Method for manufacturing electrically conductive macromolecules and solid state electrolytic capacitor using electrically conductive macromolecules
    2.
    发明授权
    Method for manufacturing electrically conductive macromolecules and solid state electrolytic capacitor using electrically conductive macromolecules 有权
    使用导电性高分子制造导电性高分子和固态电解电容器的方法

    公开(公告)号:US07459519B2

    公开(公告)日:2008-12-02

    申请号:US10541484

    申请日:2004-05-17

    申请人: Tsunenori Yoshida

    发明人: Tsunenori Yoshida

    摘要: The method for manufacturing electrically conductive macromolecules of the present invention is provided by reacting at least a monomer and an oxidizing agent to obtain electrically conductive macromolecules by a chemical polymerization method, the method including reacting the monomer and the oxidizing agent at least in a polymerizing vessel that contains a steam atmosphere. With this method, it is possible to obtain flat, electrically conductive macromolecules (10). Thus, it is possible to provide a method and an apparatus for manufacturing electrically conductive macromolecules in which it is possible to combine both low ESR and high capacity in a solid state electrolytic capacitor, realize low losses, and have low current leakage.

    摘要翻译: 本发明的导电性高分子的制造方法是通过至少使单体与氧化剂反应而通过化学聚合法进行导电性高分子化而提供的,所述方法包括使单体和氧化剂至少在聚合容​​器 含有蒸汽气氛。 通过这种方法,可以获得平坦的,导电的大分子(10)。 因此,可以提供一种用于制造导电性大分子的方法和装置,其中可以在固态电解电容器中组合低ESR和高容量,实现低损耗并且具有低电流泄漏。

    Shelf-stable polyester/HMMM powder coating
    4.
    发明授权
    Shelf-stable polyester/HMMM powder coating 失效
    保质期聚酯/ HMMM粉末涂料

    公开(公告)号:US5302462A

    公开(公告)日:1994-04-12

    申请号:US848514

    申请日:1992-03-09

    摘要: The reaction of less than the stoichiometric amount of a methoxymethyl aminotriazine with a linear, hydroxyl-terminated polyester in a mixture of the two wherein the polyester to triazine ratio is from about 97:3 to about 70:30 by weight affords a storage stable coating powder which forms an attractive, pin hole-free film when fused on a substrate at thicknesses of from about 3.9 to about 6.8 mils.

    摘要翻译: 二甲基甲基氨基三嗪与直链羟基封端的聚酯在两者的混合物中的反应,其中聚酯与三嗪的比例为约97:3至约70:30,得到保存稳定的涂层 粉末,其在约3.9至约6.8密耳的厚度下在基底上熔合时形成有吸引力的无针孔膜。

    Preparation of insoluble polymer powders which are only slightly
swellable
    5.
    发明授权
    Preparation of insoluble polymer powders which are only slightly swellable 失效
    只能轻微溶胀的不溶性聚合物粉末的制备

    公开(公告)号:US4658002A

    公开(公告)日:1987-04-14

    申请号:US777329

    申请日:1985-09-18

    CPC分类号: C08F26/10

    摘要: Insoluble polymer powders which are only slightly swellable are prepared by polymerization of N-vinylpyrrolidone or a mixture of (a) an N-vinylcarboxamide, acrylamide, methacrylamide, acrylic acid, methacrylic acid, acrylates, methacrylates and/or a vinyl ester and (b) from 0.1 to 10% by weight, based on the total amount of monomers, of, as a crosslinking agent, a compound possessing two or more ethylenically unsaturated double bonds, in a powder bed in the presence of a heat-transfer medium and in the absence of oxygen and polymerization initiators, at from 90.degree. to 220.degree. C., the powder state being maintained, the reaction mass being circulated and the heat-transfer medium evaporated from the polymerization zone.The resulting polymers are used as adsorbents, as formulation assistants for crop protection agents or as ion exchangers.

    摘要翻译: 通过聚合N-乙烯基吡咯烷酮或(a)N-乙烯基甲酰胺,丙烯酰胺,甲基丙烯酰胺,丙烯酸,甲基丙烯酸,丙烯酸酯,甲基丙烯酸酯和/或乙烯基酯和(b)的混合物来制备仅稍微溶胀的不溶性聚合物粉末 ),基于作为交联剂的单体总量的0.1〜10重量%的具有两个以上烯键式不饱和双键的化合物,在传热介质存在下在粉末床中, 不存在氧和聚合引发剂,在90℃至220℃下保持粉末状态,使反应物质循环并且传热介质从聚合区蒸发。 所得聚合物用作作为作物保护剂的配方助剂或作为离子交换剂的吸附剂。