferring the droplets into a precipitation bath to form polyarylene ether beads in the precipitation bath which (A) comprises at least one aprotic solvent (component (1)) and at least one protic solvent (component (2)), (B) has a temperature of 0° C. to Tc, where the critical temperature Tc in [° C.] can be determined by the numerical equation Tc=(99−c)/0.61 in which c is the concentration of component (1) in the precipitation bath in [% by weight] and (C) has component (1) in concentrations of 5% by weight to cc, where the critical concentration cc in [% by weight] can be determined by the numerical equation cc=99−0.61*T in which T is the temperature in the precipitation bath in [° C], where the percentages by weight are each based on the sum of the percentages by weight of component (1) and of component (2) in the precipitation bath.
摘要翻译: 用于从聚亚芳基醚溶液制备聚亚芳基醚珠粒的方法,包括以下步骤:i)将聚亚芳基醚溶液分成液滴,ii)将沉淀液转移到沉淀浴中,以在沉淀槽中形成聚亚芳基醚珠粒,其中(A) 至少一种非质子溶剂(组分(1))和至少一种质子溶剂(组分(2)),(B)具有0℃至Tc的温度,其中[℃]中的临界温度Tc可以 通过数值方程Tc =(99-c)/0.61确定,其中c是沉淀浴中组分(1)的浓度[重量%],(C)的组分(1)的浓度为5% 重量至cc,其中[重量%]中的临界浓度cc可以通过数值方程式cc = 99-0.61 * T确定,其中T是沉淀浴中的温度[℃],其中重量百分数 分别基于组分(1)和组分(2)i的重量百分比的总和i 沉淀浴。
-
公开(公告)号:US20160214068A1
公开(公告)日:2016-07-28
申请号:US14917488
申请日:2014-09-04
申请人: BASF SE
发明人: Martin WEBER , Christian MALETZKO , Joerg ERBES , Tobias KORTEKAMP , Bastiaan Bram, Pieter STAAL , Thomas HEIL
CPC分类号: B01D71/68 , B01D67/0006 , B01D69/08 , B29C47/0011 , B29C47/0014 , B29C47/0026 , B29C47/8895 , B29K2081/06 , B29L2031/755 , C08G65/4056 , C08G75/23
摘要: The present invention relates to a method of forming a polyarylene ether sulfone polymer by converting a reaction mixture (RG) comprising a dihalogen component (A1), a dihydroxy component (B1) and potassium carbonate (C1) having a volume-average particle size of
摘要翻译: 本发明涉及通过将含有二卤代物(A1),二羟基成分(B1)和碳酸钾(C1)的反应混合物(RG)转化成具有体积平均粒径的聚亚芳基醚砜聚合物的方法 <25μm。 本发明还涉及通过所述方法获得的聚亚芳基醚砜聚合物可从所述聚芳醚砜聚合物获得的产物和由所述聚亚芳基醚砜聚合物形成的膜。
-
公开(公告)号:US20160208056A1
公开(公告)日:2016-07-21
申请号:US14904491
申请日:2014-07-16
申请人: BASF SE
发明人: Joerg ERBES , Gerhard LANGE , Tobias KORTEKAMP , Cecile SCHNEIDER
CPC分类号: C08J3/14 , C08G65/46 , C08G75/23 , C08J3/12 , C08J2381/06
摘要: Process for producing polyarylene ether beads from a polyarylene ether solution, comprising the steps of i) dividing the polyarylene ether solution into droplets, ii) transferring the droplets into a precipitation bath to form polyarylene ether beads in the precipitation bath which (A) comprises at least one aprotic solvent (component (1)) and at least one protic solvent (component (2)), (B) has a temperature of 0° C. to Tc, where the critical temperature Tc in [° C.] can be determined by the numerical equation Tc=(77−c)/0.58 in which c is the concentration of component (1) in the precipitation bath in [% by weight] and (C) has component (1) in concentrations of 5% by weight to cc, where the critical concentration cc in [% by weight] can be determined by the numerical equation cc=77−0.58*T in which T is the temperature in the precipitation bath in [° C.], where the percentages by weight are each based on the sum of the percentages by weight of component (1) and of component (2) in the precipitation bath.
摘要翻译: 用于从聚亚芳基醚溶液制备聚亚芳基醚珠粒的方法,包括以下步骤:i)将聚亚芳基醚溶液分成液滴,ii)将沉淀液转移到沉淀浴中,以在沉淀槽中形成聚亚芳基醚珠粒,其中(A) 至少一种非质子溶剂(组分(1))和至少一种质子溶剂(组分(2)),(B)具有0℃至Tc的温度,其中[℃]中的临界温度Tc可以 通过数值方程Tc =(77-c)/0.58确定,其中c是沉淀浴中组分(1)的浓度[重量%],(C)中组分(1)的浓度为5% 重量至cc,其中[重量%]的临界浓度cc可以通过数值方程式cc = 77-0.58 * T确定,其中T是沉淀浴中的温度[℃],其中百分比由 重量分别基于组分(1)和组分(2)的重量百分比的总和, 在沉淀浴中。
-
公开(公告)号:US20160159990A1
公开(公告)日:2016-06-09
申请号:US14904614
申请日:2014-07-16
申请人: BASF SE
发明人: Joerg ERBES , Stefan MUESSIG , Tobias KORTEKAMP , Marco KRUEGER , Markus STEFFEN , Angela ULZHOEFER , Cecile SCHNEIDER , Alexandra WIEDEMANN , Simon GRAMLICH
CPC分类号: C08J3/14 , B29C47/0011 , B29K2081/06 , C08G65/46 , C08G75/23 , C08J3/12 , C08J2381/06 , C08J2381/08
摘要: The invention relates to a process for producing polyarylene ether beads from a polyarylene ether solution, comprising the steps of i) dividing the polyarylene ether solution in a division apparatus which is made to vibrate with a frequency of 10 to 1400 Hz to obtain droplets, ii) transferring the droplets into a precipitation bath to form polyarylene ether beads in the precipitation bath which (A) comprises at least one aprotic solvent (component (1)) and at least one protic solvent (component (2)), (B) has a temperature of 0° C. to Tc, where the critical temperature Tc in [° C.] can be determined by the numerical equation Tc=(77−c)/0.58 in which c is the concentration of component (1) in the precipitation bath in [% by weight] and (C) has component (1) in concentrations of 5% by weight to cc, where the critical concentration cc in [% by weight] can be determined by the numerical equation cc=77−0.58*T in which T is the temperature in the precipitation bath in [° C.], where the percentages by weight are each based on the sum of the percentages by weight of component (1) and of component (2) in the precipitation bath.
摘要翻译: 本发明涉及一种由聚亚芳基醚溶液制备聚亚芳基醚珠粒的方法,包括以下步骤:i)将分散装置中的聚亚芳基醚溶液除以10-1400Hz的频率振动得到液滴,ii (A)包含至少一种非质子溶剂(组分(1))和至少一种质子溶剂(组分(2)),(B)具有至少一种质子溶剂 0℃至Tc的温度,其中[℃]中的临界温度Tc可以通过数值方程Tc =(77-c)/0.58确定,其中c是组分(1)中的浓度 沉淀浴中的[重量%]和(C)的组分(1)的浓度为5重量%〜cc,其中临界浓度cc [重量%]可以通过数学式cc = 77-0.58 * T,其中T是沉淀浴中的温度[℃],其中 重量百分比分别基于沉淀浴中组分(1)和组分(2)的重量百分比之和。
-
-
-
-