公开(公告)号:US20190337097A1
公开(公告)日:2019-11-07
申请号:US15970518
申请日:2018-05-03
Applicant: United Technologies Corporation
Inventor: Henry H. Thayer , Dmitri Novikov , Robert J. Meehan , Bartolomeo Palmieri
IPC: B23K26/362 , F01D5/28 , B23K26/0622 , B23K26/146 , B23K26/402 , B23K31/10
Abstract: A method for stripping ceramic from a component includes applying a liquid to a ceramic coating of an outer surface of the component. The method also includes directing a plurality of laser pulses at the ceramic coating with the applied liquid in order to spall the ceramic coating from the component.
-
公开(公告)号:US20170283930A1
公开(公告)日:2017-10-05
申请号:US15626837
申请日:2017-06-19
Applicant: United Technologies Corporation
Inventor: Robert J. Meehan , Neil B. Ridgeway , Christopher J. Millea
IPC: C23C4/02
CPC classification number: C23C4/02 , B23K26/082 , B23K26/122 , B23K26/1224 , B23K26/123 , B23K26/40 , B23K2103/10 , C23C4/073 , C23C4/134 , C23C4/18 , C23C14/022 , C23C14/083 , C23C14/30 , C23C14/325 , C23C28/3215 , C23C28/3455 , F01D5/288 , F05D2230/13 , F05D2230/31 , F05D2300/701
Abstract: A method of forming a thermal barrier coating on a metal part includes laser cleaning a surface of the metal part to remove undesirable oxides and residues from the surface of the part. It further includes depositing an aluminum containing bondcoat on the part and thermally interdiffusing the bondcoat and the part with a heat treatment. Laser cleaning a surface of the bondcoat to remove oxides and debris from the surface forms an alpha aluminum oxide layer on the bondcoat. A ceramic topcoat is then deposited on the alpha aluminum oxide layer at a temperature above 1800° F. (982° C.).
-
公开(公告)号:US11440139B2
公开(公告)日:2022-09-13
申请号:US15970518
申请日:2018-05-03
Applicant: United Technologies Corporation
Inventor: Henry H. Thayer , Dmitri Novikov , Robert J. Meehan , Bartolomeo Palmieri
IPC: B23K26/00 , B23K26/362 , B23K26/0622 , B23K26/146 , B23K26/402 , B23K31/10 , F01D5/28 , B23K101/34
Abstract: A method for stripping ceramic from a component includes applying a liquid to a ceramic coating of an outer surface of the component. The method also includes directing a plurality of laser pulses at the ceramic coating with the applied liquid in order to spall the ceramic coating from the component.
-
公开(公告)号:US09683281B2
公开(公告)日:2017-06-20
申请号:US14683820
申请日:2015-04-10
Applicant: United Technologies Corporation
Inventor: Robert J. Meehan , Neil B. Ridgeway , Christopher J. Millea
IPC: B05D3/00 , C08J7/18 , G21H5/00 , C23C4/02 , C23C4/18 , C23C14/08 , C23C14/30 , C23C28/00 , C23C4/073 , B23K26/082 , C23C4/134 , B23K26/122 , B23K26/12 , B23K26/40 , C23C14/02 , C23C14/32 , F01D5/28 , B23K103/10
CPC classification number: C23C4/02 , B23K26/082 , B23K26/122 , B23K26/1224 , B23K26/123 , B23K26/40 , B23K2103/10 , C23C4/073 , C23C4/134 , C23C4/18 , C23C14/022 , C23C14/083 , C23C14/30 , C23C14/325 , C23C28/3215 , C23C28/3455 , F01D5/288 , F05D2230/13 , F05D2230/31 , F05D2300/701
Abstract: A method of forming a thermal barrier coating on a metal part includes laser cleaning a surface of the metal part to remove undesirable oxides and residues from the surface of the part. It further includes depositing an aluminum containing bondcoat on the part and thermally interdiffusing the bondcoat and the part with a heat treatment. Laser cleaning a surface of the bondcoat to remove oxides and debris from the surface forms an alpha aluminum oxide layer on the bondcoat. A ceramic topcoat is then deposited on the alpha aluminum oxide layer at a temperature above 1800° F. (982° C.).
-
公开(公告)号:US20160298222A1
公开(公告)日:2016-10-13
申请号:US14683820
申请日:2015-04-10
Applicant: United Technologies Corporation
Inventor: Robert J. Meehan , Neil B. Ridgeway , Christopher J. Millea
IPC: C23C4/02 , B23K26/082 , B23K26/12 , B23K26/40 , C23C14/32 , C23C4/134 , C23C14/30 , C23C14/08 , C23C14/02 , B23K26/122 , C23C4/073
CPC classification number: C23C4/02 , B23K26/082 , B23K26/122 , B23K26/1224 , B23K26/123 , B23K26/40 , B23K2103/10 , C23C4/073 , C23C4/134 , C23C4/18 , C23C14/022 , C23C14/083 , C23C14/30 , C23C14/325 , C23C28/3215 , C23C28/3455 , F01D5/288 , F05D2230/13 , F05D2230/31 , F05D2300/701
Abstract: A method of forming a thermal barrier coating on a metal part includes laser cleaning a surface of the metal part to remove undesirable oxides and residues from the surface of the part. It further includes depositing an aluminum containing bondcoat on the part and thermally interdiffusing the bondcoat and the part with a heat treatment. Laser cleaning a surface of the bondcoat to remove oxides and debris from the surface forms an alpha aluminum oxide layer on the bondcoat. A ceramic topcoat is then deposited on the alpha aluminum oxide layer at a temperature above 1800° F. (982° C.).
Abstract translation: 在金属部件上形成热障涂层的方法包括激光清洗金属部件的表面以从部件的表面去除不需要的氧化物和残留物。 它还包括在该部件上沉积含铝的粘合剂涂层,并用热处理热粘合涂层和部件。 激光清洁粘合涂层的表面以从表面去除氧化物和碎屑在粘合涂层上形成α氧化铝层。 然后在高于1800°F(982℃)的温度下,在α氧化铝层上沉积陶瓷面漆。
-
-
-
-