Poly(arylene ether)/polyamide composition
    1.
    发明授权
    Poly(arylene ether)/polyamide composition 有权
    聚(亚芳基醚)/聚酰胺组合物

    公开(公告)号:US07413684B2

    公开(公告)日:2008-08-19

    申请号:US11107684

    申请日:2005-04-15

    IPC分类号: H01B1/24

    CPC分类号: H01B1/24

    摘要: A conductive composition comprises a poly(arylene ether), a polyamide, a conductive additive, and an impact modifier, wherein the composition demonstrates less than or equal to 0.0150 grams of composition buildup on the die face per minute of running time per meter of die opening perimeter after extruding the composition at a steady state for five minutes.

    摘要翻译: 导电组合物包括聚(亚芳基醚),聚酰胺,导电添加剂和抗冲击改性剂,其中组合物表现出每分钟模具面积的每毫升模具面积的0.0150克, 将组合物在稳定状态下挤出五分钟后的开口周长。

    CONDUCTIVE THERMOPLASTIC COMPOSITION
    2.
    发明申请
    CONDUCTIVE THERMOPLASTIC COMPOSITION 审中-公开
    导电热塑性组合物

    公开(公告)号:US20070235699A1

    公开(公告)日:2007-10-11

    申请号:US11763658

    申请日:2007-06-15

    IPC分类号: C08G69/00

    摘要: Disclosed herein is a method of making conductive thermoplastic compositions, particularly conductive poly(arylene ether)/polyamide compositions using a conductive masterbatch, whereas the conductive masterbatch is made by a method comprising mixing conductive carbon black and a first resin to form a conductive carbon black/resin mixture; and compounding the conductive carbon black/resin mixture with a second resin, wherein the first resin is a powder.

    摘要翻译: 本发明公开了一种制备导电热塑性组合物,特别是使用导电母料的导电性聚(亚芳基醚)/聚酰胺组合物的方法,而导电母料通过包括混合导电炭黑和第一树脂以形成导电炭黑的方法制备 /树脂混合物; 并将所述导电炭黑/树脂混合物与第二树脂混合,其中所述第一树脂是粉末。

    Polyphenylene ether resin concentrates containing organic phosphates
    3.
    发明授权
    Polyphenylene ether resin concentrates containing organic phosphates 有权
    聚苯醚树脂浓缩物含有机磷酸盐

    公开(公告)号:US06486244B2

    公开(公告)日:2002-11-26

    申请号:US09764678

    申请日:2001-01-18

    IPC分类号: C08K332

    摘要: The invention relates to a process for the manufacture of a thermoplastic composition comprising a polyphenylene ether resin and a styrenic resin wherein the processes comprises a concentrate of polyphenylene ether resin with an organic phosphate compound. The concentrate allows for ease of handling of polyphenylene ether resin without the risk of dust ignition while obtaining substantially the same physical properties as obtained with polyphenylene ether resin powder. The invention also relates to articles formed out of the compositions made by the process of the invention.

    摘要翻译: 本发明涉及一种制造包含聚苯醚树脂和苯乙烯树脂的热塑性组合物的方法,其中该方法包括聚苯醚树脂与有机磷酸盐化合物的浓缩物。 浓缩物可以容易地处理聚苯醚树脂,而不会发生灰尘点燃的危险,同时获得与聚苯醚树脂粉末获得的基本相同的物理性能。 本发明还涉及由通过本发明的方法制备的组合物形成的制品。

    Polyphenylene ether resin concentrates
    4.
    发明授权
    Polyphenylene ether resin concentrates 有权
    聚苯醚树脂浓缩液

    公开(公告)号:US6096821A

    公开(公告)日:2000-08-01

    申请号:US285419

    申请日:1999-04-02

    摘要: The invention relates to a process for the manufacture of a thermoplastic composition comprising a polyphenylene ether resin and optionally, a styrenic resin wherein the processes comprises a polyphenylene ether resin in a particulate form having less than about 5% by weight, preferably less than about 2% by weight, more preferably less than about 1% by weight, and most preferably essentially no particles less than about 75 microns in size. The particulate form allows for ease of handling of polyphenylene ether resin with a substantially reduced risk of dust ignition while obtaining substantially the same physical properties as obtained with polyphenylene ether resin powder.The invention also relates to articles formed out of the compositions made by the process of the invention.

    摘要翻译: 本发明涉及一种用于制造包含聚苯醚树脂和任选的苯乙烯树脂的热塑性组合物的方法,其中所述方法包括颗粒形式的聚苯醚树脂,其具有小于约5重量%,优选小于约2重量% 重量%,更优选小于约1重量%,最优选基本上不含小于约75微米尺寸的颗粒。 颗粒形式允许易于处理聚苯醚树脂,同时获得与聚苯醚树脂粉末获得的基本上相同的物理性能,其具有显着降低灰尘点燃的风险。 本发明还涉及由通过本发明的方法制备的组合物形成的制品。

    Process for the manufacture of low gloss resins
    10.
    发明授权
    Process for the manufacture of low gloss resins 失效
    低光泽树脂制造工艺

    公开(公告)号:US5536780A

    公开(公告)日:1996-07-16

    申请号:US110142

    申请日:1993-08-20

    CPC分类号: C08L69/00 C08J3/005

    摘要: A process for making reduced gloss thermoplastic resin compositions is provided. The process involves compounding a nitrile polymer with an electrophilic reagent to form a polymeric gel compound, blending the polymeric gel compound with a first thermoplastic resin and a weight ratio of between 5:1 and 0.5:1 to make a concentrate comprising gels dispersed in the first thermoplastic resin, and admixing the concentrate with a second thermoplastic resin produced the desired composition, wherein the concentrate is used at a level of from 2 to 60 percent by weight based on the total weight of the composition. The process provides improved product consistency, and consistently yields a product exhibiting reduced gloss and high levels of impact strength with a uniformly dispersed concentration of polymeric gels therein. The compositions are useful in making molded articles exhibiting consistent reduced gloss and high impact strengths.

    摘要翻译: 提供一种制备减少光泽的热塑性树脂组合物的方法。 该方法包括将腈聚合物与亲电试剂混合以形成聚合物凝胶化合物,将聚合物凝胶化合物与第一热塑性树脂混合,并且重量比为5:1至0.5:1以制备包含分散在 第一热塑性树脂,并将浓缩物与产生所需组合物的第二热塑性树脂混合,其中基于组合物的总重量,浓缩物的用量为2-60重量%。 该方法提供了改进的产品一致性,并且一致地产生具有均匀分散的聚合物凝胶浓度的光泽降低和冲击强度高的产品。 所述组合物可用于制备具有一致的降低光泽度和高冲击强度的模塑制品。