Abstract:
The present invention relates to a micropowder, wherein the particles of the micropowder have a Dv10 value of at least 2 micrometer and the micropowder comprises mesopores which have an average pore diameter in the range of from 2 to 50 nm and comprise, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc.
Abstract:
The present invention relates to a micropowder, wherein the particles of the micropowder have a Dv10 value of at least 2 micrometer and the micropowder comprises mesopores which have an average pore diameter in the range of from 2 to 50 nm and comprise, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc.
Abstract:
The present invention relates to a process for the regeneration of a catalyst comprising a titanium-containing zeolite, said catalyst having been used in a process for the preparation of an olefin oxide and having phosphate deposited thereon, said process for the regeneration comprising the steps: (a) separating the reaction mixture from the catalyst, (b) washing the catalyst obtained from (a) with liquid aqueous system; (c) optionally drying the catalyst obtained from (b) in a gas stream comprising an inert gas at a temperature of less than 300° C.; (d) calcining the catalyst obtained from (c) in a gas stream comprising oxygen at a temperature of at least 300° C.
Abstract:
The present invention relates to a micropowder, wherein the particles of the micropowder have a Dv10 value of at least 2 micrometer and the micropowder comprises mesopores which have an average pore diameter in the range of from 2 to 50 nm and comprise, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc.