HIGH-STRENGTH COLD-ROLLED STEEL SHEET
    1.
    发明申请
    HIGH-STRENGTH COLD-ROLLED STEEL SHEET 有权
    高强度冷轧钢板

    公开(公告)号:US20100252147A1

    公开(公告)日:2010-10-07

    申请号:US12742323

    申请日:2008-11-20

    摘要: The invention provides a high-strength cold-rolled steel sheet which is improved in elongation and stretch-flangeability and exhibits more excellent formability. The high-strength cold-rolled steel sheet has a composition which contains by mass C: 0.03 to 0.30%, Si: 0.1 to 3.0%, Mn: 0.1 to 5.0%, P: 0.1% or below, S: 0.005% or below, N: 0.01% or below, and Al: 0.01 to 1.00% with the balance consisting of iron and unavoidable impurities. The high-strength cold-rolled steel sheet has a structure which comprises at least 40% (up to 100% inclusive) in terms of area fraction of tempered martensite having a hardness of 300 to 380 Hv and the balance ferrite. The cementite particles in the tempered martensite take such dispersion that 10 or more cementite particles having equivalent-circle diameters of 0.02 to less than 0.1 μm are present per one μm2 of the tempered martensite and three or fewer cementite particles having equivalent-circle diameters of 0.1 μm or above are present per one μm2 of the tempered martensite.

    摘要翻译: 本发明提供了一种提高伸长率和拉伸凸缘性的高强度冷轧钢板,并且具有更优异的成形性。 高强度冷轧钢板的组成为C:0.03〜0.30%,Si:0.1〜3.0%,Mn:0.1〜5.0%,P:0.1%以下,S:0.005%以下 ,N:0.01%以下,Al:0.01〜1.00%,余量由铁和不可避免的杂质构成。 高强度冷轧钢板具有以硬度为300〜380Hv的回火马氏体的面积率和平衡铁素体为至少40%(含有100%以上)的结构。 回火马氏体中的渗碳体颗粒采用这样的分散体,每1μm回火马氏体和三个或更少个当量圆直径为0.1的渗碳体颗粒存在10个或更多个当量圆直径为0.02至小于0.1μm的渗碳体颗粒 每1μm2的回火马氏体存在1μm以上。

    Cold-rolled steel sheet and method for producing the same
    2.
    发明授权
    Cold-rolled steel sheet and method for producing the same 有权
    冷轧钢板及其制造方法

    公开(公告)号:US08840738B2

    公开(公告)日:2014-09-23

    申请号:US13258823

    申请日:2010-04-02

    摘要: A cold-rolled steel sheet of the present invention which has a composition containing, in terms of % by mass, C: 0.05-0.30%, Si: 3.0% or less (including 0%), Mn: 0.1-5.0%, P: 0.1% or less (including 0%), S: 0.010% or less (including 0%), and Al: 0.001-0.10%, and remainder being mainly iron, and which has a structure comprising, in terms of area ratio, 10-80% ferrite, less than 5% (including 0%) of the sum of retained austenite and martensite, and a hard phase as the remainder. The steel sheet gives a KAM value frequency distribution curve in which the relationship between the proportion of frequency having a KAM value ≦0.4, XKAM≦0.4°, and the area ratio of ferrite, Vα satisfies XKAM≦0.4°/Vα≧0.8 and the proportion of frequency having a KAM value in the range of 0.6-0.8, XKAM=0.6-0.8° is 10-20%. In the hard phase adjoining the ferrite, cementite, grains having an equivalent circle diameter of 0.1 μm or larger exist so that three or less such cementite grains are dispersed per μm2 of the hard phase. The steel sheet has improved balance between elongation and stretch flangeability and has better formability.

    摘要翻译: 本发明的冷轧钢板,其组成为以质量%计含有C:0.05〜0.30%,Si:3.0%以下(含0%),Mn:0.1-5.0%,P :0.1%以下(包括0%),S:0.010%以下(包括0%),Al:0.001-0.10%,余量主要为铁,其结构为面积比, 10-80%的铁素体,小于残留奥氏体和马氏体之和的5%(包括0%),剩余部分为硬质相。 钢板给出KAM值频率分布曲线,其中具有KAM值< lE; 0.4,XKAM≦̸ 0.4°的频率的比例与铁素体的面积比Vα之间的关系满足XKAM≦̸ 0.4°/Vα≥0.8,以及 KAM值在0.6-0.8,XKAM = 0.6-0.8°范围内的频率比例为10-20%。 在与铁素体相邻的硬相中,存在具有当量圆直径为0.1μm以上的渗碳体,每μm2硬相分散3个以下的渗碳体粒子。 钢板具有提高伸长率和拉伸凸缘性之间的平衡,并且具有更好的成形性。

    High-strength cold-rolled steel sheet
    3.
    发明授权
    High-strength cold-rolled steel sheet 有权
    高强度冷轧钢板

    公开(公告)号:US08679265B2

    公开(公告)日:2014-03-25

    申请号:US12742323

    申请日:2008-11-20

    IPC分类号: C22C38/00 C22C38/22 C22C38/08

    摘要: The invention provides a high-strength cold-rolled steel sheet which is improved in elongation and stretch-flangeability and exhibits more excellent formability. The high-strength cold-rolled steel sheet has a composition which contains by mass C: 0.03 to 0.30%, Si: 0.1 to 3.0%, Mn: 0.1 to 5.0%, P: 0.1% or below, S: 0.005% or below, N: 0.01% or below, and Al: 0.01 to 1.00% with the balance consisting of iron and unavoidable impurities. The high-strength cold-rolled steel sheet has a structure which comprises at least 40% (up to 100% inclusive) in terms of area fraction of tempered martensite having a hardness of 300 to 380 Hv and the balance ferrite. The cementite particles in the tempered martensite take such dispersion that 10 or more cementite particles having equivalent-circle diameters of 0.02 to less than 0.1 μm are present per one μm2 of the tempered martensite and three or fewer cementite particles having equivalent-circle diameters of 0.1 μm or above are present per one μm2 of the tempered martensite.

    摘要翻译: 本发明提供了一种提高伸长率和拉伸凸缘性的高强度冷轧钢板,并且具有更优异的成形性。 高强度冷轧钢板的组成为C:0.03〜0.30%,Si:0.1〜3.0%,Mn:0.1〜5.0%,P:0.1%以下,S:0.005%以下 ,N:0.01%以下,Al:0.01〜1.00%,余量由铁和不可避免的杂质构成。 高强度冷轧钢板具有以硬度为300〜380Hv的回火马氏体的面积率和平衡铁素体为至少40%(含有100%以上)的结构。 回火马氏体中的渗碳体颗粒采用这样的分散体,每1μm回火马氏体和三个或更少个当量圆直径为0.1的渗碳体颗粒存在10个或更多个当量圆直径为0.02至小于0.1μm的渗碳体颗粒 每1μm2的回火马氏体存在1μm以上。

    COLD-ROLLED STEEL SHEET AND METHOD FOR PRODUCING THE SAME
    4.
    发明申请
    COLD-ROLLED STEEL SHEET AND METHOD FOR PRODUCING THE SAME 有权
    冷轧钢板及其制造方法

    公开(公告)号:US20120012231A1

    公开(公告)日:2012-01-19

    申请号:US13258823

    申请日:2010-04-02

    摘要: A cold-rolled steel sheet of the present invention which has a composition containing, in terms of % by mass, C: 0.05-0.30%, Si: 3.0% or less (including 0%), Mn: 0.1-5.0%, P: 0.1% or less (including 0%), S: 0.010% or less (including 0%), and Al: 0.001-0.10%, and remainder being mainly iron, and which has a structure comprising, in terms of area ratio, 10-80% ferrite, less than 5% (including 0%) of the sum of retained austenite and martensite, and a hard phase as the remainder. The steel sheet gives a KAM value frequency distribution curve in which the relationship between the proportion of frequency having a KAM value ≦0.4, XKAM≦0.4°, and the area ratio of ferrite, Vα satisfies XKAM≦0.4°/Vα≧0.8 and the proportion of frequency having a KAM value in the range of 0.6-0.8, XKAM=0.6-0.8° is 10-20%. In the hard phase adjoining the ferrite, cementite, grains having an equivalent circle diameter of 0.1 μm or larger exist so that three or less such cementite grains are dispersed per μm2 of the hard phase. The steel sheet has improved balance between elongation and stretch flangeability and has better formability.

    摘要翻译: 本发明的冷轧钢板,其组成为以质量%计含有C:0.05〜0.30%,Si:3.0%以下(含0%),Mn:0.1-5.0%,P :0.1%以下(包括0%),S:0.010%以下(包括0%),Al:0.001-0.10%,余量主要为铁,其结构为面积比, 10-80%的铁素体,小于残留奥氏体和马氏体之和的5%(包括0%),剩余部分为硬质相。 钢板给出KAM值频率分布曲线,其中具有KAM值< lE; 0.4,XKAM≦̸ 0.4°的频率的比例与铁素体的面积比Vα之间的关系满足XKAM≦̸ 0.4°/Vα≥0.8,以及 KAM值在0.6-0.8,XKAM = 0.6-0.8°范围内的频率比例为10-20%。 在与铁素体相邻的硬相中,存在具有当量圆直径为0.1μm以上的渗碳体,每μm2硬相分散3个以下的渗碳体粒子。 钢板具有提高伸长率和拉伸凸缘性之间的平衡,并且具有更好的成形性。

    Electronic apparatus
    7.
    发明授权
    Electronic apparatus 失效
    电子仪器

    公开(公告)号:US08564941B2

    公开(公告)日:2013-10-22

    申请号:US12827088

    申请日:2010-06-30

    IPC分类号: H05K5/00 H05K7/00 G06F1/16

    CPC分类号: G06F1/1616

    摘要: An electronic apparatus includes a keyboard unit, a first circuit board, and a first electronic component. The keyboard unit includes a plate that includes a front surface and a bottom surface facing each other and a first coupling portion protruding from the bottom surface, and a plurality of keys provided on the front surface side of the plate. The first circuit board is provided to face the bottom surface via the first coupling portion and includes a second coupling portion to be coupled with the first coupling portion and a first front surface as a surface on a side that faces the bottom surface. The first electronic component is mounted on the first front surface of the first circuit board.

    摘要翻译: 电子设备包括键盘单元,第一电路板和第一电子元件。 键盘单元包括:板,其包括彼此面对的前表面和底表面;以及从底表面突出的第一联接部分和设置在板的前表面侧上的多个键。 第一电路板经由第一联接部分设置为面对底面,并且包括与第一联接部分联接的第二联接部分和作为面向底面的一侧上的表面的第一前表面。 第一电子部件安装在第一电路板的第一前表面上。

    Method and apparatus for producing mono-lower-alkyl monoalkanolamine
    9.
    发明授权
    Method and apparatus for producing mono-lower-alkyl monoalkanolamine 有权
    单低级烷基单链烷醇胺的制备方法和装置

    公开(公告)号:US08415502B2

    公开(公告)日:2013-04-09

    申请号:US12994599

    申请日:2008-10-24

    IPC分类号: C07C213/04

    摘要: A reaction column (12) to which a raw material mixture (11) containing a mono-lower-alkylamine (AA: raw material I) and an alkylene oxide (AO: raw material II) is supplied, an unreacted raw material distillation column (14) that separates an unreacted raw material (15) from a reaction product (13a) (containing the unreacted raw material (15), a target reaction product (monomer) (17), and a by-product (dimer) (18)), and a flash drum (16) to which a reaction product (13b) (containing the target reaction product (monomer) (17) and the by-product (dimer) (18)) is supplied, the flash drum (16) separating a mono-lower-alkyl monoalkanolamine (monomer, the target reaction product 17) in a gas state, are provided.

    摘要翻译: 将供给含有单低级烷基胺(AA:原料I)和环氧烷(AO:原料II))的原料混合物(11)的反应塔(12),未反应原料蒸馏塔 14),将未反应的原料(15)与反应产物(13a)(含有未反应的原料(15)),目标反应产物(单体)(17)和副产物(二聚体)(18)分离, )和提供有反应产物(13b)(含有目标反应产物(单体)(17)和副产物(二聚体)(18))的闪蒸筒),闪蒸鼓(16) 分离出气态下的单低级烷基单烷醇胺(单体,目标反应产物17)。