摘要:
A method of producing a directly blow-formed container. The method includes subjecting a multilayered parison having an inner surface formed of an olefin resin to direct blow forming, the olefin resin containing (i) an organic bleeding lubricant having a melting point of not higher than 50° C. in an amount of 5 to 10% by mass, and (ii) a high silica zeolite having a silica/alumina mole ratio of not less than 80 in an amount of 0.2 to 3.0% by mass.
摘要:
A method of producing a directly blow-formed container. The method includes subjecting a multilayered parison having an inner surface formed of an olefin resin to direct blow forming, the olefin resin containing (i) an organic bleeding lubricant having a melting point of not higher than 50° C. in an amount of 5 to 10% by mass, and (ii) a high silica zeolite having a silica/alumina mole ratio of not less than 80 in an amount of 0.2 to 3.0% by mass.
摘要:
A polylactic acid formed body including a polylactic acid base material (1) and a hydrocarbon film (3) vapor-deposited on the surface of the base material by a plasma CVD method. The polylactic acid base material (1) exhibits a sharp X-ray diffraction peak in which a half-width of peak appearing in the 10°-25° wide angle X-ray measurement is not more than 1.22°, and the hydrocarbon film (3) is vapor-deposited on the surface of the polylactic acid base material (1), and includes two layers of a high CH2 layer (3a) having a ratio of CH2 per the total of CH, CH2 and CH3 of not less than 40% and a low CH2 layer (3b) formed on the high CH2 layer (3a) and having a ratio of CH2 per the total of CH, CH2 and CH3 of not more than 35%.
摘要:
A polylactic acid formed body including a polylactic acid base material (1) and a hydrocarbon film (3) vapor-deposited on the surface of the base material by a plasma CVD method. The polylactic acid base material (1) exhibits a sharp X-ray diffraction peak in which a half-width of peak appearing in the 10°-25° wide angle X-ray measurement is not more than 1.22°, and the hydrocarbon film (3) is vapor-deposited on the surface of the polylactic acid base material (1), and includes two layers of a high CH2 layer (3a) having a ratio of CH2 per the total of CH, CH2 and CH3 of not less than 40% and a low CH2 layer (3b) formed on the high CH2 layer (3a) and having a ratio of CH2 per the total of CH, CH2 and CH3 of not more than 35%.
摘要:
A multi-layer direct blow bottle in which a metallic layer containing a metal pigment having an average thickness of not more than 1 μm dispersed in a resin is formed at a position where it is visible from the outer surface side.
摘要:
A decorative resin composition containing a metal pigment having an average thickness of not more than 600 nm dispersed in a blend of a low-density polyethylene (LDPE) having a density of not less than 0.910 g/cm3 but less than 0.930 g/cm3 and a linear low-density polyethylene (LLDPE) having a density of 0.910 to 0.925 g/cm3.