REINFORCED THERMOPLASTIC ARTICLES, COMPOSITIONS FOR THE MANUFACTURE OF THE ARTICLES, METHODS OF MANUFACTURE, AND ARTICLES FORMED THEREFROM
    1.
    发明申请
    REINFORCED THERMOPLASTIC ARTICLES, COMPOSITIONS FOR THE MANUFACTURE OF THE ARTICLES, METHODS OF MANUFACTURE, AND ARTICLES FORMED THEREFROM 审中-公开
    强化热塑性制品,制品制造的组合物,制造方法和形成的制品

    公开(公告)号:US20130244528A1

    公开(公告)日:2013-09-19

    申请号:US13784901

    申请日:2013-03-05

    申请人: Daniel F. LOWERY

    发明人: Daniel F. LOWERY

    摘要: A composition for the manufacture of a porous, compressible article, the composition comprising a combination of: a plurality of reinforcing fibers; a plurality of polysulfone fibers; and a plurality of polymeric binder fibers; wherein the polymeric binder fibers have a melting point lower than the polysulfone fibers; methods for forming the porous, compressible article; and articles containing the porous, compressible article. An article comprising a thermoformed dual matrix composite is also disclosed, wherein the composite exhibits a time to peak release, as measured by FAR 25.853 (OSU test), a 2 minute total heat release, as measured by FAR 25.853 (OSU test), and an NBS optical smoke density of less than 200 at 4 minutes, determined in accordance with ASTM E-662 (FAR/JAR 25.853).

    摘要翻译: 一种用于制造多孔,可压缩制品的组合物,所述组合物包含以下组合:多个增强纤维; 多个聚砜纤维; 和多个聚合物粘合纤维; 其中聚合物粘合纤维的熔点低于聚砜纤维; 形成多孔,可压缩制品的方法; 和含有多孔,可压缩制品的制品。 还公开了一种包含热成型双基质复合材料的制品,其中通过FAR 25.853(OSU试验)测量,复合材料显示峰值释放时间,通过FAR 25.853(OSU试验)测量的2分钟总热释放,以及 在4分钟内小于200的NBS光学烟雾密度根据ASTM E-662(FAR / JAR 25.853)测定。

    Steam purification of polyimide resins
    2.
    发明授权
    Steam purification of polyimide resins 有权
    聚酰亚胺树脂的蒸汽净化

    公开(公告)号:US08357773B1

    公开(公告)日:2013-01-22

    申请号:US13286161

    申请日:2011-10-31

    IPC分类号: C08G64/00 C08G63/02

    摘要: The disclosure relates to a steam stripping process for producing purified polyimides, e.g., polyetherimide homopolymers and polyetherimide copolymers. The process can include contacting an initial polyimide with steam to remove a volatile species from the initial polyimide to produce a purified polyimide. The purified polyimide can have a weight average molecular weight of from 5,000 to 80,000 Daltons. The weight average molecular weight of the purified polyimide can be greater than or equal to 90% of the weight average molecular weight of the initial polyimide. The purified polyimide can have less than 44 ppm of a volatile species, having a molecular weight of less than 250 Daltons. The polyimide can have less than 10 ppm of a metal cation.

    摘要翻译: 本公开涉及用于生产纯化的聚酰亚胺的蒸汽汽提方法,例如聚醚酰亚胺均聚物和聚醚酰亚胺共聚物。 该方法可以包括使初始聚酰亚胺与蒸汽接触以从初始聚酰亚胺中除去挥发性物质以产生纯化的聚酰亚胺。 纯化的聚酰亚胺可以具有5,000至80,000道尔顿的重均分子量。 纯化的聚酰亚胺的重均分子量可以大于或等于初始聚酰亚胺的重均分子量的90%。 纯化的聚酰亚胺可以具有小于44ppm的分子量小于250道尔顿的挥发性物质。 聚酰亚胺可以具有小于10ppm的金属阳离子。

    Solventless process for the preparation of amine functional polyetherimide resins with improved melt flow
    4.
    发明授权
    Solventless process for the preparation of amine functional polyetherimide resins with improved melt flow 有权
    用于制备具有改进的熔体流动的胺官能聚醚酰亚胺树脂的无溶剂方法

    公开(公告)号:US08722187B2

    公开(公告)日:2014-05-13

    申请号:US13286093

    申请日:2011-10-31

    IPC分类号: B32B27/34

    摘要: The disclosure relates to a process that includes blending a polyimide resin and a primary alky amine organic compound to produce an aryl amine functionalized polyimide, having aryl amine functionality in excess of any anhydride functionality. The polyimide resin can have a weight average molecular weight (Mw) from 5,000 to 100,000 daltons. The organic compound can include at least one primary aliphatic amine without a direct linkage of a nitrogen to an aryl group and without a functionality selected from a halogen functionality, a hydroxyl functionality, a sulfonic acid functionality, a sulfonic acid salt functionality, and combinations thereof. The disclosure also relates to alkyl imide functionalized polyimides also with aryl amine functionalized polyimides, having aryl amine functionality in excess of any anhydride functionality and articles produced therefrom.

    摘要翻译: 本公开涉及一种方法,其包括将聚酰亚胺树脂和伯烷基胺有机化合物混合以制备芳基胺官能化聚酰亚胺,其芳基胺官能度超过任何酸酐官能度。 聚酰亚胺树脂的重均分子量(Mw)可以为5,000至100,000道尔顿。 有机化合物可以包括至少一种伯脂族胺,而不将氮直接连接到芳基上,而不具有选自卤素官能团,羟基官能团,磺酸官能团,磺酸盐官能团及其组合的官能团 。 本公开还涉及具有芳基胺官能化聚酰亚胺的烷基酰亚胺官能化聚酰亚胺,其具有超过任何酸酐官能团的芳基胺官能团和由其制备的制品。