摘要:
There is disclosed a heat-insulating member including a pair of substrates and an airtight sealing part, in which the airtight sealing part is formed in an outer peripheral part between the pair of substrates to form a space between the pair of substrates, the space being in a vacuum or reduced pressure state, a sealing material that forms the airtight sealing part includes a low-melting glass, and the low-melting glass contains a vanadium oxide, barium oxide, phosphorus oxide, and tungsten oxide, in which the following two relational expressions are satisfied in terms of oxide contents: V2O5+BaO+P2O5+WO3≧90 and V2O5>BaO>P2O5>WO3 (wherein unit: mol %). Thereby, influence on environmental impact can be reduced and maintenance of airtightness and an improvement in acid resistance can be achieved.
摘要:
Neutron-absorbing glass that can be input into water, wherein gadolinium oxide, boron oxide, and zinc oxide are contained and B2O3 is contained 42 to 65 mol % in terms of oxide above.
摘要:
An electronically active glass has the composition (TxOy)z-(MuOv)w—(Na/LiBO2)t wherein T is a transition metal selected from V and Mo, M is a metal selected from Ni, Co, Na, Al, Mn, Cr, Cu, Fe, Ti and mixtures thereof, x, y, u, and v are the stoichiometric coefficients resulting in a neutral compound, i.e. x=2y/(oxidation state of T) and u=2v/(oxidation state of M), z, w and t are weight-%, wherein z is 70-80, w is 0-20 t is 10-30, and the sum of z, w and t is 100 weight-%, in particular V2O5—LiBO2 and V2O5—NiO—LiBO2.
摘要:
Provided is an optical glass which can satisfy all of the following requirements: (1) it contains no environmentally undesirable components; (2) it can easily achieve a low glass transition point; (3) it has a high refractive index and high dispersion; (4) it can easily provide a glass having a superior visible light transmittance; and (5) it has superior resistance to devitrification during preparation of a preform. The optical glass has a refractive index nd of 2.0 or more, an Abbe's number vd of 20 or less, a glass transition point of 450° C. or below, and a glass composition, in % by mass, of 70 to 90% Bi2O2, 4 to 29.9% B2O2, 0.1 to 10% Li2O+Na2O+K2O, and 0 to 2.5% SiO2+Al2O2 and is substantially free of lead component, arsenic component, F component, TeO2, and GeO2.
摘要翻译:提供可以满足以下所有要求的光学玻璃:(1)不含有环境不良成分; (2)可以轻松实现低玻璃化转变点; (3)折射率高,色散高; (4)可以容易地提供具有优异的可见光透射率的玻璃; 和(5)在制备预成型品时具有优异的抗失透性。 光学玻璃的折射率nd为2.0以上,阿贝数vd为20以下,玻璃化转变点为450℃以下,玻璃组合物的质量%为70〜90%的Bi 2 O 2 ,4〜29.9%的B 2 O 2,0.1〜10%的Li 2 O + Na 2 O + K 2 O和0〜2.5%的SiO 2 + Al 2 O 2,并且基本上不含铅成分,砷成分,F成分,TeO 2和GeO 2。
摘要:
A plasma display panel of the present invention includes display electrodes and address electrodes that cross each other. The electrode to be covered with the first dielectric layer contains at least one selected from silver and copper. The first glass contains Bi2O3. The first glass further contains 0 to 4 wt % of MoO3 and 0 to 4 wt % of WO3, and the total of the contents of MoO3 and WO3 that are contained in the first glass is in a range of 0.1 to 8 wt %. The first glass may contain, as components thereof: 0 to 15 wt % SiO2; 10 to 50 wt % B2O3; 15 to 50 wt % ZnO; 0 to 10 wt % Al2O3; 2 to 40 wt % Bi2O3; 0 to 5 wt % MgO; 5 to 38 wt % CaO+SrO+BaO; 0 to 4 wt % MoO3; and 0 to 4 wt % WO3, and the total of the contents of MoO3 and WO3 that are contained in the first glass is in the range of 0.1 to 8 wt %.
摘要:
For mounting on a substrate by using an electroconductive adhesive, an electroconductive paste for forming an external electrode which has improved moisture resistance and which is resistant to occurrence of external-electrode peeling, as well as a ceramic electronic component including the electroconductive paste are provided. The electroconductive paste includes a base-metal electroconductive powder, first glass frit, and an organic vehicle, wherein the first glass frit has a B2O3 content of 10 to 20 percent by mole, a SiO2 content of 50 to 65 percent by mole, an alkali metal oxide content of 10 to 20 percent by mole, a ZnO content of 1 to 5 percent by mole, a TiO2 content of 1 to 5 percent by mole, a ZrO2 content of 1 to 5 percent by mole, and an Al2O3 content of 1 to 5 percent by mole.
摘要翻译:为了通过使用导电粘合剂安装在基板上,提供了用于形成具有改善的耐湿性并且耐外部电极剥离发生的外部电极的导电浆料以及包括导电浆料的陶瓷电子部件。 导电浆料包括贱金属导电粉末,第一玻璃料和有机载体,其中第一玻璃料的B 2 O 3含量为10至20摩尔%,SiO 2含量为50至65摩尔%,碱 金属氧化物含量为10〜20摩尔%,ZnO含量为1〜5摩尔%,TiO 2含量为1〜5摩尔%,ZrO 2含量为1〜5摩尔%,Al 2 O 3含量为1 至5摩尔%。
摘要:
The plasma display panel (PDP) includes a front substrate and a second dielectric layer. At least one of the front substrate and the second dielectric layer is formed of a glass material. The glass material includes a transition metal oxide and a rare earth metal oxide. The transition metal oxide is at least one of oxides of cobalt (Co), nickel (Ni), selenium (Se), iron (Fe), manganese (Mn), chromium (Cr), vanadium (V) and scandium (Sc). The rare earth metal oxide is at least one of oxides of praseodymium (Pr), neodymium (Nd), samarium (Sm), dysprosium (Dy) and holmium (Ho).
摘要:
A glass composition for covering electrodes of the present invention contains: 0 to 15 wt % SiO2; 10 to 50 wt % B2O3; 15 to 50 wt % ZnO; 0 to 10 wt % Al2O3; 2 to 40 wt % Bi2O3; 0 to 5 wt % MgO; 5 to 38 wt % CaO+SrO+BaO; 0 to 0.1 wt % Li2O+Na2O+K2O; 0 to 4 wt % MoO3; and 0 to 4 wt % WO3, and the total of the contents of MoO3 and WO3 is in the range of 0.1 to 8 wt %. The glass composition for covering electrodes of the present invention may contain: 0 to 2 wt % SiO2; 10 to 50 wt % B2O3; 15 to 50 wt % ZnO; 0 to 10 wt % Al2O3; 2 to 40 wt % Bi2O3; 0 to 5 wt % MgO; 5 to 38 wt % CaO+SrO+BaO; 0 to 4 wt % MoO3; and 0 to 4 wt % WO3, and the total of the contents of MoO3 and WO3 may be in the range of 0.1 to 8 wt %.
摘要翻译:本发明的覆盖电极用玻璃组合物含有:0〜15重量%的SiO 2; 10至50重量%B 2 O 3 3; 15〜50wt%的ZnO; 0至10重量%的Al 2 O 3 3; 2至40重量%的Bi 2 O 3 3; 0〜5重量%的MgO; 5〜38重量%CaO + SrO + BaO; 0〜0.1重量%Li 2 O + Na 2 O + K 2 O; 0至4wt%MoO 3 3; 和0至4重量%的WO 3,MoO 3 3和WO 3 3的含量的总和在0.1至8的范围内 重量%。 本发明的覆盖电极用玻璃组合物可以含有0〜2重量%的SiO 2, 10至50重量%B 2 O 3 3; 15〜50wt%的ZnO; 0至10重量%的Al 2 O 3 3; 2至40重量%的Bi 2 O 3 3; 0〜5重量%的MgO; 5〜38重量%CaO + SrO + BaO; 0至4wt%MoO 3 3; 和0〜4重量%的WO 3,MoO 3 3和WO 3的含量的总和可以在0.1〜 8重量%。
摘要:
A plasma display panel of the present invention includes display electrodes and address electrodes that cross each other. The electrode to be covered with the first dielectric layer contains at least one selected from silver and copper. The first glass contains Bi2O3. The first glass further contains 0 to 4 wt % of MoO3 and 0 to 4 wt % of WO3, and the total of the contents of MoO3 and WO3 that are contained in the first glass is in a range of 0.1 to 8 wt %. The first glass may contain, as components thereof: 0 to 15 wt % SiO2; 10 to 50 wt % B2O3; 15 to 50 wt % ZnO; 0 to 10 wt % Al2O3; 2 to 40 wt % Bi2O3; 0 to 5 wt % MgO; 5 to 38 wt % CaO+SrO+BaO; 0 to 4 wt % MoO3; and 0 to 4 wt % WO3, and the total of the contents of MoO3 and WO3 that are contained in the first glass is in the range of 0.1 to 8 wt %.
摘要翻译:本发明的等离子体显示面板包括彼此交叉的显示电极和地址电极。 被第一介电层覆盖的电极含有选自银和铜中的至少一种。 第一个玻璃含有Bi 2 O 3 O 3。 第一玻璃还含有0至4重量%的MoO 3 3和0至4重量%的WO 3,并且MoO 3的含量的总和< 第一玻璃中含有的/ SUB&gt;和WO 3 3的比例在0.1〜8重量%的范围内。 作为其组分,第一玻璃可以含有0至15重量%的SiO 2; 10至50重量%B 2 O 3 3; 15〜50wt%的ZnO; 0至10重量%的Al 2 O 3 3; 2至40重量%的Bi 2 O 3 3; 0〜5重量%的MgO; 5〜38重量%CaO + SrO + BaO; 0至4wt%MoO 3 3; 和0〜4重量%的WO 3,第一玻璃中含有的MoO 3 3和WO 3的含量的总和是 在0.1〜8重量%的范围内。