摘要:
A pressure-sensitive adhesive layer-attached polarizing film of the invention includes: a polarizing film; and a pressure-sensitive adhesive layer provided on the polarizing film, wherein the polarizing film includes a polarizer and a transparent protective film provided on only one side of the polarizer, the pressure-sensitive adhesive layer is provided on a side of the polarizer where the transparent protective film is absent, and the pressure-sensitive adhesive layer is made of a pressure-sensitive adhesive composition containing a (meth)acryl-based polymer (A) and an alkali metal salt (B). The pressure-sensitive adhesive layer-attached polarizing film has a pressure-sensitive adhesive layer with an antistatic function and satisfactory durability and whose optical properties are less likely to be degraded.
摘要:
A pressure-sensitive adhesive composition, comprising: (A) a (meth)acryl-based polymer; and (B) an ionic compound comprising an anion component and a cation component, wherein the anion component is at least one of an anion component represented by the general formula (1): (CnF2n+1SO2)2N−, (1) wherein n is an integer of 3 to 10, and an anion component represented by the general formula (2): CF2(CmF2mSO2)2N−, (2) wherein m is an integer of 2 to 10.
摘要翻译:一种压敏粘合剂组合物,其包含:(A)(甲基)丙烯酸类聚合物; 和(B)包含阴离子组分和阳离子组分的离子化合物,其中阴离子组分是由通式(1)表示的阴离子组分中的至少一种:(CnF2n + 1SO2)2N-,(1)其中n 为3〜10的整数,通式(2)表示的阴离子成分:CF 2(C m F 2 m SO 2)2 N - ,(2)其中,m为2〜10的整数。
摘要:
A pressure-sensitive adhesive optical film of the invention comprises an optical film and a pressure-sensitive adhesive layer provided on the optical film, wherein the pressure-sensitive adhesive layer has a thickness (μm) standard deviation of 0.12 μm or less. The pressure-sensitive adhesive optical film makes it possible to reduce the problem of visible unevenness caused by a pressure-sensitive adhesive layer.
摘要:
A pressure-sensitive adhesive layer-attached polarizing film of the invention includes: a polarizing film; and a pressure-sensitive adhesive layer provided on the polarizing film, wherein the polarizing film includes a polarizer and a transparent protective film provided on only one side of the polarizer, the pressure-sensitive adhesive layer is provided on a side of the polarizer where the transparent protective film is absent, and the pressure-sensitive adhesive layer is made of a pressure-sensitive adhesive composition containing a (meth)acryl-based polymer (A) and an alkali metal salt (B). The pressure-sensitive adhesive layer-attached polarizing film has a pressure-sensitive adhesive layer with an antistatic function and satisfactory durability and whose optical properties are less likely to be degraded.
摘要:
A pressure-sensitive adhesive composition, comprising: a (meth)acryl-based polymer (A); and an ionic compound (B) comprising an anion component and a cation component, wherein the (meth)acryl-based polymer (A) is a hydroxyl group-containing (meth)acryl-based polymer (A) containing a monomer unit derived from a hydroxyl group-containing monomer, and the anion component has an organic group and three or more carbon atoms. The anion component is preferably at least one of anion components represented by the following formula (1): (CnF2n+1SO2)2N− (1) wherein n is an integer of 3 to 10; the following formula (2): CF2(CmF2mSO2)2N− (2) wherein m is an integer of 2 to 10; and the following formula (3): −O3S(CF2)lSO3− (3) wherein l is an integer of 3 to 10.
摘要翻译:一种压敏粘合剂组合物,其包含:(甲基)丙烯酸类聚合物(A); 以及包含阴离子成分和阳离子成分的离子性化合物(B),其中,所述(甲基)丙烯酸类聚合物(A)为含有源自羟基的(甲基)丙烯酸系聚合物(A) 含羟基的单体,阴离子成分具有有机基团和三个以上的碳原子。 阴离子成分优选为下述式(1)表示的阴离子成分中的至少一种:(CnF2n + 1SO2)2N-(1)其中,n为3〜10的整数, 下式(2):CF 2(CmF 2 m SO 2)2 N - (2)其中m为2〜10的整数; 和下式(3):-O 3 S(CF 2)l SO 3 - (3)其中l为3〜10的整数。
摘要:
A pressure-sensitive adhesive layer-attached polarizing film of the invention includes: a polarizing film; and a pressure-sensitive adhesive layer provided on the polarizing film, wherein the polarizing film includes a polarizer and a transparent protective film provided on only one side of the polarizer, the pressure-sensitive adhesive layer is provided on a side of the polarizer where the transparent protective film is absent, and the pressure-sensitive adhesive layer is made of a pressure-sensitive adhesive composition containing a (meth)acryl-based polymer (A) and an alkali metal salt (B). The pressure-sensitive adhesive layer-attached polarizing film has a pressure-sensitive adhesive layer with an antistatic function and satisfactory durability and whose optical properties are less likely to be degraded.
摘要:
A pressure-sensitive adhesive composition for use on an acryl- or cycloolefin-based polarizing film, comprising: a hydroxyl group-containing (meth)acryl-based polymer (A) containing a monomer unit derived from a hydroxyl group-containing monomer; and an ionic compound (B) comprising an anion component and a cation component, wherein the anion component has an organic group having 2 or more carbon atoms.
摘要:
A pressure-sensitive adhesive layer-attached optical film of the present invention comprises an optical film; and a pressure-sensitive adhesive layer and made from an ammonia-containing water-dispersible pressure-sensitive adhesive, wherein the pressure-sensitive adhesive layer has an ammonia content of 10 to 500 μg per 1 g of the pressure-sensitive adhesive layer, and shows a difference of 0 to 500 μg per 1 g of the pressure-sensitive adhesive layer in ammonia content before and after a heat durability test and humidity durability test, and the optical film includes a polarizing film with a degree of polarization of 99.99% or more. The pressure-sensitive adhesive layer-attached optical film has optical properties which are less changeable even in a high-temperature and/or high-humidity environment.
摘要:
Provided is a PSA sheet having a PSA layer. The PSA layer includes a layer A forming at least one surface thereof. The PSA sheet has an adhesive strength N0 of 2.0 N/10 mm or greater, after one day at room temperature following application of the layer A side to a surface of an alkaline float glass plate as an adherend having a contact angle of 5°-10° with distilled water; has an N1 to N0 reduction rate of 30% or lower, wherein N1 is a water-resistant adhesive strength measured after stored at room temperature for one day, immersed in water for 30 minutes, taken out from the water and then residual water is wiped off, and has an N2 to NO reduction rate of 40% or higher, wherein N2 is a water-peel strength measured after stored at room temperature for one day, 20 μL distilled water is dropped onto the adherend and is allowed to enter a PSA layer/adherend interfacial edge. N2 is measured at a tensile speed of 300 mm/min at a peel angle of 180°.
摘要:
Provided is a method for peeling a PSA sheet adhered on a polarizing plate. The PSA sheet has a PSA layer. The PSA layer includes a layer A forming at least one surface of the PSA layer. Of the polarizing plate, the surface to which the PSA sheet is adhered is corona-treated or plasma-treated. The peeling method includes a water-peel step in which the PSA sheet is peeled from the polarizing plate, in a state where an aqueous liquid exits at the interface between the polarizing plate and the PSA sheet at the front line of peeling the PSA sheet from the polarizing plate, with the aqueous liquid allowed to further enter the interface following the movement of the peel front line.