Abstract:
Provided is a method of fabricating an organic light emitting device that may form a light scattering layer having an irregular random structure at a low temperature. The method includes providing a substrate coated with a precursor layer; sequentially forming a metal layer and an organic layer on the precursor layer; performing a heat treatment of the organic layer to form an organic mask from the organic layer; patterning the metal layer by using the organic mask to form a metal mask; patterning the precursor layer by using the metal mask to form a light scattering layer having an irregular random structure; removing the metal mask and the organic mask; and sequentially stacking a planarization layer, a first electrode, an organic light emitting layer, a second electrode, and a passivation layer on the light scattering layer.
Abstract:
Provided are a random wrinkle structure-formable compound, a composition including the same, a film including a random wrinkle structure, a method of forming the film, and an organic light emitting device including the film. A compound according to the present invention is coated and then, a film having a surface structure of random wrinkles may be simply formed through simple ultraviolet (UV) curing or thermosetting. When the film thus formed is used in an organic light emitting device, light generated from the organic light emitting device is scattered on surfaces of the random wrinkles to prevent light guide or total reflection, and thus, light is extracted to the outside. That is, a random structure disposed at the outside of the device performs a light extraction function and consequently, light efficiency of the organic light emitting device may be increased.
Abstract:
Provided are a composition for a light transmittance control film, and a light transmittance control film. According to the inventive concept, the light transmittance control film includes a matrix part including a copolymer and a polymer chain which is grafted to the copolymer, and a dispersed part including a polymer derived from a first monomer, and are provided in the matrix part, wherein the polymer chain is derived from the first monomer, first light transmittance is shown while external force is applied, and second light transmittance which is greater than the first light transmittance may be shown after the external force is removed.
Abstract:
The present invention relates to a shape-variable electronic device and an operation method of the same and, more specifically, the shape-variable electronic device includes: a substrate having a cell region; a light source unit on the cell region; and a flexible layer vertically spaced apart from the light source unit. The flexible layer includes an actuator part that changes a shape of the flexible layer, and the actuator part includes: a photo-thermal response part that receives light emitted from the light source unit and generates thermal energy; a deformation part which receives the thermal energy from the photo-thermal response part and of which mechanical stiffness is reduced; and a top electrode and a bottom electrode on both surfaces of the deformation part, respectively.
Abstract:
Provided are a composition for a light transmittance control film, and a light transmittance control film. According to the inventive concept, the light transmittance control film includes a matrix part including a copolymer and a polymer chain which is grafted to the copolymer; and a dispersed part including a polymer derived from a first monomer, and are provided in the matrix part, wherein the polymer chain is derived from the first monomer, first light transmittance is shown while external force is applied, and second light transmittance which is greater than the first light transmittance may be shown after the external force is removed.
Abstract:
A composition for forming film having wrinkle structure and a method of forming the film are disclosed. The composition includes photo-curable agent and photoinitiator dissolved in the photo-curable agent. The cut off wavelength of light transmittance of the photo-curable agent is greater than the cut off wavelength of light absorbance of the photoinitiator. Photo-cured thin film is formed at the upper portion of composition layer at an initial time period of irradiation. By subsequent contraction, the photo-cured thin film forms wrinkles. The wrinkle structure is controlled by the relation of the cut off wavelength of light transmittance of the photo-curable agent and the cut off wavelength of light absorbance of the photoinitiator, the photo-curing rate of the composition and the thickness of the composition layer, and the photoinitiator concentration, etc., before photo-curing. The film may increase the emission efficiency of LED and OLED and the sensing effect of sensor.
Abstract:
Disclosed is a varifocal lens module. A varifocal lens module according to an embodiment includes a lens formed of a flexible and transparent material and having a focal length varying according to a variable shape thereof; at least one driving part expanded or contracted in response to an electric signal; and at least one structural body configured to physically or chemically connect the lens and each driving part.
Abstract:
There are provided an image processing apparatus and a control method thereof. An image processing apparatus includes an image sensor for acquiring a target image, an image processing module for performing focusing on a specific area of the acquired target image and determining a focal surface of the target image on the basis of the performed focusing, and a drive control module for controlling the curvature of the image sensor, based on the determined focal surface.
Abstract:
Provided is a method of fabricating an organic scattering layer. The method may include providing a deposition apparatus with a reaction chamber and a source chamber, loading a substrate in the reaction chamber, supplying carrier gas into the source chamber that may be configured to supply an evaporated organic source material into the reaction chamber, a temperature of the carrier gas ranging from 25° C. to 50° C., and spraying the carrier gas and the evaporated organic source material into the reaction chamber through a showerhead to deposit an organic scattering layer on the substrate, the organic scattering layer including organic particles, which may be provided in a molecularized form of the evaporated organic source material, and thereby having an uneven surface.
Abstract:
Provided is a dual-mode display including a substrate, and a plurality of sub pixels on the substrate. Each of the sub pixels may include an emissive device, a reflective optical filter provided on a surface of the emissive device, and an optical shutter provided on other surface of the emissive device.