摘要:
The present invention is intended to provide a sliding member which exhibits an excellent anti-seizure property even under starved lubricant conditions. In the present invention, there is provided a sliding member with a structure, in which a coating layer having a sliding surface is adhered to the surface of the base material, wherein the coating layer does not contain a resin binder but has solid lubricant plate crystal particles laminated therein, wherein these solid lubricant plate crystal particles have a lamellar crystal structure in which (001) planes are stacked in parallel, and at least in the sliding surface, the orientation index of the (001) plane of the solid lubricant plate crystal particles is 90% or more.
摘要:
The present invention is intended to provide a sliding member which exhibits an excellent anti-seizure property even under starved lubricant conditions. In the present invention, there is provided a sliding member with a structure, in which a coating layer having a sliding surface is adhered to the surface of the base material, wherein the coating layer does not contain a resin binder but has solid lubricant plate crystal particles laminated therein, wherein these solid lubricant plate crystal particles have a lamellar crystal structure in which (001) planes are stacked in parallel, and at least in the sliding surface, the orientation index of the (001) plane of the solid lubricant plate crystal particles is 90% or more.
摘要:
A slide member including a base material; and an overlay that is formed over the base material and that consists of Ag or Ag alloy including crystal planes (hk1) represented by Miller indices; wherein a relative X-ray diffraction intensity of crystal plane (200) to a sum of X-ray diffraction intensities of crystal planes (200), (111), (220), (311), and (222) of the overlay ranges between 1%≦(200)/{(200)+(111)+(220)+(311)+(222)}≦20% and the relative X-ray diffraction intensity of the crystal plane (200) to the X-ray diffraction intensity of the crystal plane (111) ranges between 1%≦(200)/(111)≦30%.
摘要:
A slide member including a base material; and an overlay that is formed over the base material and that consists of Ag or Ag alloy including crystal planes (hk1) represented by Miller indices; wherein a relative X-ray diffraction intensity of crystal plane (200) to a sum of X-ray diffraction intensities of crystal planes (200), (111), (220), (311), and (222) of the overlay ranges between 1%≦(200)/{(200)+(111)+(220)+(311)+(222)}≦20% and the relative X-ray diffraction intensity of the crystal plane (200) to the X-ray diffraction intensity of the crystal plane (111) ranges between 1%≦(200)/(111)≦30%.
摘要:
In a slide member in which an overlay is provided on a slide receiving surface of a base member, the overlay is formed by attaching a mixed solid lubricant on the slide receiving surface of the base member. The mixed solid lubricant is made by mixing a large amount of hydrogen containing solid lubricant which contains a large amount of hydrogen, and a small amount of hydrogen containing solid lubricant which contains a smaller hydrogen amount than the large amount of hydrogen containing lubricant. Thereby, a lubricant absence region where the solid lubricant is absent in a thickness direction is formed on the slide receiving surface of the base member after sliding, and an oxidized portion where the base member is oxidized is formed in the lubricant absence region.
摘要:
Disclosed is a Cu--Pb alloy bearing and a producing method thereof. The Cu--Pb alloy bearing consists of a backing metal layer and a Cu--Pb bearing alloy layer which is bonded to the backing metal layer and whose matrix contains dispersed Pb-phase grains. Within an at least 30 .mu.m thick surface region of the Cu--Pb bearing alloy layer, the Pb-phase grains comprise at least one of In and Sn in an amount or a total amount of not less than 2 wt %, respectively, which are elements added into the Pb-phase grains by migration.
摘要:
A slide member including a base material; an intermediate layer consisting of Ag or Ag-based alloy and an additive element of a first quantity formed over the base material; and an overlay comprising Bi or Bi-based alloy and the additive element of a second quantity formed over the intermediate layer, wherein the additive element consists of a low melting point metal, the first quantity being five times or greater than the second quantity.
摘要:
There is disclosed a bearing structure having an excellent fretting resistance. In the bearing structure in which a sliding bearing is mounted at its back face on a housing, and rotatably supports a rotation shaft at an inner face thereof, and a covering layer of an amorphous alloy is formed on at least one of the back face of the sliding bearing and an inner surface of the housing. Thanks to an excellent non-adhesion property of the amorphous alloy, adhesion is less liable to develop between the back face of the bearing and the housing even if a slight friction repeatedly occurs therebetween, thereby imparting an excellent fretting resistance to the bearing structure.
摘要:
In a slide member in which an overlay is provided on a slide receiving surface of a base member, the overlay is formed by attaching a mixed solid lubricant on the slide receiving surface of the base member. The mixed solid lubricant is made by mixing a large amount of hydrogen containing solid lubricant which contains a large amount of hydrogen, and a small amount of hydrogen containing solid lubricant which contains a smaller hydrogen amount than the large amount of hydrogen containing lubricant. Thereby, a lubricant absence region where the solid lubricant is absent in a thickness direction is formed on the slide receiving surface of the base member after sliding, and an oxidized portion where the base member is oxidized is formed in the lubricant absence region.
摘要:
Disclosed is a sliding member having a bearing alloy layer, an intermediate layer of Ni or a Ni alloy formed on the bearing alloy layer, and an overlay layer of a Sn alloy containing Cu formed on the intermediate layer. There exist Sn—Cu compounds in the overlay layer, which protrudently extend from the intermediate layer. The hard Sn—Cu compounds contribute to the overlay layer in improving fatigue resistance property. A soft Sn matrix being rich in an outer surface region of the overlay layer is responsible for keeping good conformability to have excellent anti-seizure property.