Abstract:
Cure in place pressure sensitive adhesive compositions are described that comprise one or more of a bodying component, a structural diluent, a radical diluent as well as additives such as crosslinkers, external catalysts, photoinitiators and stabilizers/process aids. The bodying component can be acrylic or non-acrylic.
Abstract:
Cure in place pressure sensitive adhesive compositions are described that comprise one or more of a bodying component, a structural diluent, a radical diluent as well as additives such as crosslinkers, external catalysts, photoinitiators and stabilizers/process aids. The bodying component can be acrylic or non-acrylic.
Abstract:
Provided is a conductive adhesive tape comprising: a substrate that is formed in a nano-web form having a number of pores by spinning a polymer material by a spinning method; and a conductive adhesive layer that is formed in a non-porous form by directly spinning a conductive adhesive material by a spinning method on one or both surfaces of the substrate, or that is laminated on one or both surfaces of the substrate. Accordingly, thickness of the adhesive tape can be made thin, adhesive strength of the adhesive tape can be enhanced, and the adhesive tape can be precisely attached on even a curved surface. Further, when removing the adhesive tape from components, the adhesive layer can be prevented from remaining on the surface of the components.
Abstract:
A tape for fixing an electrode assembly and a method of manufacturing a battery are provided. The tape for fixing an electrode assembly can effectively fix an electrode assembly in a can by realizing a 3D shape by means of an electrolyte. Thus, the tape can be useful in preventing the electrode assembly from moving and rotating inside a can by external vibration or impact and also preventing damage of welded regions of a tab or disconnection of inner circuits.
Abstract:
Pressure sensitive adhesive compositions containing 92 to 99.9 parts of a block copolymer adhesive composition and 0.1 to less than 8 parts of an acrylic adhesive composition are described. Tapes including such adhesives, and methods of making such tapes are also described.
Abstract:
A method of preparing a window module includes providing a metal frame having a first major surface, applying a structural glazing tape to the first major surface of the metal frame, and positioning a glass panel overtop the structural glazing tape. The structural glazing tape includes a polymer foam tape having first and second major surfaces, an adhesive layer overlying the first major surface for bonding the structural glazing tape to the structural frame, and a release layer overlying the second major surface. The method further includes filling a channel defined by the glass panel, the metal frame, and the structural glazing tape with a curable sealant, and curing the sealant to bond the glass panel and the metal frame together.
Abstract:
Methods for bonding a polymer surface (e.g., a fluoropolymer surface) to a substrate, including foam tape substrates, and articles produced thereby. The methods can include using a primer composition having an amidine catalyst in combination with an amino-substituted organosilane ester.
Abstract:
An ethylene-propylene-diene rubber foamed material is obtained by foaming a rubber composition containing an ethylene-propylene-diene rubber. The ethylene-propylene-diene rubber foamed material has a 50% compressive load value of 0.1 to 2.0 N/cm2 and the content ratio of a sulfur atom calculated based on the measurement result of a fluorescent X-ray measurement, based on mass, is 1000 ppm or less.
Abstract:
An ethylene-propylene-diene rubber foamed material is obtained by foaming a rubber composition containing an ethylene-propylene-diene rubber. A rate of change of an 80% compressive load value CL2 after being heated at 150° C. for 10 days to an 80% compressive load value CL1 before being heated is −50% or more and 50% or less and the 80% compressive load value CL1 before being heated is 0.5 N/cm2 or more and 10 N/cm2 or less.
Abstract translation:通过使含有乙烯 - 丙烯 - 二烯橡胶的橡胶组合物发泡,得到乙烯 - 丙烯 - 二烯橡胶发泡体。 在加热之前,在150℃加热10天后80%压缩载荷值CL1的80%压缩载荷值CL2的变化率为-50%以上且50%以下,80%压缩 加热前的负载值CL1为0.5N / cm 2以上且10N / cm 2以下。
Abstract:
There is provided a resin foam excellent in dustproof performance, particularly dustproof performance in a dynamic environment. The resin foam of the present invention has a thickness recovery ratio of 65% or more, wherein the thickness recovery ratio is defined as a ratio of a thickness 1 second after releasing a compressed state to an initial thickness, when the resin foam is compressed for 1 minute in the thickness direction so as to give a thickness equal to 20% of the initial thickness in a 23° C. atmosphere; and then the compressed state is released in a 23° C. atmosphere.