Container in which inner surface is formed from olefin resin layer
摘要:
A method of producing a directly blow-formed container. The method includes subjecting a multilayered parison having an inner surface formed of an olefin resin to direct blow forming, the olefin resin containing (i) an organic bleeding lubricant having a melting point of not higher than 50° C. in an amount of 5 to 10% by mass, and (ii) a high silica zeolite having a silica/alumina mole ratio of not less than 80 in an amount of 0.2 to 3.0% by mass.