摘要:
The invention provides chunk polycrystalline silicon having a concentration of carbon at the surface of 0.5-35 ppbw. A process for cleaning polycrystalline silicon chunks having carbon contaminations at the surface, includes a thermal treatment of the polycrystalline silicon chunks in a reactor at a temperature of 350 to 600° C., the polycrystalline silicon chunks being present in an inert gas atmosphere during the thermal treatment, and the polycrystalline silicon chunks after the thermal treatment having a concentration of carbon at the surface of 0.5-35 ppbw.
摘要:
The invention relates to a polycrystalline silicon portion having at least one fracture surface or cut surface, which includes metal contamination of from 0.07 ng/cm2 to 1 ng/cm2. The invention also relates to a method for breaking a silicon body, preferably a rod of polycrystalline silicon, including the steps: a) determining the lowest natural bending frequency of the silicon body; b) exciting the silicon body in its lowest natural bending frequency by means of an oscillation generator, the excitation being carried out at an excitation point of the silicon body such that the silicon body breaks at the excitation point; so that a silicon portion having a fracture surface results which includes metal contamination of from 0.07 ng/cm2 to 1 ng/cm2.
摘要翻译:本发明涉及具有至少一个断裂面或切割面的多晶硅部分,其包括0.07ng / cm 2至1ng / cm 2的金属污染。 本发明还涉及一种用于破坏硅体,优选多晶硅棒的方法,包括以下步骤:a)确定硅体的最低自然弯曲频率; b)通过振荡发生器激发其最低自然弯曲频率的硅体,激发在硅体的激发点处进行,使得硅体在激发点处断裂; 从而导致具有0.07ng / cm 2至1ng / cm 2的金属污染的具有断裂面的硅部分。
摘要:
A rod having a length of 0.5 m to 4 m and having a diameter of 25 mm to 220 mm, comprising a high-purity alloy composed of 0.1 to 50 mol % germanium and 99.9 to 50 mol % silicon, the alloy having been deposited on a thin silicon rod or on a thin germanium-alloyed silicon rod, the deposited alloy having a polycrystalline structure.
摘要:
The invention provides chunk polycrystalline silicon having a concentration of carbon at the surface of 0.5-35 ppbw. A process for cleaning polycrystalline silicon chunks having carbon contaminations at the surface, includes a thermal treatment of the polycrystalline silicon chunks in a reactor at a temperature of 350 to 600° C., the polycrystalline silicon chunks being present in an inert gas atmosphere during the thermal treatment, and the polycrystalline silicon chunks after the thermal treatment having a concentration of carbon at the surface of 0.5-35 ppbw.
摘要:
The present invention relates to polycrystalline silicon chunks which are cubic and have a metal content of less than 200 pptw and a dopant content of less than 50 ppta. Methods for producing polycrystalline silicon chunks, include the steps of providing a polycrystalline silicon rod, comminuting the polycrystalline silicon rod into cubic chunks, and cleaning the polycrystalline silicon chunks, wherein comminution takes place using a spiked-roll crusher having at least one spiked roll, the spiked roll including W2C phases or WC phases with 0.1-10% of a metal carbide selected from the group consisting of titanium carbide, chromium carbide, molybdenum carbide, vanadium carbide, and nickel carbide or consisting of steel with 1-25% W.