Heterophasic propylene polymer material and propylene-based resin composition

    公开(公告)号:US11613601B2

    公开(公告)日:2023-03-28

    申请号:US16493562

    申请日:2018-03-12

    IPC分类号: C08F297/08 C08K3/34 C08L23/10

    摘要: A heterophasic propylene polymerization material, including a propylene polymer component (I) and an ethylene-α-olefin copolymer component (II), the heterophasic propylene polymerization material satisfying features (i) to (v): (i) the heterophasic propylene polymerization material contains a xylene-soluble content by 20 wt % or more; (ii) xylene-soluble content in the heterophasic propylene polymerization material has a limiting viscosity [η]CXS not less than 5 dL/g; (iii) a melt flow rate of the propylene polymer component (I) is 70 g/10 min or more; (iv) MFR of the heterophasic propylene polymerization material is not less than 5 g/10 min; and (v) the number of gels of 100 μm or more in diameter on a sheet for counting gels, including the heterophasic propylene polymerization material, is 1000 or less per 100 cm2 of the sheet.

    Composition and process
    9.
    发明授权

    公开(公告)号:US11427670B2

    公开(公告)日:2022-08-30

    申请号:US16348376

    申请日:2017-11-15

    申请人: BOREALIS AG

    IPC分类号: C08F297/08 C08K3/04

    摘要: A polymer composition and a process for the production of this composition comprising a base resin is disclosed herein. The base resin includes a very high molecular weight component, a low molecular weight component, and a high molecular weight component having a weight average molecular weight higher than the weight average molecular weight of the low molecular weight component but lower than the weight average molecular weight of the very high molecular weight component. An amount of the very high molecular weight component in the base resin is 0.5 to 8 wt %. The very high molecular weight component has a viscosity average molecular weight of greater than 1100 kg/mol. The composition has FRR21/5 of equal to or greater than 38, a melt flow rate MFR21 of equal to or greater than 6.5 g/10 min and a viscosity at a shear stress of 747 Pa (eta747) of 450 to 3000 kPas.