MULTICOMPONENT FIBER COMPRISING A PHASE CHANGE MATERIAL
    74.
    发明申请
    MULTICOMPONENT FIBER COMPRISING A PHASE CHANGE MATERIAL 审中-公开
    包含相变材料的多层纤维

    公开(公告)号:US20070089276A1

    公开(公告)日:2007-04-26

    申请号:US11532145

    申请日:2006-09-15

    IPC分类号: D01G27/00

    摘要: The present invention is a multicomponent fiber comprising a temperature-regulating inner fiber component encapsulated by an outer fiber component. The invention further provides methods of preparing the inventive multicomponent fiber and methods of preparing a temperature-regulating fiber component incorporating at least one phase change material.

    摘要翻译: 本发明是一种多组分纤维,其包含由外纤维成分包封的温度调节内纤维成分。 本发明还提供了制备本发明的多组分纤维的方法和制备掺入至少一种相变材料的温度调节纤维组分的方法。

    Elastomeric fibers comprising controlled distribution block copolymers
    77.
    发明申请
    Elastomeric fibers comprising controlled distribution block copolymers 审中-公开
    包含受控分布嵌段共聚物的弹性纤维

    公开(公告)号:US20070055015A1

    公开(公告)日:2007-03-08

    申请号:US11219478

    申请日:2005-09-02

    IPC分类号: C08L53/00

    摘要: Bicomponent fibers comprising a thermoplastic polymer and an elastomeric compound are made which can be continuously extruded from the melt at high production rates. The elastomeric compound comprises a selectively hydrogenated block copolymer having a controlled distribution elastomeric block which has a mono alkenyl arene blockiness index of less than 40 mol % and high flow. Elastomeric fibers are also provided which comprise a controlled distribution block copolymer and a slip agent. The fibers are useful for the manufacture of articles such as woven fabrics, spunbond non-woven fabrics or filters, staple fibers, yarns and bonded, carded webs. The bicomponent fibers can be made using a process comprising coextrusion of the thermoplastic polymer and elastomeric compound to produce fibers at spinning speeds of at least 1000 mpm and having a denier from 0.1 to 50 g/9000 m.

    摘要翻译: 制备包含热塑性聚合物和弹性体化合物的双组分纤维,其可以以高生产率从熔体中连续挤出。 弹性体化合物包括具有受控分布的弹性体嵌段的选择性氢化嵌段共聚物,其具有小于40mol%的单链烯基芳烃嵌段指数和高流动性。 还提供弹性纤维,其包含受控分布嵌段共聚物和增滑剂。 纤维可用于制造诸如机织织物,纺粘非织造织物或过滤器,短纤维,纱线和粘合的梳理纤维网之类的制品。 双组分纤维可以使用包括共挤出热塑性聚合物和弹性体化合物以在纺丝速度为至少1000mpm并具有0.1-50g / 9000m的旦数的纤维的方法制备。

    Potential crimping composite fiber and method for production thereof, and fiber aggregate, and nonwoven fabric
    79.
    发明申请
    Potential crimping composite fiber and method for production thereof, and fiber aggregate, and nonwoven fabric 有权
    潜在卷曲复合纤维及其制造方法,纤维集合体,无纺布等

    公开(公告)号:US20070014987A1

    公开(公告)日:2007-01-18

    申请号:US10569666

    申请日:2004-08-26

    IPC分类号: D02G3/00

    摘要: A latently crimpable conjugate fiber is constructed using a first component containing an ethylene-α-olefin copolymer polymerized with a metallocene catalyst and a second component formed from a thermal plastic polymer having a melting point T2 higher than a melting point T1 of the first component, such that the first component is exposed with an exposed length of at least 20% relative to a peripheral length of the fiber, and which fiber has a single fiber dry heat shrinkage percentage of at least 50%, which is determined according to JIS-L-1015 (dry heat shrinkage percentage) at 100° C. under an initial tension of 0.018 mN/dtex (2 mg/d) for 15 minutes and a single fiber dry heat shrinkage percentage of at least 15%, which is determined under the same condition under an initial tension of 0.450 mN/dtex (50 mg/dtex) for 15 minutes. The latently crimpable conjugate fiber develops crimps and has thermal adhesiveness at a low temperature.

    摘要翻译: 使用含有与茂金属催化剂聚合的乙烯-α-烯烃共聚物的第一组分和由熔点比T 2高的热塑性聚合物形成的第二组分构成潜在可卷曲的复合纤维 使得第一组分相对于纤维的周长以暴露长度为至少20%的程度暴露,并且哪种纤维具有单纤维干热 在100℃,初始张力为0.018mN / dtex(2mg / d)下,按照JIS-L-1015(干热收缩率)测定15分钟的收缩率为50%以上,单次 纤维干热收缩率至少为15%,其在相同条件下在初始张力为0.450mN / dtex(50mg / dtex)下测定15分钟。 容易卷曲的复合纤维发生卷曲并在低温下具有热粘合性。