Abstract:
The object of the present invention is to provide an exhaust gas purifying catalyst that can achieve high purification performance while suppressing H2S emissions. The object is solved by an exhaust gas purifying catalyst in which the top layer of a catalyst coating layer comprises a ceria-zirconia composite oxide having a pyrochlore-type ordered array structure, in which the ceria-zirconia composite oxide contains at least one additional element selected from the group consisting of praseodymium, lanthanum, and yttrium at 0.5 to 5.0 mol % in relation to the total cation amount, and the molar ratio of (cerium+additional element):(zirconium) is within the range from 43:57 to 48:52.
Abstract:
An exhaust gas purification catalyst device includes a substrate and one or more catalyst coating layers on the substrate, wherein the one or more catalyst coating layers include copper ion-exchanged zeolite and alkali-containing zeolite containing one or more metals selected from among alkali metals and alkaline earth metals, the exhaust gas purification catalyst device satisfying either of the following conditions (A) and (B): (A) both the copper ion-exchanged zeolite and the alkali-containing zeolite are contained in one of the catalyst coating layers, and (B) the catalyst coating layer includes a first catalyst coating layer containing the copper ion-exchanged zeolite and a second catalyst coating layer containing the alkali-containing zeolite, with the first catalyst coating layer and second catalyst coating layer being layered together in direct contact.
Abstract:
The object of the present invention is to provide a high-performance exhaust gas purifying catalyst that can achieve oxygen absorption/release capacity and NOx purification performance. The object is solved by an exhaust gas purifying catalyst, which comprises a ceria-zirconia composite oxide having a pyrochlore-type ordered array structure in the upstream part of the catalyst coating layer, in which the ceria-zirconia composite oxide contains at least one additional element selected from the group consisting of praseodymium, lanthanum, and yttrium at 0.5 to 5.0 mol % of the total cation amount, and has a molar ratio of (cerium+the additional element):(zirconium) of 43:57 to 48:52.
Abstract:
A ceria-zirconia-based composite oxide containing a composite oxide of ceria and zirconia is provided, in which primary particles having a particle diameter of 1.5 to 4.5 μm account for, on a particle number basis, at least 50% of all primary particles in the ceria-zirconia-based composite oxide, and the molar ratio of cerium to zirconium in the ceria-zirconia-based composite oxide is between 43:57 and 55:45.
Abstract:
A ceria-zirconia composite oxide includes at least one of lanthanum, yttrium, and praseodymium. A rate of a total content of the at least one rare earth element to a total content of cerium and zirconium is 0.1 at % to 4.0 at %. A content of the rare earth element present in near-surface regions, which are at a distance of less than 50 nm from surfaces of primary particles of the ceria-zirconia composite oxide, accounts for 90 at % or more of the total content of the rare earth element. An average particle size of the primary particles of the ceria-zirconia composite oxide is 2.2 μm to 4.5 μm. After a predetermined durability test, the intensity ratio I(14/29) of a diffraction line at 2θ=14.5° to a diffraction line at 2θ=29° and the intensity ratio I(28/29) of a diffraction line at 2θ=28.5° to the diffraction line at 2θ=29° respectively satisfy the following conditions: I(14/29)≧0.02, and I(28/29)≦0.08.
Abstract:
A ceria-zirconia-based composite oxide containing a composite oxide of ceria and zirconia is provided, in which primary particles having a particle diameter of 1.5 to 4.5 μm account for, on a particle number basis, at least 50% of all primary particles in the ceria-zirconia-based composite oxide, and the molar ratio of cerium to zirconium in the ceria-zirconia-based composite oxide is between 43:57 and 55:45.
Abstract:
A ceria-zirconia-based composite oxide including a composite oxide containing ceria and zirconia, wherein the ceria-zirconia-based composite oxide contains at least one member selected from the group consisting of praseodymium, lanthanum, and yttrium in an amount of 0.5 to 5.0 mol % relative to a total amount of the cations contained in the ceria-zirconia-based composite oxide, where the ratio of the content of both cerium and the at least one member selected from the group consisting of praseodymium, lanthanum, and yttrium in the ceria-zirconia-based composite oxide to the content of zirconium therein ([cerium and the at least one member selected from the group consisting of praseodymium, lanthanum, and yttrium]:[zirconium]) is in the range of 43:57 to 48:52 by mole ratio.