    摘要: The thermoplastic, isocyanate-free polyurethane which contains acidic groups, is soluble in tetrahydrofuran, has a molecular weight of from 15,000 to 70,000 and is composed ofA) 1 mol of a polyol having a molecular weight of from 400 to 4000,B) from 0.3 to 9 mol of a mixture ofB1) if required, a diol of 2 to 18 carbon atoms andB2) from 0.03 to 0.4 mol of a diol having at least one acidic group,C) from 0 to 1 mol of a polyol having 3 to 18 carbon atoms and at least 3 OH groups,D) from 1.25 to 13 mol of a diisocyanate of 6 to 30 carbon atoms andE) from 0 to 1 mol of a primary or secondary amino alcohol of 2 to 16 carbon atoms,the molar ratio of the OH and any NH groups present in the sum of the components A, B, C and E to the NCO groups of component D being from 0.98 to 1.4, is obtainable by reacting the above components in the melt and is suitable in particular as a binder for magnetic recording media.

    摘要翻译: 含有酸性基团的热塑性无异氰酸酯的聚氨酯可溶于四氢呋喃,其分子量为15,000至70,000,由A)1mol分子量为400至4000的多元醇组成,B)为 0.3〜9摩尔的B1)如果需要,2至18个碳原子的二醇和B2)0.03至0.4摩尔的具有至少一个酸性基团的二元醇,C)0至1摩尔多元醇 3至18个碳原子和至少3个OH基团,D)1.25至13摩尔的6至30个碳原子的二异氰酸酯和E)0至1摩尔的2至16个碳原子的伯或仲氨基醇, 存在于组分A,B,C和E的总和中的OH和组分D的NCO基团之间的OH和任何NH基团的摩尔比为0.98至1.4,可通过使熔体中的上述组分反应并且是合适的 特别是作为磁记录介质的粘合剂。

    Production of polyurethane moldings by the reaction injection molding
process
    20.
    再颁专利
    Production of polyurethane moldings by the reaction injection molding process 失效
    通过反应注塑成型工艺生产聚氨酯模塑制品

    公开(公告)号:USRE33609E

    公开(公告)日:1991-06-11

    申请号:US331874

    申请日:1989-03-31

    申请人: Neil H. Nodelman

    发明人: Neil H. Nodelman

    IPC分类号: C08G18/32 C08G18/38 C08G18/66

    摘要: The present invention is directed to a process for the production of polyurethane moldings by reacting a reaction mixture comprising(a) an organic polyisocyanate(b) a compatible polyol blend comprising(i) at least one polyether polyol having a hydroxyl functionality of from 2 to 8, and a molecular weight of from 350 to below 1800, and(ii) at least one hydroxyl functional organic material containing from 2 to 8 hydroxyl groups and having a molecular weight below 350, components (i) and (ii) being used in a weight ratio of component (b)(i) to (b)(ii) of from about 10:1 to about 1:10, and(iii) no more than 45% by weight based on the weight of component (b) of an active hydrogen containing compound having a molecular weight of 1800 or more,said reaction mixture being processed as a one-shot system by the RIM process at an isocyanate index of from about 70 to about 130.