Stainless steel sheet with excellent heat and corrosion resistances for brake disk
    2.
    发明授权
    Stainless steel sheet with excellent heat and corrosion resistances for brake disk 有权
    不锈钢板对制动盘具有优良的耐热和耐腐蚀性能

    公开(公告)号:US08852361B2

    公开(公告)日:2014-10-07

    申请号:US11794966

    申请日:2005-10-20

    CPC classification number: F16D65/125 F16D2200/0017 F16D2200/0021

    Abstract: A stainless steel sheet with excellent heat and corrosion resistances for a brake disk is provided. Specifically, in mass %, C: less than 0.10%, Si: 1.0% or less, Mn: 1.0 to 2.5%, P: 0.04% or less, S: 0.01% or less, Cr: more than 11.5% but not more than 15.0%, Ni: 0.1 to 1.0%, Al: 0.10% or less, Nb: more than 0.08% but not more than 0.6%, V: 0.02 to 0.3%, and N: more than 0.03% but not more than 0.10% are contained so that 0.03≦{C+N−(13/93)Nb}≦0.10, (5Cr+10Si+15Mo+30Nb+50V−9Ni−5Mn−3Cu−225N−270C)≦45, and {(14/50)V+(14/90)Nb}

    Abstract translation: 提供了一种对制动盘具有优异耐热腐蚀性能的不锈钢板。 具体地,以质量%计,C:小于0.10%,Si:1.0%以下,Mn:1.0〜2.5%,P:0.04%以下,S:0.01%以下,Cr:超过11.5% ,15.0%以下,Ni:0.1〜1.0%,Al:0.10%以下,Nb:0.08%以上0.6%以下,V:0.02〜0.3%,N:0.03以上0.10以下 含有0.03和n C; N(C + N - (13/93)Nb}≦̸ 0.10,(5Cr + 10Si + 15Mo + 30Nb + 50V-9Ni-5Mn-3Cu-225N-270C) {(14/50)V +(14/90)Nb}

    Soft Cr-containing steel
    3.
    再颁专利
    Soft Cr-containing steel 有权
    含软含铬钢

    公开(公告)号:USRE44709E1

    公开(公告)日:2014-01-21

    申请号:US12465286

    申请日:2009-05-13

    Abstract: The soft Cr-containing steel includes, on a % by mass basis, C: from about 0.001% to about 0.020%, Si: more than about 0.10% and less than about 0.50%, Mn: less than about 2.00%, P: less than about 0.060%, S: less than about 0.008%, Cr: from about 12.0% to about 16.0%, Ni: from about 0.05% to about 1.00%, N: less than about 0.020%, Nb: from about 10×(C+N) to about 1.00%, Mo: more than about 0.80% and less than about 3.00%, wherein the contents of alloying elements, represented by Si and Mo, respectively, on a % by mass, satisfy the formula Si≦1.2-0.4 Mo, so as to prevent precipitation of the Laves phase and to stably secure an effect of increasing high-temperature strength due to solid solution Mo.

    Abstract translation: 含有软Cr的钢包括以质量%计,C:约0.001%至约0.020%,Si:大于约0.10%且小于约0.50%,Mn:小于约2.00%,P: 小于约0.060%,S:小于约0.008%,Cr:约12.0%至约16.0%,Ni:约0.05%至约1.00%,N:小于约0.020%,Nb:约10× (C + N)至约1.00%,Mo:大于约0.80%且小于约3.00%,其中由Si和Mo表示的合金元素的含量分别为质量%满足式Si @ 1.2-0.4 Mo,以防止Laves相沉淀,并稳定地确保由于固溶Mo而使高温强度提高的效果。

    Soft Cr-containing steel
    4.
    发明授权
    Soft Cr-containing steel 有权
    含软含铬钢

    公开(公告)号:US07341690B2

    公开(公告)日:2008-03-11

    申请号:US10729904

    申请日:2003-12-09

    Abstract: The soft Cr-containing steel includes, on a % by mass basis, C: from about 0.001% to about 0.020%, Si: more than about 0.10% and less than about 0.50%, Mn: less than about 2.00%, P: less than about 0.060%, S: less than about 0.008%, Cr: from about 12.0% to about 16.0%, Ni: from about 0.05% to about 1.00%, N: less than about 0.020%, Nb: from about 10×(C+N) to about 1.00%, Mo: more than about 0.80% and less than about 3.00%, wherein the contents of alloying elements, represented by Si and Mo, respectively, on a % by mass, satisfy the formula Si≦1.2−0.4Mo, so as to prevent precipitation of the Laves phase and to stably secure an effect of increasing high-temperature strength due to solid solution Mo.

    Abstract translation: 含有软Cr的钢包括以质量%计,C:约0.001%至约0.020%,Si:大于约0.10%且小于约0.50%,Mn:小于约2.00%,P: 小于约0.060%,S:小于约0.008%,Cr:约12.0%至约16.0%,Ni:约0.05%至约1.00%,N:小于约0.020%,Nb:约10x C + N)至约1.00%,Mo:大于约0.80%且小于约3.00%,其中由Si和Mo表示的合金元素的含量分别为质量%满足式Si < 1.2-0.4Mo,以防止Laves相沉淀,并稳定地确保由于固溶Mo而使高温强度提高的效果。

    Martensitic stainless steel for disk brakes
    5.
    发明申请
    Martensitic stainless steel for disk brakes 有权
    马氏体不锈钢用于盘式制动器

    公开(公告)号:US20060113008A1

    公开(公告)日:2006-06-01

    申请号:US10546248

    申请日:2004-04-23

    Abstract: A martensitic stainless steel, having high temper softening resistance, for disc brakes is provided. The martensitic stainless steel is not seriously softened by maintaining the steel at more than 600° C. The steel has a hardness of 32 or more or a hardness of 30 or more in HRC after the steel is tempered at 650° C. for one hour or tempered at 670° C. for one hour, respectively. In particular, the martensitic stainless steel for disc brakes contains less than 0.050 mass % carbon, 1.0 mass % or less silicon, 2.0 mass % or less manganese, 0.04 mass % or less phosphorus, 0.010 mass % or less sulfur, 0.2 mass % or less aluminum, more than 11.5 mass % to 15.0 mass % chromium, 0.5 mass % to 2.0 mass % nickel, more than 0.50 mass % to 4.0 mass %. copper, more than 0.08 mass % to 0.6 mass % niobium, and less than 0.09 mass % nitrogen, the remainder being iron and unavoidable impurities. The carbon content, the nitrogen content, the niobium content, the chromium content, the silicon content, the nickel content, the manganese content, and the copper content satisfy the following inequalities (1) and (2): 0.03≦[C]+[N]−13/93×[Nb]≦0.09   (1) 5×[Cr]+10×[Si]+30×[Nb]−9×[Ni]−5×[Mn]−3×[Cu]−225×[N]−270×[C]≦40   (2).

    Abstract translation: 提供了具有高回火软化阻力的马氏体不锈钢用于盘式制动器。 通过将钢保持在600℃以上,马氏体系不锈钢不会严重软化。钢在650℃回火1小时后,HRC中的硬度为32以上,硬度为30以上。 或分别在670℃回火1小时。 特别是用于盘式制动器的马氏体不锈钢含有小于0.050质量%的碳,1.0质量%以下的硅,2.0质量%以下的锰,0.04质量%以下的磷,0.010质量%以下的硫,0.2质量%或 大于11.5质量%至15.0质量%的铬,0.5质量%至2.0质量%的镍,大于0.50质量%至4.0质量%。 铜,0.08质量%〜0.6质量%的铌,小于0.09质量%的氮,余量为铁和不可避免的杂质。 碳含量,氮含量,铌含量,铬含量,硅含量,镍含量,锰含量和铜含量满足以下不等式(1)和(2):< 公式描述=“在线公式”end =“lead”?> 0.03 <= [C] + [N] -13 / 93x [Nb] <= 0.09(1)<?in-line-formula description =“In “公式”end =“tail”?> <?in-line-formula description =“In-line Formulas”end =“lead”?> 5x [Cr] + 10x [Si] + 30x [Nb] -9x [ Ni] -5x [Mn] -3x [Cu] -225x [N] -270x [C] <= 40(2)。 <?in-line-formula description =“In-line Formulas”end =“tail”?>

    Soft Cr-containing steel
    6.
    发明授权
    Soft Cr-containing steel 无效
    含软含铬钢

    公开(公告)号:US06740174B2

    公开(公告)日:2004-05-25

    申请号:US09987327

    申请日:2001-11-14

    Abstract: The soft Cr-containing steel includes, on a % by mass basis, C: from about 0.001% to about 0.020%, Si: more than about 0.10% and less than about 0.50%, Mn: less than about 2.00%, P: less than about 0.060%, S: less than about 0.008%, Cr: from about 12.0% to about 16.0%, Ni: from about 0.05% to about 1.00%, N: less than about 0.020%, Nb: from about 10×(C+N) to about 1.00%, Mo: more than about 0.80% and less than about 3.00%, wherein the contents of alloying elements, represented by Si and Mo, respectively, on a % by mass, satisfy the formula Si ≦1.2−0.4 Mo, so as to prevent precipitation of the Laves phase and to stably secure an effect of increasing high-temperature strength due to solid solution Mo.

    Abstract translation: 含有软Cr的钢包括以质量%计,C:约0.001%至约0.020%,Si:大于约0.10%且小于约0.50%,Mn:小于约2.00%,P: 小于约0.060%,S:小于约0.008%,Cr:约12.0%至约16.0%,Ni:约0.05%至约1.00%,N:小于约0.020%,Nb:约10x C + N)至约1.00%,Mo:大于约0.80%且小于约3.00%,其中由Si和Mo表示的合金元素的含量分别为质量%满足式Si < 1.2-0.4 Mo,以防止Laves相沉淀,并稳定地确保由于固溶Mo而使高温强度提高的效果。

    Martensitic stainless steel for disk brakes
    7.
    发明授权
    Martensitic stainless steel for disk brakes 有权
    马氏体不锈钢用于盘式制动器

    公开(公告)号:US08357247B2

    公开(公告)日:2013-01-22

    申请号:US10546248

    申请日:2004-04-23

    Abstract: A martensitic stainless steel, having high temper softening resistance, for disc brakes is provided. The martensitic stainless steel is not seriously softened by maintaining the steel at more than 600° C. The steel has a hardness of 32 or more or a hardness of 30 or more in HRC after the steel is tempered at 650° C. for one hour or tempered at 670° C. for one hour, respectively. In particular, the martensitic stainless steel for disc brakes contains less than 0.050 mass % carbon, 1.0 mass % or less silicon, 2.0 mass % or less manganese, 0.04 mass % or less phosphorus, 0.010 mass % or less sulfur, 0.2 mass % or less aluminum, more than 11.5 mass % to 15.0 mass % chromium, 0.5 mass % to 2.0 mass % nickel, more than 0.50 mass % to 4.0 mass %. copper, more than 0.08 mass % to 0.6 mass % niobium, and less than 0.09 mass % nitrogen, the remainder being iron and unavoidable impurities. The carbon content, the nitrogen content, the niobium content, the chromium content, the silicon content, the nickel content, the manganese content, and the copper content satisfy the following inequalities (1) and (2): 0.03≦[C]+[N]−13/93×[Nb]≦0.09   (1) 5×[Cr]+10×[Si]+30×[Nb]−9×[Ni]−5×[Mn]−3×[Cu]−225×[N]−270×[C]≦40   (2).

    Abstract translation: 提供了具有高回火软化阻力的马氏体不锈钢用于盘式制动器。 通过将钢保持在600℃以上,马氏体系不锈钢不会严重软化。钢在650℃回火1小时后,HRC中的硬度为32以上,硬度为30以上。 或分别在670℃回火1小时。 特别是用于盘式制动器的马氏体不锈钢含有小于0.050质量%的碳,1.0质量%以下的硅,2.0质量%以下的锰,0.04质量%以下的磷,0.010质量%以下的硫,0.2质量%或 大于11.5质量%至15.0质量%的铬,0.5质量%至2.0质量%的镍,大于0.50质量%至4.0质量%。 铜,0.08质量%〜0.6质量%的铌,小于0.09质量%的氮,余量为铁和不可避免的杂质。 碳含量,氮含量,铌含量,铬含量,硅含量,镍含量,锰含量和铜含量满足以下不等式(1)和(2):0.03&nlE; [C] + [N] -13 / 93×[Nb]&nlE; 0.09(1)5×[Cr] + 10×[Si] + 30×[Nb] -9×[Ni] -5×[Mn] [Cu] -225×[N] -270×[C]&nlE; 40(2)。

    Stainless Steel Sheet with Excellent Heat and Corrosion Resistances for Brake Disk
    9.
    发明申请
    Stainless Steel Sheet with Excellent Heat and Corrosion Resistances for Brake Disk 有权
    不锈钢板具有优良的耐热性和制动盘的耐腐蚀性

    公开(公告)号:US20080000737A1

    公开(公告)日:2008-01-03

    申请号:US11794966

    申请日:2005-10-20

    CPC classification number: F16D65/125 F16D2200/0017 F16D2200/0021

    Abstract: A stainless steel sheet with excellent heat and corrosion resistances for a brake disk is provided. Specifically, in mass %, C: less than 0.10%, Si: 1.0% or less, Mn: 1.0 to 2.5%, P: 0.04% or less, S: 0.01% or less, Cr: more than 11.5% but not more than 15.0%, Ni: 0.1 to 1.0%, Al: 0.10% or less, Nb: more than 0.08% but not more than 0.6%, V: 0.02 to 0.3%, and N: more than 0.03% but not more than 0.10% are contained so that 0.03≦{C+N−(13/93)Nb}≦0.10, (5Cr+10Si+15Mo+30Nb+50V−9Ni−5Mn−3Cu−225N−270C)≦45, and {(14/50)V+(14/90)Nb}

    Abstract translation: 提供了一种对制动盘具有优异耐热腐蚀性能的不锈钢板。 具体地,以质量%计,C:小于0.10%,Si:1.0%以下,Mn:1.0〜2.5%,P:0.04%以下,S:0.01%以下,Cr:超过11.5% ,15.0%以下,Ni:0.1〜1.0%,Al:0.10%以下,Nb:0.08%以上0.6%以下,V:0.02〜0.3%,N:0.03以上0.10以下 含有0.03≤{C + N-(13/93)Nb}≤0.10,(5Cr + 10Si + 15Mo + 30Nb + 50V-9Ni-5Mn-3Cu-225N-270C)= 45,以及 {(14/50)V +(14/90)Nb}