摘要:
A polyimide resin containing a repeating structural unit of the following formula (1), a repeating structural unit of the following formula (2), and a repeating structural unit of the following formula (A) or a repeating structural unit of the following formula (B), a content ratio of formula (1) with respect to the total of formula (1) and formula (2) being from 40 to 70 mol %, and a content ratio of formula (A) or formula (B) with respect to the total of formula (1) and formula (2) being more than 0 mol % and 25 mol % or less: wherein R1 represents a divalent group having from 6 to 22 carbon atoms containing at least one alicyclic hydrocarbon structure; R2 represents a divalent chain aliphatic group having from 5 to 20 carbon atoms; Ra represents a divalent group containing at least one aromatic ring which is bonded to a monovalent or divalent electron-attracting group; Rb represents a divalent group containing —SO2— or —Si(Rx)(Ry)O— wherein Rx and Ry each independently represent a chain aliphatic group having from 1 to 3 carbon atoms, or a phenyl group; and X1, X2, Xa, and Xb each independently represent a tetravalent group having from 6 to 22 carbon atoms containing at least one aromatic ring.
摘要:
Provided are [1] a xylylenediamine composition containing xylylenediamine and a pyridine compound (A) having at least one substituent including an amino group, wherein the content of the pyridine compound (A) is 0.001 to 0.1 parts by mass based on 100 parts by mass of the xylylenediamine; and [2] a method for producing a polyamide resin including the steps of introducing a pyridine compound (A) having at least one substituent including an amino group, a diamine including xylylenediamine (but excluding a diamine corresponding to the above-mentioned pyridine compound (A)), and a dicarboxylic acid into a reaction system and performing a polycondensation reaction, wherein the amount of the pyridine compound (A) to be introduced is 0.001 to 0.1 parts by mass based on 100 parts by mass of xylylenediamine.
摘要:
Provided are [1] a xylylenediamine composition containing xylylenediamine and a compound represented by the following general formula (1), wherein the content of the compound represented by the general formula (1) is 0.001 to 0.1 parts by mass based on 100 parts by mass of the xylylenediamine; and a method for producing a polyamide resin including the steps of introducing a compound represented by the following general formula (1), a diamine including xylylenediamine (but excluding the compound represented by the general formula (1)), and a dicarboxylic acid into a reaction system and performing a polycondensation reaction, wherein the amount of the compound represented by the general formula (1) to be introduced is 0.001 to 0.1 parts by mass based on 100 parts by mass of the xylylenediamine, where, in the general formula (1), n and m each independently represent an integer of 0 to 6, excluding the case where n and m are both 1.
摘要:
Provided are [1] a packaging body consisting of a resin composition containing a polyester resin (A), a polyamide resin (B), and an oxidation reaction accelerator (C), wherein when a thickness of the packaging body is defined as d (μm), and an average long diameter, an average short diameter, and a volume fraction of dispersed particles of the polyamide resin (B) in the packaging body are defined as L (μm), W (μm), and Vf, respectively, the following expression (1A) is satisfied; an oxygen transmission rate after a lapse of 100 hours after preparing of the packaging body is 0.01 [cc/(package·day·0.21 atm)] or less; and a haze value is 8% or less, and [2] a method for preserving goods by filling in a packaging body containing a polyester resin (A), a polyamide resin (B), and an oxidation reaction accelerator (C), wherein a content of the polyamide resin (B) in the packaging body is 2.0 to 3.5% by mass, and when an oxygen transmission rate of the packaging body after a lapse of 100 hours after preparing of the packaging body is defined as X [cc/(package·day·0.21 atm)], a volume of the packaging body is defined as V [L], and a mass of the packaging body is defined as M [g], the following expression (1B) is satisfied. 10
摘要:
Provided is a non-weave fabric containing a thermoplastic resin fiber and a carbon fiber as major ingredients, capable of yielding a resin molded article when molded thereinto, which is excellent in mechanical strength and in appearance, and, a multi-layered sheet having the non-weave fabric and a textile layer, which is excellent in mechanical strength and less likely to warp. The non-weave fabric includes a thermoplastic resin fiber (A), a carbon fiber (B), and a thermoplastic resin (C) having a glass transition temperature lower than that of the thermoplastic resin fiber (A), the ratio of content of the thermoplastic resin (C) being 1 to 50% by weight of the total content of the thermoplastic resin fiber (A) and the thermoplastic resin (C).
摘要:
A polyamide resin is produced by polycondensing a polyamide oligomer having a relative viscosity of from 1.1 to 1.3 and a water content of 3% by weight or less by melt-kneading using an intermeshed co-rotation twin screw extruder having at least one or more open vents OV1 and OV2 and at least one or more vacuum vents VV1 and VV2. A pressure-decreasing element Y for increasing the resin filling rate is provided at a position nearer to the supply section side than positions at which the vacuum vents VV1 and VV2 are provided, and an area of 30% or less of the total screw length is a vacuum area having a pressure of 300 Torr or less.
摘要:
Provided is a fiber fabric excellent in high mechanical strength and shapability. The fiber fabric comprising warps and wefts: wherein either one of the warps and the wefts is configured by a polyamide resin fiber composed of a polyamide resin composition, and the other is configured by a continuous carbon fiber; in an arbitrary square area of the fiber fabric, one side of the arbitrary square area is aligned in parallel to the warps, and other one side of the arbitrary square area is aligned in parallel to the wefts, the continuous carbon fiber has an average length 1.1 to 1.6 times longer than the length of a side of the square; the polyamide resin composition contains a polyamide resin in which 50% by mole or more of diamine structural units thereof is derived from xylylenediamine; and wherein the polyamide resin has a number-average molecular weight (Mn) of 6,000 to 30,000, and 0.5 to 5% by mass of the polyamide resin has a molecular weight of 1,000 or smaller.
摘要:
Provided is a polyether polyamide composition including a polyether polyamide in which a diamine constituent unit thereof is derived from a specified polyether diamine compound and a xylylenediamine, and a dicarboxylic acid constituent unit thereof is derived from an α,ω-linear aliphatic dicarboxylic acid having from 4 to 20 carbon atoms and a stabilizer.
摘要:
The present invention provides a polyester-based resin composition containing: a resin component which contains 80 to 98 mass % of polyester resin (A) including aromatic dicarboxylic acid units and diol units, and 20 to 2 mass % of polyamide resin (B) including diamine units and dicarboxylic acid units, the diamine units containing 70 mol % or more m-xylylenediamine units and the dicarboxylic acid units containing 70 mol % or more α,ω-aliphatic dicarboxylic acid units; and 0.005 to 0.1 parts by mass of a specific epoxy-functional polymer (C) with respect to 100 parts by mass of the resin component.
摘要:
A xylylenediamine-based polyamide resin/fiber composite material and molding are provided that do not exhibit a decline in properties under high temperatures and high humidities, and that exhibit a high elastic modulus and present little warping, and exhibit better recycle characteristics, a better moldability, and a better productivity than for thermosetting resins. The polyamide resin-type composite material comprises a fibrous material (B) impregnated with a polyamide resin (A) wherein at least 50 mole % of diamine structural units derived from xylylenediamine, and having a number-average molecular weight (Mn) of 6,000 to 30,000, and containing a component of a molecular weight of not more than 1,000 at 0.5 to 5 mass %.