摘要:
Provided is a production method for producing pellets that are used for producing an iron-nickel alloy and that are produced by mixing at least a nickel oxide ore, a carbonaceous reducing agent, and an iron oxide and agglomerating the obtained mixtures, the method comprising: a step S11 for producing at least two types of mixtures having different mixing ratios of nickel oxide ore, carbonaceous reducing agent, and iron oxide; and a step S12 for forming pellets, which are agglomerates having a layered structure, by using the two or more types of mixtures such that the mixture with the highest content ratio of iron oxide, among the two or more types of mixtures forms the outermost layer.
摘要:
The invention relates to a method for producing a ferroalloy containing nickel. From a fine-grained raw material containing iron and chromium and a fine-grained raw material containing nickel, a mixture is formed with binding agent, the mixture is agglomerated so that first formed objects of desired size are obtained. The objects formed are heat treated in order to strengthen the objects so that the heat treated objects withstand conveyance and loading into a smelter furnace. Further, the objects are smelted under reducing circumstances in order to achieve ferrochromenickel, a ferroalloy of a desired composition containing at least iron, chromium and nickel.
摘要:
Aspects of the present invention refer to a MHP process do produce rough ferro-nickel product and that may include the steps of mixing nickel hydroxide with an iron source and slagging agents, putting the mixture in contact with a reducing agent producing a ferronickel alloy, and producing a roasted product that has disseminated ferronickel alloy inside the structure.
摘要:
The invention relates to a method for producing a ferroalloy containing nickel. From a fine-grained raw material containing iron and chromium and a fine-grained raw material containing nickel, a mixture is formed with binding agent, the mixture is agglomerated so that first formed objects of desired size are obtained. The objects formed are heat treated in order to strengthen the objects so that the heat treated objects withstand conveyance and loading into a smelter furnace. Further, the objects are smelted under reducing circumstances in order to achieve ferrochromenickel, a ferroalloy of a desired composition containing at least iron, chromium and nickel.
摘要:
The invention relates to a method for producing a ferroalloy containing nickel. From a fine-grained raw material containing iron and chromium and a fine- grained raw material containing nickel, a mixture is formed with binding agent, the mixture is agglomerated so that first formed objects of desired size are obtained. The objects formed are heat treated in order to strengthen the objects so that the heat treated objects withstand conveyance and loading into a smelter furnace. Further, the objects are smelted under reducing circumstances in order to achieve ferrochromenickel, a ferroalloy of a desired composition containing at least iron, chromium and nickel.
摘要:
A metallic article is produced by furnishing one or more nonmetallic precursor compound comprising the metallic base nickel, cobalt, iron, iron-nickel, or iron-nickel-cobalt, and at least one alloying element. The nonmetallic precursor compound(s) are chemically reduced to produce an initial metallic particle without melting the initial metallic particle. The initial metallic particle is thereafter melted and solidified to produce the metallic article. The melted-and-solidified metal may be used in the as-cast form, or it may be converted to billet and further worked to the final form.
摘要:
A method of recovering copper and nickel from sulphidic minerals containing copper, nickel and iron comprises the steps of roasting the mineral, preferably to provide magnetite; sulphating, for example with sulphuric acid, sulphur trioxide, metal sulphate and/or sulphur dioxide together with oxygen; and a subsequent leaching of the sulphated material and recovery of copper from the leaching solution, for example by electrolysis. All or part of the leaching solution with its nickel content is recycled to the roasting stage, and the nickel content is removed in the form of nickel oxide together with the leaching residue, from which nickel can be recovered.
摘要:
Disclosed is a method of recovering ferronickel from oxidated nickel ores,omprising preparing of a charge accompanied by roasting ore, a reducing agent and flux, followed by electric smelting of the charge. According to the proposed method, roasting of the ore with the reducing agent and roasting of the flux are carried out separately.